B29C41/04

DEVICE FOR PRODUCING PLASTIC BODIES
20230202077 · 2023-06-29 ·

The device relates to a device for producing plastic bodies wherein the device comprises a photopolymer curing unit comprising at least one radiation source with a selected radiation spectrum or spectrums for curing of light hardening photopolymer, a mold which mold is partially or wholly comprised of light transmissive material which material allows the passage of radiation of selected spectrum or spectrums for curing of light hardening photopolymers, and a fixture for securing and rotating the mold along one or more axis.

Light hardening photopolymer is introduced into the cavity of the mold and exposed to a selected radiation spectrum or spectrums for curing of light hardening photopolymers through the mold light transmissive material thereby hardening and curing the light hardening photopolymer whereupon the cured light hardening photopolymer is removed from the mold and the process repeated.

The device permits the production of photopolymer molded bodies or photopolymer coated bodies in a continuous or discontinuous process.

APPARATUS FOR MANUFACTURING THIN-WALLED BODIES OF REVOLUTION

The technical solution relates to the field of processing polymers and can be used in various branches of the national economy for manufacturing hollow articles of the bodies-of-revolution type (tubes), and in particular for manufacturing semifinished biodegradable polymeric stents which are usable in medicine for replacing hollow organs, for example blood vessels. The apparatus for manufacturing thin-walled bodies of revolution comprises a heatable expander which is mounted rotatably about a longitudinal axis, and a feeder for supplying mouldable material, said feeder being mounted above the expander so as to be movable therealong, wherein the lower part of the feeder is heatable, the expander is hollow with a reflective internal surface, and the heater of the expander is in the form of a laser, the radiation of which is transported into the expander. The use of the apparatus will make it possible to reduce the thermal action on a polymer when producing semi-finished articles with defined geometrical dimensions from polymeric materials.

METHOD OF MANUFACTURING INTRAMEDULLARY NAILS MADE OF CHITOSAN FOR LONG BONES FRACTURES TREATMENT

The method, characterized in that, the powdered chitosan is dissolved in water to obtain a 5% solution, into which a 70-90% acetic acid is added and after the formation of the blank intramedullary nail and carrying a coagulating bath and neutralization bath it is subjected to a crosslinking bath in a solution formed from 0.5 to 2% of sodium tri-polyphosphate and 0.5% to 3% Na3PO4 for 24 to 48 hours in temperature of 50° C. to 140° C. and then it is subjected to the drying process, for a period of 6 to 10 days, and finally the surface of the blank is treated to form the intramedullary nail. The surface treatment is carried out until the surface of the intramedullary nail contains at least 20%-40% of the pore of the depth of 0.1 mm to 1 mm.

METHOD OF MANUFACTURING INTRAMEDULLARY NAILS MADE OF CHITOSAN FOR LONG BONES FRACTURES TREATMENT

The method, characterized in that, the powdered chitosan is dissolved in water to obtain a 5% solution, into which a 70-90% acetic acid is added and after the formation of the blank intramedullary nail and carrying a coagulating bath and neutralization bath it is subjected to a crosslinking bath in a solution formed from 0.5 to 2% of sodium tri-polyphosphate and 0.5% to 3% Na3PO4 for 24 to 48 hours in temperature of 50° C. to 140° C. and then it is subjected to the drying process, for a period of 6 to 10 days, and finally the surface of the blank is treated to form the intramedullary nail. The surface treatment is carried out until the surface of the intramedullary nail contains at least 20%-40% of the pore of the depth of 0.1 mm to 1 mm.

METHODS FOR MAKING INFLATABLE INTERIOR PANEL ARRANGEMENTS FOR MOTOR VEHICLES
20170355107 · 2017-12-14 ·

Methods for making inflatable interior panel arrangements for motor vehicles are provided. In one example, a method for making inflatable interior panel arrangement for a motor vehicle includes introducing a molding material into a molding tool that has tooling surfaces. The molding material is contacted with a first tooling surface of the tooling surfaces having a tooling surface temperature different than tooling surface tempe. The molding tool is closed such that the tooling surfaces define a substantially enclosed cavity in the molding tool. An inflatable interior panel is formed comprising rotating the molding tool to cover the tooling surfaces of the substantially enclosed cavity with the molding material. The inflatable interior panel comprises an inflatable bladder section and an outer panel section that is integrally coupled to the inflatable bladder section and that has a panel portion stiffness greater than a bladder portion stiffness of the inflatable bladder section.

METHOD AND FIXTURE FOR MOLDING A TANK WITH AN EMBEDDED RING
20230182352 · 2023-06-15 ·

A method of and fixture for molding a product with an embedded ring. A system for molding a ring into a product including a rotational molding mold with an opening formed in the rotational molding mold sized to fit a ring. A fixture is removably couplable to the ring, wherein the ring and the fixture when coupled are removably couplable in the opening. The fixture is removed from the ring after the ring is molded into a product. A method of manufacturing a product with an embedded ring includes: coupling a ring to a fixture; clamping the fixture and the ring in an opening in a mold top; clamping the mold top to a mold bottom; rotomolding a product; unclamping the fixture from the mold top; uncoupling the fixture from the ring; unclamping the mold top and the mold bottom; and removing the product from the mold.

METHOD AND FIXTURE FOR MOLDING A TANK WITH AN EMBEDDED RING
20230182352 · 2023-06-15 ·

A method of and fixture for molding a product with an embedded ring. A system for molding a ring into a product including a rotational molding mold with an opening formed in the rotational molding mold sized to fit a ring. A fixture is removably couplable to the ring, wherein the ring and the fixture when coupled are removably couplable in the opening. The fixture is removed from the ring after the ring is molded into a product. A method of manufacturing a product with an embedded ring includes: coupling a ring to a fixture; clamping the fixture and the ring in an opening in a mold top; clamping the mold top to a mold bottom; rotomolding a product; unclamping the fixture from the mold top; uncoupling the fixture from the ring; unclamping the mold top and the mold bottom; and removing the product from the mold.

THREE-AXIS ROTATIONAL MOULDING MACHINE
20230166429 · 2023-06-01 · ·

Rotational moulding machine (1) comprising a fixed frame (2), a support arm (3) comprising a first (4) and a second portion (5) rigidly joined together, the support arm (3) being rotationally fixed to the fixed frame (2) only at the first portion (4) to rotate about a first axis of rotation (101) substantially horizontal, a movable frame (6) rotationally fixed to the support arm (3) to rotate about a second axis of rotation (102) substantially perpendicular to the first axis of rotation (101), the movable frame (6) comprising a supporting portion (7) lying in a plane substantially perpendicular to the second axis of rotation (102), and an actuation system (8) rigidly fixed to the movable frame (6) at the supporting portion (7) and structured to secure a mould (20) and rotate the mould (20) about a third axis of rotation (103) substantially perpendicular to the second axis of rotation (102).

Rotomolded Articles Comprising at Least One Layer Comprising a Metallocene-Catalyzed Polyethylene Resin
20170313863 · 2017-11-02 ·

The present invention relates to a rotomolded article, comprising at least one layer, wherein said at least one layer comprising comprises at least one metallocene-catalyzed polyethylene resin comprising at least two metallocene-catalyzed polyethylene fractions A and B; and at least one ionomer;

wherein the polyethylene resin comprises: at least 25% to at most 55% by weight of polyethylene fraction A based on the total weight of the polyethylene resin, wherein fraction A has a density at least 0.005 g/cm.sup.3 higher than the density of the polyethylene resin; and wherein the polyethylene resin has a density of at least 0.930 g/cm.sup.3 to at most 0.954 g/cm.sup.3 as measured according to ASTM D-1505 at 23° C.; a melt index MI2 of at least 1.0 g/10 min to at most 25.0 g/10 min as determined according to ISO 1133, condition D, at 190° C. and under a load of 2.16 kg.

The present invention also relates to a process for preparing said rotomolded article.

Rotomolded Articles Comprising at Least One Layer Comprising a Metallocene-Catalyzed Polyethylene Resin
20170313863 · 2017-11-02 ·

The present invention relates to a rotomolded article, comprising at least one layer, wherein said at least one layer comprising comprises at least one metallocene-catalyzed polyethylene resin comprising at least two metallocene-catalyzed polyethylene fractions A and B; and at least one ionomer;

wherein the polyethylene resin comprises: at least 25% to at most 55% by weight of polyethylene fraction A based on the total weight of the polyethylene resin, wherein fraction A has a density at least 0.005 g/cm.sup.3 higher than the density of the polyethylene resin; and wherein the polyethylene resin has a density of at least 0.930 g/cm.sup.3 to at most 0.954 g/cm.sup.3 as measured according to ASTM D-1505 at 23° C.; a melt index MI2 of at least 1.0 g/10 min to at most 25.0 g/10 min as determined according to ISO 1133, condition D, at 190° C. and under a load of 2.16 kg.

The present invention also relates to a process for preparing said rotomolded article.