Patent classifications
B32B25/08
POLARIZING FILM LAMINATE
Provided is a polarizing film laminate that is reworkable and excellent in bonding property over a long period of time. The polarizing film laminate includes: a polarizing plate including a polarizer; a first pressure-sensitive adhesive layer; a supporting substrate; and a second pressure-sensitive adhesive layer, which are laminated in the stated order, wherein the second pressure-sensitive adhesive layer surface of the polarizing film laminate has a pressure-sensitive adhesive strength to glass of 1.0 N/25 mm or more at a peel angle of 90° and a peel rate of 300 mm/min.
BARRIER LAMINATE FILMS FOR LAP SEALS
A multilayer laminate (100) comprises an oriented polyethylene film (102), a biaxially oriented film (104) adhered to the oriented polyethylene film (102), a barrier film (106) adhered to the biaxially oriented film (104), and a multilayer polyethylene (PE) film (108) adhered to the barrier film (106). The biaxially oriented film (104) comprises one or more components selected from biaxially oriented polyamide (BOPA), biaxially oriented polyethylene terephthalate (BOPET), and biaxially oriented polypropylene (BOPP).
PIPE FOR CONVEYING FLUIDS IN HVACR SYSTEMS
The present invention relates to a composite coating for an inner tube delimiting a passageway for a fluid for obtaining a pipe for conveying fluids in HVACR systems.
Method of making a multilayered elastomeric article
Elastomeric articles, such as gloves, made from more than one layer, are provided. The gloves can include a first (grip side) layer in which a first colorant is compounded or integrated and a second (donning side) layer in which a second colorant is compounded or integrated. Alternatively, the gloves can include a translucent first layer and a second layer in which a colorant is compounded or integrated. Either arrangement can enable a breach of the first layer to be more easily detected, either due to the high level of contrast between the first layer and the second when a first colorant and a second colorant are utilized, or due to the translucence of the first layer as compared to the donning side layer, where the intensity of the second layer is increased upon a breach of the translucent first layer.
Method of making a multilayered elastomeric article
Elastomeric articles, such as gloves, made from more than one layer, are provided. The gloves can include a first (grip side) layer in which a first colorant is compounded or integrated and a second (donning side) layer in which a second colorant is compounded or integrated. Alternatively, the gloves can include a translucent first layer and a second layer in which a colorant is compounded or integrated. Either arrangement can enable a breach of the first layer to be more easily detected, either due to the high level of contrast between the first layer and the second when a first colorant and a second colorant are utilized, or due to the translucence of the first layer as compared to the donning side layer, where the intensity of the second layer is increased upon a breach of the translucent first layer.
Resin composition, production method for resin composition, and molded body using resin composition
There is provided a resin composition, comprising an ethylene-vinyl alcohol copolymer and a nonionic surfactant, wherein the ethylene-vinyl alcohol copolymer has an ethylene unit content of 15 to 60 mol %, and a saponification degree of 90 mol % or more; the ethylene-vinyl alcohol copolymer is contained as a major component; and the nonionic surfactant is contained at 3 to 400 ppm. The resin composition is produced by melt-kneading a mixture comprising the nonionic surfactant, water and the ethylene-vinyl alcohol copolymer. By using the resin composition thus produced, a discharge amount during melt molding can be increased and a molded article with an excellent appearance can be provided.
Photovoltaic module frontsheet and backsheet
A photovoltaic module includes at least one solar cell, an encapsulant encapsulating the at least one solar cell, a frontsheet juxtaposed with the encapsulant, and backsheet juxtaposed with the encapsulant. The frontsheet includes a glass layer, a polymer layer attached to the glass layer, and an adhesive layer attaching the polymer layer to the glass layer. The backsheet includes a single-layer, moisture-resistant, fire-retardant membrane.
DEVICE FOR EXTINGUISHING FIRE OR LIMITING FIRE OUTBREAKS
A fire extinguishing device is for a motor vehicle. The fire extinguishing device includes an internal cavity containing a pressurized fire extinguishing fluid. The cavity is delimited by a wall, the wall having at least one barrier layer (b) containing a semi-aromatic polyamide composition (B).
Method for manufacturing fluid device composite member
A fluid device composite member includes: a silicone member that includes a body part which is made of silicone and which has a flow-path-defining section for defining a flow path on one surface of the body part, and that includes barrier layer having hydrophilicity or hydrophobicity disposed in at least a portion of the flow-path-defining section; and a resin substrate disposed on another surface of the body part opposite to the one surface. This method for manufacturing the fluid device composite member includes a layered body manufacturing step in which a liquid silicone material is placed on a surface of the resin substrate, and the liquid silicone material is cured at a temperature of 100° C. or less to obtain a layered body in which a silicone cured product is bonded to the resin substrate.
Elastomeric films having low tear propagation
Multilayer thermoplastic films, and laminates and articles comprising the films, wherein the film comprises at least one inner layer and at least two outer layers, wherein the inner layer comprises a polymeric composition comprising from about 55% to about 95% of one or more non-hydrogenated styrenic block copolymers, olefinic block copolymers, or combinations thereof; and each outer layer comprises at least 20% polypropylene and has a thickness of from about 5% to about 15% of the total film thickness, and further wherein the film has a constant force tear propagation of about 20% or less.