B29C55/18

Apparatus for longitudinal orientation of thermoplastic film material

Apparatus for longitudinal orientation of thermoplastic film material (4) comprises a width-reduction zone upstream of the longitudinal stretching zone, through which the width of the film is gradually reduced so as to allow longitudinal stretching without necking. The width-reduction zone comprises at least one, preferably several, pairs of pleating rollers (16, 17) comprising intermeshing grooves or discs for pleating the material, the length of said width reduction zone preferably being less than 3 times the original width of the film. The width-reducing zone has upstream (14) and downstream (15) rollers or roller assemblies, with curved axes and optionally also conveyor belts for providing smooth width reduction. Longitudinal stretching is preferably between at least two, and preferably more than two, pairs of stretching rollers (9, 10, 11, 12) which are relatively close together. The pleats may be provided in several stages with increasing pleats per stage, while guiding means preferably lay all the pleats to one side. The apparatus allows achievement of high tensile strength, yield point, resistance to tear propagation and puncture resistance, especially for polyethylene and polypropylene films.

Apparatus for longitudinal orientation of thermoplastic film material

Apparatus for longitudinal orientation of thermoplastic film material (4) comprises a width-reduction zone upstream of the longitudinal stretching zone, through which the width of the film is gradually reduced so as to allow longitudinal stretching without necking. The width-reduction zone comprises at least one, preferably several, pairs of pleating rollers (16, 17) comprising intermeshing grooves or discs for pleating the material, the length of said width reduction zone preferably being less than 3 times the original width of the film. The width-reducing zone has upstream (14) and downstream (15) rollers or roller assemblies, with curved axes and optionally also conveyor belts for providing smooth width reduction. Longitudinal stretching is preferably between at least two, and preferably more than two, pairs of stretching rollers (9, 10, 11, 12) which are relatively close together. The pleats may be provided in several stages with increasing pleats per stage, while guiding means preferably lay all the pleats to one side. The apparatus allows achievement of high tensile strength, yield point, resistance to tear propagation and puncture resistance, especially for polyethylene and polypropylene films.

ULTRA LARGE-WIDTH AND CONSECUTIVE COATING DEVICE AND METHOD FOR MANUFACTURING MEMBRANE USING THE SAME

Provided is an ultra large-width coating device applied to a consecutive process. More particularly, the present invention relates to a coating device capable of maximizing productivity by consecutively manufacturing a large-width film without reducing physical properties of the manufactured film by overcoming a problem in that a coating width is limited during a coating process using the existing contact type coating roller, and a method for manufacturing an ultra large-width membrane using the same.

ULTRA LARGE-WIDTH AND CONSECUTIVE COATING DEVICE AND METHOD FOR MANUFACTURING MEMBRANE USING THE SAME

Provided is an ultra large-width coating device applied to a consecutive process. More particularly, the present invention relates to a coating device capable of maximizing productivity by consecutively manufacturing a large-width film without reducing physical properties of the manufactured film by overcoming a problem in that a coating width is limited during a coating process using the existing contact type coating roller, and a method for manufacturing an ultra large-width membrane using the same.

METHOD FOR PRODUCING PRINTED NONWOVEN-FILM LAMINATES
20210237418 · 2021-08-05 ·

The invention relates to a method for producing a printed nonwoven film laminate from a starting film web of a thermoplastic polymer material and a starting nonwoven web, wherein the melting point of the starting nonwoven web is above the crystallite melting point of at least one component of the polymer material of the starting film web. The method includes at least partially coating the starting film web with a printing ink and with an adhesion promoter; heating the coated film web together with the starting nonwoven web to a temperature which is above the crystallite melting point of the at least one component of the polymer material of the starting film web and of the adhesion promoter and below the crystallite melting point of the starting nonwoven web, to obtain a laminate; and cooling the laminate obtained through a cooled roller nip. Furthermore, the invention relates to printed nonwoven film laminates produced by the method and their use.

Method of manufacturing an activated composite web and an activated composite web for absorptive devices

A method of manufacturing an activated composite web includes laminating a film layer to a nonwoven web to form a composite web, forming a plurality of apertured protuberances in the film layer, and passing the composite web through intermeshing elements to form an activated composite web. The intermeshing elements form a plurality of first lanes, with first widths, substantially unaffected by activation, and a plurality of second lanes, with second widths. The second widths are less than the first widths. Portions of the plurality of apertured protuberances define first apertures in the first lanes and second apertures in the second lanes. The cross-sections of the second apertures are larger than the first apertures. The first apertures have their major axes substantially aligned in the first direction while the second apertures have their major axis substantially aligned in the second direction. An activated composite web also is provided.

Method of manufacturing an activated composite web and an activated composite web for absorptive devices

A method of manufacturing an activated composite web includes laminating a film layer to a nonwoven web to form a composite web, forming a plurality of apertured protuberances in the film layer, and passing the composite web through intermeshing elements to form an activated composite web. The intermeshing elements form a plurality of first lanes, with first widths, substantially unaffected by activation, and a plurality of second lanes, with second widths. The second widths are less than the first widths. Portions of the plurality of apertured protuberances define first apertures in the first lanes and second apertures in the second lanes. The cross-sections of the second apertures are larger than the first apertures. The first apertures have their major axes substantially aligned in the first direction while the second apertures have their major axis substantially aligned in the second direction. An activated composite web also is provided.

Patterned substrates

Patterned substrates having a first substrate region that is incrementally mechanically stretched with corrugations and a second substrate region having a plurality of discrete unstretched portions completely surrounded by the first substrate region.

Polymer Nanocomposites and Methods of Making the Same
20210179807 · 2021-06-17 ·

A method of fabricating a polymer composite material by mixing a polymer material with a planar material, depositing the mixture on a substrate, and stretching the resulting thin film, is described. Polymer composite materials produced using said method and ballistic resistant materials comprising said polymer composite materials are also described.

Polymer Nanocomposites and Methods of Making the Same
20210179807 · 2021-06-17 ·

A method of fabricating a polymer composite material by mixing a polymer material with a planar material, depositing the mixture on a substrate, and stretching the resulting thin film, is described. Polymer composite materials produced using said method and ballistic resistant materials comprising said polymer composite materials are also described.