B01J23/26

PROCESS FOR REDUCING THE SULPHUR CONTENT OF ANATASE TITANIA AND THE SO-OBTAINED PRODUCT

An anatase titanium dioxide includes at least one compound selected from oxides of Si, Al, and Zr in an amount of 2-50% b.w., calculated as oxides, of a total weight of the oxides, and a sulfur content of less than 150 ppm based on the total weight of the oxides.

PROCESS FOR REDUCING THE SULPHUR CONTENT OF ANATASE TITANIA AND THE SO-OBTAINED PRODUCT

An anatase titanium dioxide includes at least one compound selected from oxides of Si, Al, and Zr in an amount of 2-50% b.w., calculated as oxides, of a total weight of the oxides, and a sulfur content of less than 150 ppm based on the total weight of the oxides.

Process to convert synthesis gas to olefins using a bifunctional chromium/zinc oxide-SAPO-34 catalyst

A process for preparing C.sub.2 to C.sub.3 olefins includes introducing a feed stream having a volumetric ratio of hydrogen to carbon monoxide from greater than 0.5:1 to less than 5:1 into a reactor, and contacting the feed stream with a bifunctional catalyst. The bifunctional catalyst includes a Cr/Zn oxide methanol synthesis component having a Cr to Zn molar ratio from greater than 1.0:1 to less than 2.15:1, and a SAPO-34 silicoaluminophosphate microporous crystalline material. The reactor operates at a temperature ranging from 350 C. to 450 C., and a pressure ranging from 10 bar (1.0 MPa) to 60 bar (6.0 MPa). The process has a cumulative productivity of C.sub.2 to C.sub.3 olefins greater than 15 kg C.sub.2 to C.sub.3 olefins/kg catalyst.

Process to convert synthesis gas to olefins using a bifunctional chromium/zinc oxide-SAPO-34 catalyst

A process for preparing C.sub.2 to C.sub.3 olefins includes introducing a feed stream having a volumetric ratio of hydrogen to carbon monoxide from greater than 0.5:1 to less than 5:1 into a reactor, and contacting the feed stream with a bifunctional catalyst. The bifunctional catalyst includes a Cr/Zn oxide methanol synthesis component having a Cr to Zn molar ratio from greater than 1.0:1 to less than 2.15:1, and a SAPO-34 silicoaluminophosphate microporous crystalline material. The reactor operates at a temperature ranging from 350 C. to 450 C., and a pressure ranging from 10 bar (1.0 MPa) to 60 bar (6.0 MPa). The process has a cumulative productivity of C.sub.2 to C.sub.3 olefins greater than 15 kg C.sub.2 to C.sub.3 olefins/kg catalyst.

LIQUID FUEL CPOX REFORMER AND FUEL CELL SYSTEMS, AND METHODS OF PRODUCING ELECTRICITY
20200299131 · 2020-09-24 ·

Integrated liquid fuel catalytic partial oxidation (CPOX) reformer and fuel cell systems can include a plurality or an array of spaced-apart CPOX reactor units, each reactor unit including an elongated tube having a gas-permeable wall with internal and external surfaces. The wall encloses an unobstructed gaseous flow passageway. At least a portion of the wall has CPOX catalyst disposed therein and/or comprising its structure. The catalyst-containing wall structure and open gaseous flow passageway enclosed thereby define a gaseous phase CPOX reaction zone, the catalyst-containing wall section being gas-permeable to allow gaseous CPOX reaction mixture to diffuse therein and hydrogen rich product reformate to diffuse therefrom. The liquid fuel CPOX reformer also can include a vaporizer, one or more igniters, and a source of liquid reformable fuel. The hydrogen-rich reformate can be converted to electricity within a fuel cell unit integrated with the CPOX reactor unit.

CATALYST, AND METHOD FOR DIRECT CONVERSION OF SYNGAS TO PREPARE LIQUID FUEL AND TO PRODUCE LIGHT OLEFINS
20200276559 · 2020-09-03 ·

Direct conversion of syngas produces liquid fuels and light olefins. The catalytic reaction is conducted on a fixed bed or a moving bed. The catalyst comprises A and B components. The component A is composed of active metal oxides, and the active ingredients of the component B are zeolites with a MEL structure. The distance between the geometric centers of catalyst A and catalyst B particles is 2 nm-10 mm; a weight ratio of the catalyst A to the catalyst B is 0.1-20. The pressure of the syngas is 0.1-10 MPa; reaction temperature is 300-600 C.; and space velocity is 300-10000 h.sup.1. The reaction mainly produces gasoline with high octane number, and co-generates light olefins. Meanwhile, the selectivity for a methane byproduct is low (less than 10%).

CATALYST, AND METHOD FOR DIRECT CONVERSION OF SYNGAS TO PREPARE LIQUID FUEL AND TO PRODUCE LIGHT OLEFINS
20200276559 · 2020-09-03 ·

Direct conversion of syngas produces liquid fuels and light olefins. The catalytic reaction is conducted on a fixed bed or a moving bed. The catalyst comprises A and B components. The component A is composed of active metal oxides, and the active ingredients of the component B are zeolites with a MEL structure. The distance between the geometric centers of catalyst A and catalyst B particles is 2 nm-10 mm; a weight ratio of the catalyst A to the catalyst B is 0.1-20. The pressure of the syngas is 0.1-10 MPa; reaction temperature is 300-600 C.; and space velocity is 300-10000 h.sup.1. The reaction mainly produces gasoline with high octane number, and co-generates light olefins. Meanwhile, the selectivity for a methane byproduct is low (less than 10%).

METHODS OF PREPARING A CATALYST UTILIZING HYDRATED REAGENTS

A method of preparing a catalyst comprising a) contacting a titanium-containing compound, a solvating agent, and a solvent to form a solution; b) contacting the solution with a chrominated silica-support to form a pre-catalyst; and c) thermally treating the pre-catalyst by heating to a temperature of from about 400 C. to about 1000 C. for a time period of from about 1 minute to about 24 hours to form the catalyst.

METHODS OF PREPARING A CATALYST UTILIZING HYDRATED REAGENTS

A method of preparing a catalyst comprising a) contacting a titanium-containing compound, a solvating agent, and a solvent to form a solution; b) contacting the solution with a chrominated silica-support to form a pre-catalyst; and c) thermally treating the pre-catalyst by heating to a temperature of from about 400 C. to about 1000 C. for a time period of from about 1 minute to about 24 hours to form the catalyst.

Olefin production method using circulating fluidized bed process

Disclosed is an olefin production method which includes: (a) providing the regenerated catalyst and the hydrocarbon including not less than 90 wt % of LPG into Riser of Fast Fluidization Regime, and dehydrogenating in the presence of an alumina type catalyst; (b) separating an effluent from the dehydrogenation reaction into the catalyst and propylene mixture; (c) stripping to remove the hydrocarbon compound included in the catalyst separated at stage (b); (d) mixing the catalyst stripped at stage (c) with the gas including oxygen, and continuously regenerating it; (e) recycling the catalyst regenerated at stage (d) to stage (a), and providing it again into Riser; and (f) producing propylene product by cooling, compressing and separating propylene mixture of the reaction product separated at stage (b).