B01D2251/2067

Device and method for producing enameled wires
11605481 · 2023-03-14 · ·

A device (1) and a method for producing enameled wires, comprises an application device (3) for applying at least one enamel coating, a furnace (4) for solidifying the enamel coating and an exhaust gas purification device (7) for removing at least nitrogen oxides from an exhaust gas (9) of the furnace (4). The exhaust gas purification device (7) has a unit (13) for the selective catalytic reduction of nitrogen oxides in the exhaust gas (9) of the furnace and a feeding apparatus (11) for feeding a reducing agent, preferably an ammonia-containing compound, in particular a urea solution, into the exhaust gas (9) of the furnace (4). The feeding apparatus (11) has at least one outlet opening, which is designed in such a way that the reducing agent exits from the outlet opening substantially in the flow direction of the exhaust gas (9).

A SELECTIVE CATALYTIC REDUCTION CATALYST AND A PROCESS FOR PREPARING A SELECTIVE CATALYTIC REDUCTION CATALYST

The present invention relates to a process for preparing a catalyst for the selective catalytic reduction of nitrogen oxide comprising, among other steps, preparing a second aqueous mixture comprising water and an iron salt; and disposing the second mixture on the substrate obtained according to (ii), comprising a coating comprising a zeolitic material comprising copper, over y % of the substrate axial length from the inlet end to the outlet end of the substrate, wherein y is in the range of from 10 to x, obtaining a substrate comprising, in a first zone, the coating comprising a zeolitic material comprising copper and over y % of the substrate axial length an iron salt; and, if x > y, in a second zone extending from y % to x % of the substrate axial length from the inlet end to the outlet end, the coating comprising a zeolitic material comprising copper.

Zeolite with reduced extra-framework aluminum

The present disclosure generally provides a catalyst composition comprising a zeolite containing iron and/or copper with a reduced amount of extra-framework aluminum. The catalyst composition is useful to catalyze the reduction of nitrogen oxides in exhaust gas in the presence of a reductant.

Fluid level wake-up functionality
11598241 · 2023-03-07 · ·

A reduction device includes a housing defining an input chamber configured to receive exhaust from a power source, an output chamber, an exhaust channel configured to direct the exhaust from the input chamber to the output chamber, and a longitudinal axis. The reduction device also includes a treatment unit disposed in the exhaust channel and along the longitudinal axis. The treatment unit is configured to at least partly remove pollutant species from the exhaust. The reduction device also includes an attenuation component disposed in the housing and radially outward of the treatment unit. The attenuation component is fluidly connected to the exhaust channel, and is configured to attenuate a range of frequencies corresponding to operation of the power source. Additionally, the exhaust channel prohibits exhaust entering the input chamber from exiting the housing without passing through the treatment unit.

REDUCTANT INJECTION SYSTEM AND METHOD FOR SELECTIVE CATALYTIC REDUCTION REACTION

The present disclosure relates to reductant injection system and method for a selective catalytic reduction reaction whereby urea is injected directly to an exhaust line where a denitrification reaction occurs without using an additional urea decomposition reactor and, thus, conversion from urea to ammonia can occur very fast.

SYSTEMS AND METHODS FOR RECOVERING CATALYST PERFORMANCE

A method of recovering catalyst performance includes providing a vanadium selective catalytic reduction (VSCR) catalyst. The method includes exposing the VSCR catalyst to a first humidity level in a range of 50%-100% relative humidity, at a first temperature in a range of 20° C.-100° C., for a first period of time of at least two hours. The method includes thermally treating the VSCR catalyst at a second temperature in a range of 300° C.-600° C. for a second period of time of at least than one hour.

Exhaust gas sample collector and mixer for aftertreatment system

An exhaust gas treatment system includes an exhaust gas pathway configured to receive exhaust gas from an internal combustion engine. The exhaust gas treatment system further includes a treatment element configured to reduce an emissions component of the exhaust gas, and a sample collector positioned within the exhaust gas pathway downstream of the treatment element. The sample collector includes a plurality of inlet openings spaced about a periphery of the exhaust gas pathway and configured to receive a sample of exhaust gas from the exhaust gas pathway, and an outlet in fluid communication with the plurality of inlet openings. A sensor located at the outlet of the sample collector is configured to measure a characteristic of the sample.

Aftertreatment system including preheating oxidation catalyst

An aftertreatment system for treating an exhaust gas comprises an exhaust conduit, a preheating oxidation catalyst, a primary oxidation catalyst disposed downstream of the preheating oxidation catalyst, and a selective catalytic reduction system disposed in the exhaust conduit downstream of the primary oxidation catalyst. A controller is configured to determine a temperature of an exhaust gas at an inlet of the selective catalytic reduction system. In response to the temperature being below a threshold temperature, the controller generates a hydrocarbon insertion signal configured to cause hydrocarbons to be inserted into or upstream of the preheating oxidation catalyst so as to increase a temperature of the exhaust gas to above the threshold temperature.

Catalyst arrangement deciding method for flue gas denitrizer, maintenance method for flue gas denitrizer, flue gas denitrizer, boiler, and power generation plant

A catalyst arrangement deciding method for a flue gas denitrizer including a catalyst layer disposed in an exhaust gas passage includes: a step of investigating a location dependence of a degradation state of a catalyst in the catalyst layer after a lapse of a period of operation; and a step of deciding a first region of the catalyst layer in which a first catalyst is used and a second region of the catalyst layer in which a second catalyst different from the first catalyst is used, on the basis of the location dependence.

METHODS OF FORMING AQUEOUS UREA UTILIZING CARBON DIOXIDE CAPTURED FROM EXHAUST GAS AT WELLSITE

A method includes collecting exhaust gas comprising carbon dioxide (CO.sub.2) at a wellsite to provide a collected exhaust gas, separating CO.sub.2 from the collected exhaust gas to provide a separated CO.sub.2, and forming urea utilizing at least a portion of the separated CO.sub.2. A system for carrying out the method is also provided.