B32B2255/205

Method for applying a polymeric film to a substrate and resulting articles
11548272 · 2023-01-10 · ·

A polymeric film assembly comprising a first solidified interlayer on a polymeric film or laminate comprising the same that is contacted with at least a portion of a surface of an underlying article to provide, for example, desired surface characteristics. At least a portion of the first solidified interlayer becomes a softened interlayer positioned between the polymeric film and the surface of the article when contacted as such. The softened interlayer is then converted to a second solidified interlayer, which second solidified interlayer may be in a different form than or same form as the first solidified interlayer initially provided, for adherence of the polymeric film to at least the portion of the surface of the article. Ease of removal and/or repair of polymeric film and laminates comprising the polymeric film that are so applied is facilitated.

Display Apparatus and Method for Manufacturing the Same
20230217604 · 2023-07-06 ·

Disclosed is a display apparatus including a display panel and a cushion plate disposed under the display panel. The cushion plate may include a porous member and a reinforcing plate. A step in a side area of the display apparatus may be removed, thereby improving impact absorption ability and rigidity.

Tubular container with invisible longitudinal overlapped side seam
11691791 · 2023-07-04 · ·

A laminate tube with an invisible longitudinal overlapped side seam formed from overlap welding an edge of one margin of a laminate sheet comprising an outer plastic layer (A), a barrier layer (B), and an inner plastic layer (C) of the same material type as the outer plastic layer (A) to the other edge of the opposite margin of the laminate sheet, such that an inner surface of the laminate tube has a hump in a overlapped region, while an outer surface of the laminate tube is smooth without a hump in the overlapped region; and a process for manufacturing the laminate tube by a laminate tube manufacturing machine. The laminate permits fracture-proof welding of longitudinal margins of said laminate to give a continuous tube which is suitable for manufacturing of high-quality plastic tubes, high-quality plastic bags and the like.

Self-adhesive membrane for mitigating passive intermodulation

Materials and methods for mitigating passive intermodulation. A membrane for reducing passive intermodulation includes a first polymeric layer, a second polymeric layer, and a continuous metal layer encapsulated between the first and second polymeric layers. A self-adhesive radio frequency barrier tape includes a waterproof polymeric top layer, a metal-containing layer adhered by an adhesive layer to the polymeric top layer, a pressure sensitive adhesive layer adhered to the metal-containing layer, and a release liner on a bottom surface of the pressure sensitive adhesive layer. A method of mitigating passive intermodulation includes passing a probe over an area of interest, the probe being sensitive to an intermodulation frequency of interest, and identifying a suspected source of passive intermodulation when the amplitude of the probe output exceeds a threshold at the frequency of interest. The method further includes covering the suspected passive intermodulation source with a radio frequency barrier material.

Steel sheet for containers and method for producing steel sheet for containers
11542620 · 2023-01-03 · ·

A steel sheet for a container according to the present invention includes: a base steel sheet; a metal chromium layer; and a chromium-containing layer, in which the metal chromium layer is located on at least one surface of the base steel sheet, the chromium-containing layer is located on the metal chromium layer and contains a granular trivalent chromium compound, or contains a granular trivalent chromium compound and granular metal chromium, the metal chromium layer and the chromium-containing layer are separately disposed in two layers on the base steel sheet, in the chromium-containing layer, an average particle size of the trivalent chromium compound and the metal chromium is 10 nm or more and 100 nm or less, and an adhesion amount of the chromium-containing layer is 1.0 mg/m.sup.2 or more and 100 mg/m.sup.2 or less in terms of a Cr content.

Tube container

Proposed is a tube container in which generation of scratches on a surface of the container can be prevented. The present tube container (100) includes a tube body (30) that defines a container space (S) for contents and that has a laminated structure. The tube body (30) includes: a cylindrical laminated sheet (31) in which both edges (31a, 31b) of the sheet are butted together; and a reinforcing tape portion (reinforcing tape 35) provided on an inner surface of the laminated sheet (31) along a butted portion (32). The laminate sheet (31) includes a high hardness protective layer (18) constituting an outermost layer, an outer polyethylene-based resin layer (21) formed on an inner side of the high hardness protective layer (18), and an inner polyethylene-based resin layer (11) constituting an innermost layer, and the high hardness protective layer (18) has a pencil hardness of 3B or greater than 3B. The reinforcing tape portion (35) includes a polyethylene-based resin layer (outer reinforcing resin layer 59) as an outermost layer abutting against the inner surface of the laminate sheet (31).

Polyethylene based laminated film structure with barrier properties

Laminated film structure including at least one first film having a thin ceramic or metal coating, being laminated to a second film and whereby the laminated film structure is based on polyethylene only, i.e. polymers other than polyethylene are substantially absent and whereby the laminated film structure has good barrier properties.

Dielectric composite with reinforced elastomer and integrate electrode

The present disclosure is directed to dielectric elastomeric composites that include a retainable processing membrane, an elastomer material, and an electrically conductive material. The elastomer layer may be partially imbibed into the retainable processing membrane. The retainable processing membrane may be porous. The retainable processing membrane is compacted in the transverse in direction, machine direction, or in both directions prior to the application of an elastomer material and an electrically conductive material. The compaction of the retainable processing membrane may form structured folds or folded fibrils in the membrane, giving the retainable processing membrane a low modulus and flexibility. In some embodiments, the dielectric composites are positioned in a stacked configuration. Alternatively, the dielectric elastomeric composites may have a wound configuration. The dielectric composites have a total thickness less than about 170 μm. The dielectric elastomeric composites may be used, for example, in dielectric elastomer actuators, sensors, and in energy harvesting.

Molded product, metal-clad laminate, printed wiring board, and methods for their production
11535015 · 2022-12-27 · ·

To provide a molded product, a metal-clad laminate and a printed wiring board, each of which contains a tetrafluoroethylene type polymer, whereby an decrease in electrical characteristics is inhibited and a hole can be easily bored with UV-YAG laser; and methods for their production. A molded product containing a tetrafluoroethylene type polymer, in which the content of components other than the tetrafluoroethylene type polymer is at most 0.9 mass %, and which has a wavelength range where the extinction coefficient becomes to be from 1.2 to 4.5 at from 200 to 380 nm; and a method for its production. A metal-clad laminate having a conductive metal layer and a layer of the molded product; and a method for its production. A printed wiring board provided with the metal-clad laminate and having through-holes in the thickness direction of the polymer layer.

Bendable resin having patterned elements for improving penetration of wireless communication signals

A device attachable to a substrate for improving penetration of wireless communication signals is provided. The device is a bendable resin configured to enhance penetration of an incidental radio wave from a first region through the substrate to a second region by forming one or more communication signal beams in the second region. The bendable resin includes a base layer of a first material, and one or more patterned elements each formed by providing a meta-pattern of a second material on the base layer. The first and second materials are different and selected from the group consisting of a dielectric material and a metallic material. Each individual patterned element is configured to tilt the incidental radio wave to form the one or more communication signal beams, wherein each individual communication signal beam is beam-focused at a predetermined focal point or a predetermined focal area in the second region.