Patent classifications
B21B19/04
Process for on-line quenching of seamless steel tube using residual heat and manufacturing method
An process for the on-line quenching of seamless steel tube using residual heat, a method for manufacturing a seamless steel tube, and a seamless steel tube. The process for the on-line quenching of a seamless steel tube comprises the following steps: when the temperature of a tube is higher than Ar3, evenly spraying water along a circumferential direction of the tube so as to continuously cool the tube to be not higher than T° C., the cooling rate being controlled to be E1° C./s to E2° C./s to obtain a microstructure with martensite as the main composition, wherein T=Ms−95° C., Ms represents the martensitic phase transition temperature, E1=20×(0.5−C)+15×(3.2−Mn)−8×Cr−28×Mo−4×Ni−2800×B, and E2=96×(0.45−C)+12×(4.6−Mn), and the C, Mn, Cr, Ni, B and Mo in the equations each represents the mass percentages of corresponding elements in the seamless steel tube.
Process for on-line quenching of seamless steel tube using residual heat and manufacturing method
An process for the on-line quenching of seamless steel tube using residual heat, a method for manufacturing a seamless steel tube, and a seamless steel tube. The process for the on-line quenching of a seamless steel tube comprises the following steps: when the temperature of a tube is higher than Ar3, evenly spraying water along a circumferential direction of the tube so as to continuously cool the tube to be not higher than T° C., the cooling rate being controlled to be E1° C./s to E2° C./s to obtain a microstructure with martensite as the main composition, wherein T=Ms−95° C., Ms represents the martensitic phase transition temperature, E1=20×(0.5−C)+15×(3.2−Mn)−8×Cr−28×Mo−4×Ni−2800×B, and E2=96×(0.45−C)+12×(4.6−Mn), and the C, Mn, Cr, Ni, B and Mo in the equations each represents the mass percentages of corresponding elements in the seamless steel tube.
STEEL PIPE FOR FUEL INJECTION PIPE, AND FUEL INJECTION PIPE USING SAME
A steel pipe for a fuel injection pipe has a chemical composition consisting of, by mass %: C: 0.17 to 0.27%, Si: 0.05 to 0.40%, Mn: 0.30 to 2.00%, P: 0.020% or less, S: 0.0100% or less, O: 0.0040% or less, Ca: 0.0010% or less, Al: 0.005 to 0.060%, N: 0.0020 to 0.0080%, Ti: 0.005 to 0.015%, Nb: 0.015 to 0.045%, Cr: 0 to 1.00%, Mo: 0 to 1.00%, Cu: 0 to 0.50%, Ni: 0 to 0.50%, V: 0 to 0.15%, and the balance: Fe and impurities. The metal micro-structure consists substantially of tempered martensite, or tempered martensite and tempered bainite. A prior-austenite grain size number is 9.0 or more. The hardness is within the range of 350 to 460 HV1. When a maximum value of a square root of an area of inclusions observed in a cross section perpendicular to a longitudinal direction of the steel pipe is taken as a.sub.n (n=1 to 20), a maximum value a.sub.max of a.sub.n is 30.0 μm or less, and an average value a.sub.av of a.sub.n is 40% or more of a.sub.max.
CROSS-ROLLING MILL WITH HYDRAULIC ROLLER ACTUATOR
A cross-rolling mill for rolling a block over a mandrel forms a hollow block. It includes a plurality of working rollers, each of which exerts a substantially radially aligned rolling force onto the block. The working rollers are supported in a roll stand, and the gap between the working rollers and preferably also the alignment of the rolling axis of at least one of the working rollers relative to the block can be modified. Hydraulic actuators, preferably hydraulic capsules, are provided in order to modify the rolling gap and preferably also the alignment of the rolling axis of at least one of the working rollers relative to the block.
CROSS-ROLLING MILL WITH HYDRAULIC ROLLER ACTUATOR
A cross-rolling mill for rolling a block over a mandrel forms a hollow block. It includes a plurality of working rollers, each of which exerts a substantially radially aligned rolling force onto the block. The working rollers are supported in a roll stand, and the gap between the working rollers and preferably also the alignment of the rolling axis of at least one of the working rollers relative to the block can be modified. Hydraulic actuators, preferably hydraulic capsules, are provided in order to modify the rolling gap and preferably also the alignment of the rolling axis of at least one of the working rollers relative to the block.
PIERCING MACHINE, MANDREL BAR, AND METHOD FOR PRODUCING SEAMLESS METAL PIPE USING THE SAME
A mandrel bar of a piercing machine includes: a bar body; a coolant channel formed inside the bar body and through which a coolant flows; an inner surface cooling mechanism which is disposed in a cooling zone and is connected to the coolant channel and which, during piercing-rolling or during elongating rolling, ejects the coolant to outside of the bar body to cool an inner surface portion of a hollow shell inside the cooling zone; and an inner surface damming mechanism which is disposed adjacent to the cooling zone on a rearward side of the cooling zone and which, during piercing-rolling or during elongating rolling, suppresses the coolant that is ejected to outside of the bar body from contacting the inner surface portion of the hollow shell that is positioned rearward of the cooling zone.
PIERCING MACHINE, MANDREL BAR, AND METHOD FOR PRODUCING SEAMLESS METAL PIPE USING THE SAME
A mandrel bar of a piercing machine includes: a bar body; a coolant channel formed inside the bar body and through which a coolant flows; an inner surface cooling mechanism which is disposed in a cooling zone and is connected to the coolant channel and which, during piercing-rolling or during elongating rolling, ejects the coolant to outside of the bar body to cool an inner surface portion of a hollow shell inside the cooling zone; and an inner surface damming mechanism which is disposed adjacent to the cooling zone on a rearward side of the cooling zone and which, during piercing-rolling or during elongating rolling, suppresses the coolant that is ejected to outside of the bar body from contacting the inner surface portion of the hollow shell that is positioned rearward of the cooling zone.
Seamless steel tube with high strength and toughness and manufacturing method therefor
A seamless steel tube with high strength and toughness, comprising the following chemical elements by mass: 0.1-0.25% of C, 0.1-0.5% of Si, 0.01-0.1% of Al, 0.6-2% of Mn, the balance of Fe and other unavoidable impurities, wherein C+Mn/6≥0.35. Also provided is a method for preparing a seamless steel tube.
Seamless steel tube with high strength and toughness and manufacturing method therefor
A seamless steel tube with high strength and toughness, comprising the following chemical elements by mass: 0.1-0.25% of C, 0.1-0.5% of Si, 0.01-0.1% of Al, 0.6-2% of Mn, the balance of Fe and other unavoidable impurities, wherein C+Mn/6≥0.35. Also provided is a method for preparing a seamless steel tube.
PIERCER PLUG
A piercer plug with increased wear resistance is provided. A piercer plug includes: a plug body; and a sprayed coating formed on the surface of the plug body. The sprayed coating contains an iron-based alloy and oxides thereof. The chromium concentration determined by analyzing the sprayed coating with X-ray fluorescence analysis is 3 to 20 mass %.