B32B2307/584

Method for Production of a Tubular Body
20170283161 · 2017-10-05 ·

A method for production of a tubular body applying the following steps: Pressureless application of at least one first curable plastic layer made of reactive polyurethane materials with a core via a rotational molding process, Curing the at least one plastic layer, Winding at least one reinforcement layer onto the at least one first plastic layer, Pressureless application of at least one second curable plastic layer, wherein the reinforcement layer is embedded without holes between the two plastic layers, and Removal of the core after completion of the body.

Because of this, the position of the reinforcement layer 7 can be individually established and it can be ensured that the reinforcement layer will not penetrate into the first plastic layer during winding after the curing of the first plastic layer.

DECORATIVE SHEET

Provided is a decorative sheet having excellent abrasion-resistance. Also, provided is a decorative sheet capable of reducing abrasion sound. A decorative sheet is provided with; a linear irregularity pattern formed by a plurality of groove parts arranged side by side; and a protrusion pattern that coexists inside the linear irregularity pattern, is arranged at random without having any regularity with respect to the linear irregularity pattern, and is formed to have at least a height equal to or higher than a height of a protrusion part of the linear irregularity pattern. The protrusion pattern reinforces the linear irregularity pattern.

DISPLAY DEVICE AND METHOD OF MANUFACTURING THE SAME
20220052282 · 2022-02-17 ·

A display device including a folding area includes a display panel, a cover window disposed above the display panel, and a protective film disposed on the cover window, where the protective film includes a first region and a second region including a same material as each other and having different moduli from each other. A modulus of the second region of the protective film is less than a modulus of the first region, and the second region is disposed in the folding area.

Door body

Embodiments provide a door body which opens and closes a front part of an article body, and which has a front panel that constitutes the front of the door body, a frame that supports at least a part of the outside edge of the front panel, and a back panel that constitutes the back of the door body. According to at least one embodiment, the front panel includes a hard coat laminated sheet; the hard coat laminated sheet has a first hard coat, a second hard coat, and a transparent resin sheet layer in that order from the surface on the front side. The first hard coat is formed from a coating material which contains (A) 100 parts by mass of a polyfunctional(meth)acrylate, (B) 0.01-7 parts by mass of a water repellant and (C) 0.01-10 parts by mass of a silane coupling agent and which does not contain inorganic particles, and the second hard coat is formed from a coating material which contains (A) 100 parts by mass of the polyfunctional (meth)acrylate and (D) 50-300 parts by mass of inorganic fine particles having an average particle diameter of 1-300 nm. This door body may have a display on at least a part of the front thereof.

COMPOSITE BODY AND METHOD FOR PRODUCING SAME
20170239715 · 2017-08-24 · ·

A composite production method includes impregnating a plate-shaped porous inorganic structure and a fibrous inorganic material with a metal while the fibrous inorganic material is arranged to be adjacent to the porous inorganic structure. In the composite structure, first and second phases are adjacent to each other by using a porous inorganic structure having a porous silicon carbide ceramic sintered body and the fibrous inorganic material, the first phase being a phase in which the porous silicon carbide ceramic sintered body is impregnated with the metal, the second phase being a phase in which the fibrous inorganic material is impregnated with the metal, a percentage of the porous silicon carbide ceramic sintered body in the first phase is 50 to 80 volume percent, and a percentage of the fibrous inorganic material in the second phase is 3 to 20 volume percent. A composite is produced by the method.

LAMINATED MEMBER FOR DECORATION AND METHOD FOR PRODUCING DECORATIVE MOLDED ARTICLE

An object of the present invention is to provide a laminated member for decoration that can be molded into a complicated shape and has a superior hardcoating property. The present invention relates to a laminated member for decoration having a protective film, a coating layer and a resin substrate, wherein the surface roughness Rz(a) of the adhesive layer of the protective film on the side where the coating layer is located and the surface roughness Rz(b) of the coating layer of an unheated sample formed by peeling the protective layer, the surface roughness being taken on the side opposite from the resin substrate, define Rz(b)/Rz(a)×100 having a prescribed relationship; the surface roughness Rz(b) and the surface roughness Rz(bh) of the coating layer of a heated sample prepared by heating the unheated sample under a prescribed condition, the surface roughness being taken on the side opposite from the resin substrate, satisfy at least one of Formulas (2) and (3) below:


0%≤Rz(bh)/Rz(b)×100<30%  (2), and


0≤Rz(bh)≤Rz(b)<0.5 μm  (3);

and the unreacted (meth)acryloyl groups of the coating layer of the heated sample irradiated with a prescribed amount of active energy rays have disappeared 10 to 100% as compared with the coating layer of the unheated sample.

Coated film

According to the present invention, there is provide a coated film that can be highly prevented from suffering from deposition of oligomers from a surface of the film when exposed to a high temperature condition, and is excellent in adhesion property to various functional layers. The present invention relates to a coated film comprising a single-layer polyester film having an ester cyclic trimer content of not more than 0.7% by weight or a multilayer polyester film comprising a polyester surface layer having an ester cyclic trimer content of not more than 0.7% by weight, and a coating layer formed on at least one surface of the single-layer polyester film or multilayer polyester film, the coating layer being prepared from a coating solution comprising a crosslinking agent in an amount of not less than 70% by weight based on the weight of nonvolatile components in the coating solution.

Polymer resin, window module including the same, and display apparatus including the same

A window module including a window, a first print layer, an ink layer, and a protective layer covering the ink layer. The protective layer includes a polymer resin polymerized from monomers including a first monomer which is an acrylic monomer substituted with a hydroxy group, a second monomer having an epoxy group, and at least one of a third monomer having a substituted or unsubstituted phenyl group or a fourth monomer which is an acrylic monomer having a substituted or unsubstituted bicyclic alkyl group, and thus, has excellent durability, chemical resistance, and abrasion resistance.

Method for manufacturing plastic glazing
11426991 · 2022-08-30 ·

The present disclosure relates to a method for manufacturing highly reliable plastic glazing by forming a high hardness coating layer. The method for manufacturing plastic glazing includes: a base material layer supply step of supplying base material layer made of polycarbonate (PC) resin; an adhesive supply step of applying an adhesive to at least one side of the base material layer; a coating film supply step of seating a coating film on an upper side of the adhesive applied to the base material layer; and an attaching step of pressing the supplied coating film and of attaching to the base material layer. Through such a manufacturing method, there is an effect of improving the scratch resistance, abrasion resistance, chemical resistance, and light resistance by forming the high hardness coating layer in the base material layer made of PC.

METHOD FOR MANUFACTURING PLASTIC GLAZING
20220032597 · 2022-02-03 ·

The present disclosure relates to a method for manufacturing highly reliable plastic glazing by forming a high hardness coating layer. The method for manufacturing plastic glazing includes: a base material layer supply step of supplying base material layer made of polycarbonate (PC) resin; an adhesive supply step of applying an adhesive to at least one side of the base material layer; a coating film supply step of seating a coating film on an upper side of the adhesive applied to the base material layer; and an attaching step of pressing the supplied coating film and of attaching to the base material layer. Through such a manufacturing method, there is an effect of improving the scratch resistance, abrasion resistance, chemical resistance, and light resistance by forming the high hardness coating layer in the base material layer made of PC.