Patent classifications
B29C48/06
Apparatus for correcting the bending of a molten resin and method of correcting the bending of the molten resin
An apparatus (31) for correcting the bending of the molten resin includes a temperature-adjusting device (32) arranged surrounding an extrusion passage (12) for extruding the molten resin (8) of an extrusion die head (7) along the direction of extruding the molten resin (8), a measuring means (33) for measuring the horizontal position of the molten resin (8) extruded from an extrusion opening (20) of the extrusion passage (12), and a control means (34) for controlling the temperature-adjusting device (32) based on the results measured by the measuring means (33).
METHOD FOR PRODUCING A PET STARTING MATERIAL THAT IS SUITABLE FOR USE IN AN EXTRUSION BLOW MOLDING METHOD, AND HOLLOW ARTICLE PRODUCED IN THE EXTRUSION BLOW MOLDING METHOD
The invention relates to a method for producing an EBM bottle with 0.90 to 1.5 dL/g from a bottle-grade PET post-consumer recycling flake, i.e., a recycled, post-consumer PET with a viscosity of 0.65 to 0.84 dL/g, using extrusion processes, solid state polycondensation processes, and a blowing process.
METHOD FOR PRODUCING A PET STARTING MATERIAL THAT IS SUITABLE FOR USE IN AN EXTRUSION BLOW MOLDING METHOD, AND HOLLOW ARTICLE PRODUCED IN THE EXTRUSION BLOW MOLDING METHOD
The invention relates to a method for producing an EBM bottle with 0.90 to 1.5 dL/g from a bottle-grade PET post-consumer recycling flake, i.e., a recycled, post-consumer PET with a viscosity of 0.65 to 0.84 dL/g, using extrusion processes, solid state polycondensation processes, and a blowing process.
COMPRESSION MOULDING MACHINE AND METHOD
A compression moulding machine comprises: an extrusion unit configured to extrude a rod of pasty polymeric material; a cutting element, configured to portion the rod into individual charges; a rotary carousel, including a plurality of moulds, each mould being configured to receive a respective charge and to form a corresponding object from the charge; a feeder, configured to convey each charge to a respective mould at a feed position; an inspecting device, configured to capture inspection data, representing a composition of the rod or of the charges.
LOW COST EXTRUDABLE ISOLATOR FROM SLIT-TAPE
A dielectric isolator for a twisted pair cable includes a body formed as an elongate strip with a top surface, bottom surface, a first side edge and a second side edge. A first slot is formed in the first side edge and extends at least half way toward the center of the isolator. A second slot is formed in the second side edge and extends at least half way toward the center of the isolator. During cable manufacturing, first and second wedges open the first and second slots. First and second twisted pairs are inserted into the first and second opened slots, respectively. Third and fourth twisted pairs reside at the top and bottom surface, respectively. The isolator has the cost and reel storage savings of a flat separator tape, while simultaneously providing the internal crosstalk performance of the isolator.
LOW COST EXTRUDABLE ISOLATOR FROM SLIT-TAPE
A dielectric isolator for a twisted pair cable includes a body formed as an elongate strip with a top surface, bottom surface, a first side edge and a second side edge. A first slot is formed in the first side edge and extends at least half way toward the center of the isolator. A second slot is formed in the second side edge and extends at least half way toward the center of the isolator. During cable manufacturing, first and second wedges open the first and second slots. First and second twisted pairs are inserted into the first and second opened slots, respectively. Third and fourth twisted pairs reside at the top and bottom surface, respectively. The isolator has the cost and reel storage savings of a flat separator tape, while simultaneously providing the internal crosstalk performance of the isolator.
DEVICE AND METHOD FOR COATING A THREAD
A device for coating a thread with a coating material includes a housing, a die body, and a supply line for the coating material. The housing includes a support and a cover mounted on the support, delimiting a chamber. The die body is installed in the chamber, between the support and the cover. The die body includes a lower part and an upper part, with a calibrated die channel being located between the lower and upper parts. Between the support and the cover are an inlet through passage and an outlet through passage. The inlet and outlet passages and the die channel are aligned, so that a thread is able to be passed longitudinally therethrough. The supply line for the coating material includes a lower outlet end located close to the thread, between the inlet or upstream through passage and the die channel.
Cable made from crosslinkable composition with antioxidant and beneficial methane formation
The invention relates to a cable comprising layer(s), which layer(s) is/are obtained from a polymer composition comprising a polyethylene, a crosslinking agent and antioxidant(s), characterized in that the polymer composition contains a total amount of vinyl groups which is B vinyl groups per 1000 carbon atoms, and B.sub.1≤B, wherein B.sub.1 is 0.12, when measured prior to crosslinking according to method ASTM D6248-98, the crosslinking agent is present in an amount which is Z wt %, prior to crosslinking, based on the total amount (100 wt %) of the polymer composition, and Z.sub.1≤Z≤Z.sub.2, wherein Z.sub.1 is 0.005 and Z.sub.2 is 2.0, and that the antioxidant(s) is/are nitrogen containing antioxidant(s) being present in an amount which is W wt %, prior to crosslinking, based on the total amount (100 wt %) of the polymer composition, and W.sub.1≤W≤W.sub.2, wherein W.sub.1 is 0.005 and W.sub.2 is 1.0, the cable, e.g. a power cable, and processes for producing the cable; the cable useful in different end applications, such as wire and cable (W&C) applications.
Cable made from crosslinkable composition with antioxidant and beneficial methane formation
The invention relates to a cable comprising layer(s), which layer(s) is/are obtained from a polymer composition comprising a polyethylene, a crosslinking agent and antioxidant(s), characterized in that the polymer composition contains a total amount of vinyl groups which is B vinyl groups per 1000 carbon atoms, and B.sub.1≤B, wherein B.sub.1 is 0.12, when measured prior to crosslinking according to method ASTM D6248-98, the crosslinking agent is present in an amount which is Z wt %, prior to crosslinking, based on the total amount (100 wt %) of the polymer composition, and Z.sub.1≤Z≤Z.sub.2, wherein Z.sub.1 is 0.005 and Z.sub.2 is 2.0, and that the antioxidant(s) is/are nitrogen containing antioxidant(s) being present in an amount which is W wt %, prior to crosslinking, based on the total amount (100 wt %) of the polymer composition, and W.sub.1≤W≤W.sub.2, wherein W.sub.1 is 0.005 and W.sub.2 is 1.0, the cable, e.g. a power cable, and processes for producing the cable; the cable useful in different end applications, such as wire and cable (W&C) applications.