Patent classifications
B81C2201/112
METHOD TO FORM A ROUGH CRYSTALLINE SURFACE
Various embodiments of the present disclosure are directed towards a method to roughen a crystalline layer. A crystalline layer is deposited over a substrate. A mask material is diffused into the crystalline layer along grain boundaries of the crystalline layer. The crystalline layer and the mask material may, for example, respectively be or comprise polysilicon and silicon oxide. Other suitable materials are, however, amenable. An etch is performed into the crystalline layer with an etchant having a high selectivity for the crystalline layer relative to the mask material. The mask material defines micro masks embedded in the crystalline layer along the grain boundaries. The micro masks protect underlying portions of the crystalline layer during the etch, such that the etch forms trenches in the crystalline layer where unmasked by the micro masks.
Method and Structure for CMOS-MEMS Thin Film Encapsulation
Representative methods for sealing MEMS devices include depositing insulating material over a substrate, forming conductive vias in a first set of layers of the insulating material, and forming metal structures in a second set of layers of the insulating material. The first and second sets of layers are interleaved in alternation. A dummy insulating layer is provided as an upper-most layer of the first set of layers. Portions of the first and second set of layers are etched to form void regions in the insulating material. A conductive pad is formed on and in a top surface of the insulating material. The void regions are sealed with an encapsulating structure. At least a portion of the encapsulating structure is laterally adjacent the dummy insulating layer, and above a top surface of the conductive pad. An etch is performed to remove at least a portion of the dummy insulating layer.
Rough layer for better anti-stiction deposition
A microelectromechanical systems (MEMS) package with roughness for high quality anti-stiction is provided. A device substrate is arranged over a support device. The device substrate comprises a movable element with a lower surface that is rough and that is arranged within a cavity. A dielectric layer is arranged between the support device and the device substrate. The dielectric layer laterally encloses the cavity. An anti-stiction layer lines the lower surface of the movable element. A method for manufacturing the MEMS package is also provided.
MEMS DEVICE HAVING A RUGGED PACKAGE AND FABRICATION PROCESS THEREOF
A MEMS device formed by a substrate, having a surface; a MEMS structure arranged on the surface; a first coating region having a first Young's modulus, surrounding the MEMS structure at the top and at the sides and in contact with the surface of the substrate; and a second coating region having a second Young's modulus, surrounding the first coating region at the top and at the sides and in contact with the surface of the substrate. The first Young's modulus is higher than the second Young's modulus.
ROUGHNESS SELECTIVITY FOR MEMS MOVEMENT STICTION REDUCTION
A micro-electromechanical-system (MEMS) device may be formed to include an anti-stiction polysilicon layer on one or more moveable MEMS structures of a device wafer of the MEMS device to reduce, minimize, and/or eliminate stiction between the moveable MEMS structures and other components or structures of the MEMS device. The anti-stiction polysilicon layer may be formed such that a surface roughness of the anti-stiction polysilicon layer is greater than the surface roughness of a bonding polysilicon layer on the surfaces of the device wafer that are to be bonded to a circuitry wafer of the MEMS device. The higher surface roughness of the anti-stiction polysilicon layer may reduce the surface area of the bottom of the moveable MEMS structures, which may reduce the likelihood that the one or more moveable MEMS structures will become stuck to the other components or structures.
ROUGHNESS SELECTIVITY FOR MEMS MOVEMENT STICTION REDUCTION
A micro-electromechanical-system (MEMS) device may be formed to include an anti-stiction polysilicon layer on one or more moveable MEMS structures of a device wafer of the MEMS device to reduce, minimize, and/or eliminate stiction between the moveable MEMS structures and other components or structures of the MEMS device. The anti-stiction polysilicon layer may be formed such that a surface roughness of the anti-stiction polysilicon layer is greater than the surface roughness of a bonding polysilicon layer on the surfaces of the device wafer that are to be bonded to a circuitry wafer of the MEMS device. The higher surface roughness of the anti-stiction polysilicon layer may reduce the surface area of the bottom of the moveable MEMS structures, which may reduce the likelihood that the one or more moveable MEMS structures will become stuck to the other components or structures.
Method to form a rough crystalline surface
Various embodiments of the present disclosure are directed towards a method to roughen a crystalline layer. A crystalline layer is deposited over a substrate. A mask material is diffused into the crystalline layer along grain boundaries of the crystalline layer. The crystalline layer and the mask material may, for example, respectively be or comprise polysilicon and silicon oxide. Other suitable materials are, however, amenable. An etch is performed into the crystalline layer with an etchant having a high selectivity for the crystalline layer relative to the mask material. The mask material defines micro masks embedded in the crystalline layer along the grain boundaries. The micro masks protect underlying portions of the crystalline layer during the etch, such that the etch forms trenches in the crystalline layer where unmasked by the micro masks.
Method and Structure for CMOS-MEMS Thin Film Encapsulation
Representative methods for sealing MEMS devices include depositing insulating material over a substrate, forming conductive vias in a first set of layers of the insulating material, and forming metal structures in a second set of layers of the insulating material. The first and second sets of layers are interleaved in alternation. A dummy insulating layer is provided as an upper-most layer of the first set of layers. Portions of the first and second set of layers are etched to form void regions in the insulating material. A conductive pad is formed on and in a top surface of the insulating material. The void regions are sealed with an encapsulating structure. At least a portion of the encapsulating structure is laterally adjacent the dummy insulating layer, and above a top surface of the conductive pad. An etch is performed to remove at least a portion of the dummy insulating layer.
METHOD AND SYSTEM FOR FABRICATING A MEMS DEVICE
A method includes forming a bumpstop from a first intermetal dielectric (IMD) layer and forming a via within the first IMD, wherein the first IMD is disposed over a first polysilicon layer, and wherein the first polysilicon layer is disposed over another IMD layer that is disposed over a substrate. The method further includes depositing a second polysilicon layer over the bumpstop and further over the via to connect to the first polysilicon layer. A standoff is formed over a first portion of the second polysilicon layer, and wherein a second portion of the second polysilicon layer is exposed. The method includes depositing a bond layer over the standoff.
METHOD AND SYSTEM FOR FABRICATING A MEMS DEVICE
A device includes a substrate and an intermetal dielectric (IMD) layer disposed over the substrate. The device also includes a first plurality of polysilicon layers disposed over the IMD layer and over a bumpstop. The device also includes a second plurality of polysilicon layers disposed within the IMD layer. The device includes a patterned actuator layer with a first side and a second side, wherein the first side of the patterned actuator layer is lined with a polysilicon layer, and wherein the first side of the patterned actuator layer faces the bumpstop. The device further includes a standoff formed over the IMD layer, a via through the standoff making electrical contact with the polysilicon layer of the actuator and a portion of the second plurality of polysilicon layers and a bond material disposed on the second side of the patterned actuator layer.