B23K2103/04
Method for manufacturing electroseamed metal tube
A method for manufacturing an electric resistance welded metal pipe by butting side ends of a metal strip against each other and then welding the side ends by high frequency heating to manufacture an electric resistance welded metal pipe, each side end being provided with an inner surface side corner portion located on an inner surface side of the electric resistance welded metal pipe, the method includes a step of forming an inclined surface at the inner surface side corner portion before butting the side ends of the metal strip, and wherein the side ends are butted and welded to each other such that the inclined surface remains on an excess metal of the metal pipe after electric resistance welding and a discharged metal is not welded to the excess metal.
Heat-exchanger element and method for producing a heat-exchanger element
The invention relates to a heat-exchanger element for connection to tubes of a heat exchanger, the heat-exchanger element (1, 29, 32) consisting of a plurality of components (13, 14) welded to each other, and said components (13, 14) being interconnected by electron beam welding and being part of a heat exchanger head.
Sintered product and laser marking method for sintered product
A method according to one aspect of the present disclosure is a laser marking method for a powder compact containing metal powder, which includes: a first step of scanning with laser light of first power which is weaker over a predetermined area in a surface of the powder compact, to melt and smooth inside of the predetermined area; and a second step of scanning with laser light of second power which is greater, to form a dot formed of a recess of a predetermined depth at a predetermined location in the predetermined area.
Bimetallic joining with powdered metal fillers
A method of attaching a first metal object to a second metal object is presented. The first metal object and the second metal object are dissimilar materials. The first metal object comprises an upper surface and a lower surface. The method comprises: positioning the first metal object in intimate contact with the second metal object such that the second metal object is in contact with the lower surface of the first metal object; identifying at least one attachment location on the upper surface of the first metal object where the first metal object is in intimate contact with the second metal object; adding a powdered metal on the upper surface of the first metal object at the at least one attachment location; and firing a heat source at the powdered metal to melt the powdered metal and drive the melted powdered metal through the first metal object and into the second metal object.
ULTRASONIC ADDITIVE MANUFACTURING OF CLADDED AMORPHOUS METAL PRODUCTS
An embodiment relates to an ultrasonic additive manufacturing process, comprising joining a foil comprising a bulk metallic glass to a substrate; and forming a cladded composite comprising the foil and the substrate; wherein a thickness of the cladded composite is greater than a critical casting thickness of the bulk metallic glass, wherein the cladded composite comprises a cladding layer of the bulk metallic glass on the substrate and the bulk metallic glass comprises approximately 0% crystallinity, approximately 0% porosity, less than 50 MPa thermal stress, approximately 0% distortion, approximately 0 inch heat affected zone, approximately 0% dilution, and a strength of about 2,000-3,500 MPa.
GRAIN-ORIENTED ELECTRICAL STEEL SHEET AND MAGNETIC DOMAIN REFINEMENT METHOD THEREOF
A grain-oriented electrical steel sheet according to an embodiment of the present invention has an average degree of orientation difference of 0.5 to 10° between recrystallized grains that are in contact with a groove present on the surface of the electrical steel sheet and the bottom of the groove, and other recrystallized grains.
Methods for producing a three-dimensional vehicle door frame inner reinforcement element, for producing a vehicle door frame and for producing a vehicle reinforcement structure
A method is for producing a three-dimensional vehicle door frame inner reinforcement element (52) including an inner center pillar part (66), an inner front pillar part (68) and an inner side rail part (64) joining the inner center pillar part (66) and the inner front pillar part (68). The method includes providing an inner center pillar blank, an inner front pillar blank and an inner side rail blank, said inner blanks being substantially planar, assembling the inner center pillar blank and the inner front pillar blank to the inner side rail blank in order to form a substantially planar door frame inner reinforcement blank, and hot stamping the door frame inner reinforcement blank to shape the three-dimensional door frame inner reinforcement element (52).
Laser processing apparatus
In a laser processing apparatus for refining magnetic domains of a grain-oriented electromagnetic steel sheet by setting a laser beam to be focused on the grain-oriented electromagnetic steel sheet and scanned in a scanning direction, the laser beam focused on the grain-oriented electromagnetic steel sheet is linearly polarized light, and an angle between a linear polarization direction and the scanning direction is higher than 45° and equal to or lower than 90°.
Lap fillet arc welding joint
The present invention provides a lap fillet arc welding joint including a first metal sheet, a second metal sheet, and a weld bead. A region of the first metal sheet on one end side is bent. In a first direction, a position of a tip end of the bent region of the first metal sheet overlaps a region of the second metal sheet on one end side. In a second direction, an amount of deviation between a central axis of a region connected to the bent region of the first metal sheet and a central axis of the region of the second metal sheet on one end side is ½ times or less of average sheet thicknesses of the first metal sheet and the second metal sheet. A joint portion length is two times or more of the sheet thickness of the second metal sheet.
Resistance spot welding method
Main current passage and subsequent current passage are performed, with a cooling time of 0.01 s or more being provided between the main current passage and the subsequent current passage. Ip/I which is a ratio of a current value of the subsequent current passage to a current value of the main current passage is controlled to satisfy a predetermined relationship depending on a constant A defined by Mn content and P content of a steel sheet as a part to be welded, in relation to a welding time Tp of the subsequent current passage, a cooling time T, and the constant A.