B22D11/22

SECONDARY COOLING DEVICE AND SECONDARY COOLING METHOD FOR CONTINUOUS CASTING

What is provided is a secondary cooling device for continuous casting that is configured to cool a slab, which is sent in a casting direction, by spraying cooling water to the slab surface. The secondary cooling device for continuous casting includes a plurality of rolls disposed side by side in the vertical direction along a casting direction and a spray nozzle configured to spray the cooling water to the slab surface from between the plurality of rolls. The spray nozzle is provided such that the cooling water spray axis of the spray nozzle is inclined with respect to the major axis direction of a spray range of the cooling water on the slab surface, the major axis of the spray range is rotated upward around an axis line that is a perpendicular line to the slab surface from the spray nozzle, and the center of the spray range is positioned above a middle position between a contact position between the roll that is present above the spray nozzle and the slab surface and a contact position between the roll that is present below the spray nozzle and the slab surface.

ROLLER STAND HAVING ELASTICALLY MOUNTED SUPPORTING ROLLERS

A roller stand for a continuous billet casting machine, having a carrying frame for mounting at least one lower supporting roller and at least two lateral supporting rollers. The lateral supporting rollers are mounted elastically on the carrying frame by means of at least one passive elastic element, and have an amount of elasticity at least in a direction perpendicular to the axes of rotation of the lateral supporting rollers. A method for determining the position and/or the shape of a billet is provided. During passage through at least one roller stand, alterations in the position at least of the lateral supporting rollers relative to a reference are detected and, on the basis of this information, the shape of the billet and/or the position of the billet in relation to the center line of the billet-guide channel are/is determined.

Continuous casting mold, continuous casting device, and continuous casting method

A crack-free continuous casting mold configured so that occurrence of cracks at a casting billet can be reduced even in a case where a casting speed exceeds 500 mm/min. The continuous casting mold continuously casts a casting billet while cooling molten metal by a cooling device provided at a cooling casting mold. The cooling device includes multiple cooling nozzles configured to release coolant water to the casting billet pulled out of the cooling casting mold to cool the casting billet. Multiple ejection ports of the multiple cooling nozzles are arranged along an outer circumferential direction of a surface of the casting billet. Each ejection port has a short side and a long side, and is configured such that the long side is arranged along an axial direction of the casting billet.

Continuous casting mold, continuous casting device, and continuous casting method

A crack-free continuous casting mold configured so that occurrence of cracks at a casting billet can be reduced even in a case where a casting speed exceeds 500 mm/min. The continuous casting mold continuously casts a casting billet while cooling molten metal by a cooling device provided at a cooling casting mold. The cooling device includes multiple cooling nozzles configured to release coolant water to the casting billet pulled out of the cooling casting mold to cool the casting billet. Multiple ejection ports of the multiple cooling nozzles are arranged along an outer circumferential direction of a surface of the casting billet. Each ejection port has a short side and a long side, and is configured such that the long side is arranged along an axial direction of the casting billet.

Continuous casting mold and method for continuously casting steel

A continuous casting mold including a water-cooled copper mold having a mold copper plate including an inner wall surface, recessed portions disposed partially or entirely in a region of the inner wall surface of the water-cooled copper mold from at least a position located at a meniscus to a position located 20 mm lower than the meniscus, and material-filled layers disposed in the recessed portions with a metal or nonmetal having a thermal conductivity different from that of the mold copper plate of the water-cooled copper mold. A shape of each of the recessed portions at a surface of the mold copper plate includes a curved surface.

Method for measuring and continuously monitoring the heat transfer characteristics of a fluid in a system
11014148 · 2021-05-25 · ·

A method and apparatus for measuring quench characteristics of a fluid. The apparatus includes a probe with an energy input device electrically connected to a display unit to monitor temperature, media flow characteristics and media heat transfer characteristics. The method includes continuously measuring thermal energy transfer in a quenching media by measuring the surrounding fluid's heat transfer relative to input probe energy.

Secondary cooling method and secondary cooling device for casting product in continuous casting

A secondary cooling method and a secondary cooling device for a casting product casted in a continuous casting machine, the continuous casting machine including, in a secondary cooling zone below a mold, a plurality of pairs of support rolls that support the casting product from both sides of the casting product in a thickness direction, a cooling device being disposed between support rolls adjacent to each other along a casting direction of the continuous casting machine, the cooling device including a coolant pipe that supplies a coolant, and a coolant guide plate with a flat plate shape for spreading the coolant on the casting product, the coolant guide plate being disposed parallel to and spaced in a perpendicular direction from a surface of the casting product.

Method for casting

A method for casting that includes a.) determining a diameter (D) of a cross section of a product to be cast in meter (m), b.) determining an intended steady-state casting speed (V) of the product to be cast using direct chill casting in meter per second (m/s), c.) determining a Si content (cSi) in percent by weight based on the total weight of a melt (wt-%) for the melt to be used for casting the cast product, d.) preparing a melt comprising Zn: 5.30 to 5.9 wt-%, Mg: 2.07 to 3.3 wt-%, Cu: 1.2 to 1.45 wt-%, Fe: 0 to 0.5 wt-%, Si: according to cSi, impurities up to 0.2 wt-% each and 0.5 wt-% in total, and balance aluminium, and e.) casting the melt into the cast product having the intended diameter (D) using direct chill casting, wherein the casting is carried out using the intended steady-state casting speed (V).

Method for casting

A method for casting that includes a.) determining a diameter (D) of a cross section of a product to be cast in meter (m), b.) determining an intended steady-state casting speed (V) of the product to be cast using direct chill casting in meter per second (m/s), c.) determining a Si content (cSi) in percent by weight based on the total weight of a melt (wt-%) for the melt to be used for casting the cast product, d.) preparing a melt comprising Zn: 5.30 to 5.9 wt-%, Mg: 2.07 to 3.3 wt-%, Cu: 1.2 to 1.45 wt-%, Fe: 0 to 0.5 wt-%, Si: according to cSi, impurities up to 0.2 wt-% each and 0.5 wt-% in total, and balance aluminium, and e.) casting the melt into the cast product having the intended diameter (D) using direct chill casting, wherein the casting is carried out using the intended steady-state casting speed (V).

Production method and production apparatus of continuously cast metal rod
10974315 · 2021-04-13 · ·

Provided is a production method capable of producing a high-quality continuously cast material. A cooling liquid is supplied to each of outer peripheral surfaces of a plurality of ingots extracted in parallel from a plurality of molds to cool the plurality of ingots. Of the outer peripheral surfaces of the ingot, a region which is open and does not face another ingot is defined as an open region, and a region which faces another ingot is defined as an ingot facing region. The open region is cooled with weak cooling in which the degree of cooling by the cooling liquid in the open region is set to be less than the degree of cooling by the cooling liquid in the ingot facing region.