Patent classifications
B01J27/224
Honeycomb structure
A honeycomb structure including: a pillar-shaped honeycomb structure portion having an outer peripheral wall and partition walls disposed on an inner side of the outer peripheral wall and defining a plurality of cells extending from one end face to another end face to form flow paths; and at least an electrode portion disposed on an outer surface of the outer peripheral wall of the pillar-shaped honeycomb structure portion, wherein the pillar-shaped honeycomb structure portion is formed of ceramics containing either or both of Si and SiC, the electrode portion contains either or both of a metal and a metal compound in addition to an oxide, and a volume ratio of the oxide on an inner peripheral side of the electrode portion is higher than a volume ratio of the oxide on an outer peripheral side of the electrode portion.
EXHAUST GAS TREATMENT SYSTEM AND THE USE THEREOF FOR THE TREATMENT OF AN EXHAUST GAS
An exhaust gas treatment system (1) comprises a catalyst article (5) for the treatment of an exhaust gas, the catalyst article (5) comprising a non-metallic substrate (20) comprising a plurality of catalytically-active transition-metal-doped iron oxide magnetic particles (45), and an inductive heater (70) for inductively heating the plurality of catalytically-active magnetic particles by applying an alternating magnetic field.
CERAMIC POROUS BODY AND METHOD FOR PRODUCING THE SAME, AND DUST COLLECTING FILTER
A ceramic porous body including: skeleton portions including an aggregate and at least one bonding material; and pore portions formed between the skeleton portions, the pore portions being capable of allowing a fluid to flow therethrough, wherein the pore portions have a pore volume ratio of pores having a pore diameter of from 10 to 15 m, of from 4 to 17% or more.
CERAMIC POROUS BODY AND METHOD FOR PRODUCING THE SAME, AND DUST COLLECTING FILTER
A ceramic porous body including: skeleton portions including an aggregate and at least one bonding material; and pore portions formed between the skeleton portions, the pore portions being capable of allowing a fluid to flow therethrough, wherein the pore portions have a pore volume ratio of pores having a pore diameter of from 10 to 15 m, of from 4 to 17% or more.
SUPPORTED METAL CATALYST
A long-life catalyst which can be easily and inexpensively manufactured and has high activity and suppressed leakage of metal. A catalyst according to some embodiments includes: a substrate; and a first metal atom as a catalytic center. The substrate contains a non-metallic atom and a second metal atom, and the non-metallic atom is any one selected from the group consisting of a group 15 element, a group 16 element and a group 17 element.
SUPPORTED METAL CATALYST
A long-life catalyst which can be easily and inexpensively manufactured and has high activity and suppressed leakage of metal. A catalyst according to some embodiments includes: a substrate; and a first metal atom as a catalytic center. The substrate contains a non-metallic atom and a second metal atom, and the non-metallic atom is any one selected from the group consisting of a group 15 element, a group 16 element and a group 17 element.
COATING MATERIAL FOR HONEYCOMB STRUCTURE, OUTER PERIPHERAL COATING OF HONEYCOMB STRUCTURE, AND HONEYCOMB STRUCTURE WITH OUTER PERIPHERAL COATING
A coating material for a honeycomb structure, the coating material containing: from 1% by mass to 10% by mass of first ceramic fibers having an average axial length of from 80 m to 200 m in an inorganic raw material; and from 0.1% by mass to 15% by mass of second ceramic fibers having an average axial length of from 50 m to 70 m in the inorganic raw material.
COATING MATERIAL FOR HONEYCOMB STRUCTURE, OUTER PERIPHERAL COATING OF HONEYCOMB STRUCTURE, AND HONEYCOMB STRUCTURE WITH OUTER PERIPHERAL COATING
A coating material for a honeycomb structure, the coating material containing: from 1% by mass to 10% by mass of first ceramic fibers having an average axial length of from 80 m to 200 m in an inorganic raw material; and from 0.1% by mass to 15% by mass of second ceramic fibers having an average axial length of from 50 m to 70 m in the inorganic raw material.
Electrically heated catalytic converter and method of manufacturing the same
Provided is an electrically heated catalytic converter including at least a conductive substrate and an electrode member that is fixed to the substrate, in which a protective film is formed on a surface of at least a portion of the electrode member. In the electrically heated catalytic converter, at least a portion of the protective film is formed of Al.sub.2O.sub.3, SiO.sub.2, a composite material of Al.sub.2O.sub.3 and SiO.sub.2, or a composite oxide including Al.sub.2O.sub.3, SiO.sub.2, or a composite material of Al.sub.2O.sub.3 and SiO.sub.2 as a major component, the protective film has an amorphous structure or a partially crystalline glass structure having a crystallization rate of 30 vol % or lower with respect to the entire portion of the protective film, and a thickness of the protective film is in a range of 100 nm to 2 m.
Electrically heated catalytic converter and method of manufacturing the same
Provided is an electrically heated catalytic converter including at least a conductive substrate and an electrode member that is fixed to the substrate, in which a protective film is formed on a surface of at least a portion of the electrode member. In the electrically heated catalytic converter, at least a portion of the protective film is formed of Al.sub.2O.sub.3, SiO.sub.2, a composite material of Al.sub.2O.sub.3 and SiO.sub.2, or a composite oxide including Al.sub.2O.sub.3, SiO.sub.2, or a composite material of Al.sub.2O.sub.3 and SiO.sub.2 as a major component, the protective film has an amorphous structure or a partially crystalline glass structure having a crystallization rate of 30 vol % or lower with respect to the entire portion of the protective film, and a thickness of the protective film is in a range of 100 nm to 2 m.