B22F1/103

CASTER ASSEMBLY

A caster assembly configured to process and store a material includes a reaction chamber, a storage assembly configured to store material processed in the reaction chamber, and a blower configured to process and store the material. The reaction chamber includes a vessel configured to hold the material in a melted state prior to processing and a powder generating assembly configured to receive the material from the melting vessel. The powder generating assembly includes a feeding chamber and a feeding device disposed at least partially within the feeding chamber. The feeding device includes at least one nozzle configured to inject inert fluid, where the fluid is a gas, liquid, or combination of the two into the feeding chamber and a material inlet through which the material is configured to flow into the feeding chamber to be exposed to the inert fluid, where the fluid is a gas, liquid, or combination of the two.

CASTER ASSEMBLY

A caster assembly configured to process and store a material includes a reaction chamber, a storage assembly configured to store material processed in the reaction chamber, and a blower configured to process and store the material. The reaction chamber includes a vessel configured to hold the material in a melted state prior to processing and a powder generating assembly configured to receive the material from the melting vessel. The powder generating assembly includes a feeding chamber and a feeding device disposed at least partially within the feeding chamber. The feeding device includes at least one nozzle configured to inject inert fluid, where the fluid is a gas, liquid, or combination of the two into the feeding chamber and a material inlet through which the material is configured to flow into the feeding chamber to be exposed to the inert fluid, where the fluid is a gas, liquid, or combination of the two.

Three-dimensional printing

An example of a multi-fluid kit for three-dimensional printing includes a binder fluid and an adhesion promoter fluid. The binder fluid includes water and polymer particles in an amount ranging from about 1 wt % to about 40 wt % based on the total weight of the binder fluid. The adhesion promoter fluid includes water and an aromatic dihydrazide adhesion promoter in an amount ranging from about 0.1 wt % to about 10 wt % based on a total weight of the adhesion promoter fluid.

Three-dimensional printing

An example of a multi-fluid kit for three-dimensional printing includes a binder fluid and an adhesion promoter fluid. The binder fluid includes water and polymer particles in an amount ranging from about 1 wt % to about 40 wt % based on the total weight of the binder fluid. The adhesion promoter fluid includes water and an aromatic dihydrazide adhesion promoter in an amount ranging from about 0.1 wt % to about 10 wt % based on a total weight of the adhesion promoter fluid.

BINDER COMPOSITION FOR METAL POWDER INJECTION MOLDING
20220372282 · 2022-11-24 ·

The present invention relates to a binder composition for metal powder injection molding, and more specifically, to a binder composition for metal powder injection molding, which can be promptly debound, facilitates the setting of flow conditions in an injection process, and enables the minimization of poor debinding such as swelling, carbonization of low-molecular-weight binders, and other internal defects, during a debinding process.

The binder composition for metal powder injection molding of the present invention contains 10 to 50 wt % of a high-viscosity polyoxymethylene polymer and 50 to 90 wt % of a low-viscosity polyoxymethylene polymer.

By containing polyoxymethylenes alone, which has been produced with different viscosities, without feeding of other monomers in the polymerization process of polyoxymethylene, the binder composition for metal powder injection molding according to the present invention is more economical through low manufacturing costs compared with a conventional technique in which the rate of decomposition by a gas-phase acid is controlled by viscosity adjustment in a polymerization process, and has excellent injection characteristics and debinding/sintering characteristics compared with a technique in which polyoxymethylene and other polymer resins, such as polyolefins and polyamides, are used together.

BINDER COMPOSITION FOR METAL POWDER INJECTION MOLDING
20220372282 · 2022-11-24 ·

The present invention relates to a binder composition for metal powder injection molding, and more specifically, to a binder composition for metal powder injection molding, which can be promptly debound, facilitates the setting of flow conditions in an injection process, and enables the minimization of poor debinding such as swelling, carbonization of low-molecular-weight binders, and other internal defects, during a debinding process.

The binder composition for metal powder injection molding of the present invention contains 10 to 50 wt % of a high-viscosity polyoxymethylene polymer and 50 to 90 wt % of a low-viscosity polyoxymethylene polymer.

By containing polyoxymethylenes alone, which has been produced with different viscosities, without feeding of other monomers in the polymerization process of polyoxymethylene, the binder composition for metal powder injection molding according to the present invention is more economical through low manufacturing costs compared with a conventional technique in which the rate of decomposition by a gas-phase acid is controlled by viscosity adjustment in a polymerization process, and has excellent injection characteristics and debinding/sintering characteristics compared with a technique in which polyoxymethylene and other polymer resins, such as polyolefins and polyamides, are used together.

INJECTION MOLDING COMPOSITION, METHOD FOR PRODUCING INJECTION MOLDED BODY, AND METHOD FOR PRODUCING TITANIUM SINTERED BODY
20220371088 · 2022-11-24 ·

An injection molding composition contains a titanium-based powder containing titanium as a main component and having an average particle diameter of 15 μm or more and 35 μm or less, a ceramic powder containing a ceramic as a main material and having an average particle diameter of 1 nm or more and 100 nm or less, and an organic binder. The ceramic is an oxide-based ceramic containing an oxide as a main component, and a standard free energy of formation of the oxide at 1000° C. may be lower than a standard free energy of formation of titanium oxide at 1000° C.

INJECTION MOLDING COMPOSITION, METHOD FOR PRODUCING INJECTION MOLDED BODY, AND METHOD FOR PRODUCING TITANIUM SINTERED BODY
20220371088 · 2022-11-24 ·

An injection molding composition contains a titanium-based powder containing titanium as a main component and having an average particle diameter of 15 μm or more and 35 μm or less, a ceramic powder containing a ceramic as a main material and having an average particle diameter of 1 nm or more and 100 nm or less, and an organic binder. The ceramic is an oxide-based ceramic containing an oxide as a main component, and a standard free energy of formation of the oxide at 1000° C. may be lower than a standard free energy of formation of titanium oxide at 1000° C.

METAL PASTE FOR HYBRID ADDITIVE MANUFACTURING AND METHOD OF 3D PRINTING

Paste compositions for additive manufacturing and methods for the same are provided. The paste composition may include an organic vehicle, and one or more powders dispersed in the organic vehicle. The organic vehicle may include a solvent, a polymeric binder, a thixotropic additive, and a dispersant. The organic vehicle may be configured to provide the paste composition with a suitable viscosity. The organic vehicle may also be configured to provide a stable paste composition for a predetermined period of time.

Three-dimensional printing

An example of a method, for three-dimensional (3D) printing, includes applying a build material and patterning at least a portion of the build material. The patterning includes selectively applying a wetting amount of a binder fluid on the at least the portion of the build material and subsequently selectively applying a remaining amount of the binder fluid on the at least the portion of the build material. An area density in grams per meter square meter (gsm) of the wetting amount ranges from about 2 times less to about 30 times less than area density in gsm of the remaining amount.