Patent classifications
B32B7/12
Heat bonding of low energy surface substrates
A method comprising providing a polymeric substrate having a melting point of from about 130° C. to about 190° C., and locating a material layer onto the substrate, wherein the material layer comprises one or more polymeric materials that liquefy upon exposure to temperatures of at least about 100° C., to blend with a softened portion of the polymeric substrate. Upon exposure of one or more of the substrate and the material layer to a stimulus, the temperature is increased in a predetermined temperature zone of one or more of the substrate and material layer to cause blending of the one or more polymeric materials of the material layer with the softened portion of the polymeric substrate.
Oxygen-tight food container
The invention relates to a food packaging unit (20) comprising a food container (1) for receiving a liquid, pasty or free-flowing food. The injection-moulded, single-component, cup-shaped base body (2) of the food container surrounds, with a wall (5), a bottom (6) and an outwardly projecting collar (7), an opening (4) which is closed by a food-container-covering film (10) applied to the collar (7). The food container (1) is injection-moulded in a single layer from a polymer blend comprising two components, a first component of which being PVOH or a PVOH copolymer. The food-container-covering film (10), which can be applied to the plastic food container (1) in order to close the opening (4) by sealing, welding or adhesion, comprises a cellulose-containing layer which is coated with PVOH, or a PVOH polymer blend layer.
Oxygen-tight food container
The invention relates to a food packaging unit (20) comprising a food container (1) for receiving a liquid, pasty or free-flowing food. The injection-moulded, single-component, cup-shaped base body (2) of the food container surrounds, with a wall (5), a bottom (6) and an outwardly projecting collar (7), an opening (4) which is closed by a food-container-covering film (10) applied to the collar (7). The food container (1) is injection-moulded in a single layer from a polymer blend comprising two components, a first component of which being PVOH or a PVOH copolymer. The food-container-covering film (10), which can be applied to the plastic food container (1) in order to close the opening (4) by sealing, welding or adhesion, comprises a cellulose-containing layer which is coated with PVOH, or a PVOH polymer blend layer.
Method for producing printed material and system for producing printed material
A method for producing a printed material includes providing pressure-induced phase transition particles on a recording medium having an arithmetic average roughness Ra of 0.07 μm or more and 3.80 μm or less to form a pressure-induced phase transition particle layer having a coverage C within a range of 30% to 90%; bonding the pressure-induced phase transition particles onto the recording medium; and folding the recording medium having the pressure-induced phase transition particles bonded thereon and pressure-bonding the folded recording medium, or pressure-bonding the recording medium having the pressure-induced phase transition particles bonded thereon and another recording medium placed on top of each other. The pressure-induced phase transition particles have at least two glass transition temperatures, and the difference between the lowest glass transition temperature and the highest glass transition temperature among the glass transition temperatures exhibited by the pressure-induced phase transition particles is 30° C. or more.
Method for producing printed material and system for producing printed material
A method for producing a printed material includes providing pressure-induced phase transition particles on a recording medium having an arithmetic average roughness Ra of 0.07 μm or more and 3.80 μm or less to form a pressure-induced phase transition particle layer having a coverage C within a range of 30% to 90%; bonding the pressure-induced phase transition particles onto the recording medium; and folding the recording medium having the pressure-induced phase transition particles bonded thereon and pressure-bonding the folded recording medium, or pressure-bonding the recording medium having the pressure-induced phase transition particles bonded thereon and another recording medium placed on top of each other. The pressure-induced phase transition particles have at least two glass transition temperatures, and the difference between the lowest glass transition temperature and the highest glass transition temperature among the glass transition temperatures exhibited by the pressure-induced phase transition particles is 30° C. or more.
Vacuum skin package having implosion-resistant top web
A packaged product has a product surrounded by a vacuum skin package. The vacuum skin package has a support member and an implosion-resistant thermoplastic top web. The top web conforms with both the upper surface of the product, and an uncovered portion of the upper surface of the support member. The thermoplastic top web comprises an ethylene/α-olefin copolymer in an amount of from 55 wt % to 85 wt %, based on total weight of top web, and/or a blend of ethylene/α-olefin copolymer and cyclic olefin copolymer. Also disclosed is a vacuum skin package containing the implosion-resistant top web.
Vacuum skin package having implosion-resistant top web
A packaged product has a product surrounded by a vacuum skin package. The vacuum skin package has a support member and an implosion-resistant thermoplastic top web. The top web conforms with both the upper surface of the product, and an uncovered portion of the upper surface of the support member. The thermoplastic top web comprises an ethylene/α-olefin copolymer in an amount of from 55 wt % to 85 wt %, based on total weight of top web, and/or a blend of ethylene/α-olefin copolymer and cyclic olefin copolymer. Also disclosed is a vacuum skin package containing the implosion-resistant top web.
Ballistic protection material and use thereof
The present invention relates to a protective material, preferably a ballistic protection material, having a protective function against ballistic active bodies (launch bodies), in particular against reinforcement-penetrating and/or armor-piercing projectiles, thrust bodies or penetrating bodies, and to the use thereof.
Inflation and sealing device with web control
The present disclosure is directed to a web control guide for an inflation and sealing assembly of a protective packaging formation device for inflating a web material into a chain of inflated cushions. The web control guide is positioned along a material path at a transverse spacing from a first compression element and constrains a first thickness of the material path measured normal to the longitudinal and transverse directions of the material path. The transverse spacing and constrained thickness dimension are sufficiently small to prevent transverse movement of the flexible material towards the first compression element to avoid excessive heating of the web material outside a sealing zone.
Method of manufacturing curved thin glass sheet having functional layer and method of manufacturing curved joined glass sheet having functional layer
The present invention relates to a method capable of easily manufacturing a curved thin glass sheet and a curved joined glass sheet to which functionality is added.