B01J29/60

Method of producing separation membrane
11969692 · 2024-04-30 · ·

A method of producing a separation membrane includes a seed crystal adhesion step of adhering zeolite seed crystals to a porous support formed of stainless steel to obtain a seed crystal-bearing support and a separation layer formation step of forming a porous separation layer formed of a zeolite on the seed crystal-bearing support. The stainless steel has a contact angle with water of 90? or more. The seed crystal adhesion step includes bringing the zeolite seed crystals and a solvent having a contact angle with the stainless steel of 30? or less into contact with the porous support.

Process for producing aromatics, p-xylene and terephthalic acid, and device for producing aromatics

The present invention relates to a process for producing aromatics, a process for producing p-xylene and terephthalic acid, and a device for producing aromatics. The process for producing aromatics at least comprises a step of producing C8 olefin from a compound having a lactone group and a step of producing aromatics from the C8 olefin. The process for producing aromatics has the characters of high yield of aromatics and high selectivity to xylene.

Process for producing aromatics, p-xylene and terephthalic acid, and device for producing aromatics

The present invention relates to a process for producing aromatics, a process for producing p-xylene and terephthalic acid, and a device for producing aromatics. The process for producing aromatics at least comprises a step of producing C8 olefin from a compound having a lactone group and a step of producing aromatics from the C8 olefin. The process for producing aromatics has the characters of high yield of aromatics and high selectivity to xylene.

Method of forming a catalyst with an ion-modified binder

An alkylation catalyst having a zeolite catalyst component and a binder component providing mechanical support for the zeolite catalyst component is disclosed. The binder component is an ion-modified binder that can include metal ions selected from the group consisting of Co, Mn, Ti, Zr, V, Nb, K, Cs, Ga, B, P, Rb, Ag, Na, Cu, Mg, Fe, Mo, Ce, and combinations thereof. The metal ions reduce the number of acid sites on the zeolite catalyst component. The metal ions can range from 0.1 to 50 wt % based on the total weight of the ion-modified binder. Optionally, the ion-modified binder is present in amounts ranging from 1 to 80 wt % based on the total weight of the catalyst.

Process for producing aromatics, p-xylene and terephthalic acid

The present invention relates to a process for producing aromatics, p-xylene and terephthalic acid. The process for producing aromatics comprises a step of contacting an oxygen-containing raw material with an aromatization catalyst, under aromatization reaction conditions, to produce aromatics. The process for producing aromatics has an advantage of high yield of carbon as aromatics.

Process for removing oxygenates from naphtha

A process is presented for the removal of contaminants like oxygenates from hydrocarbons. The contaminant oxygenates are removed from hydrocarbons that may be feed to cracking units. A crude feed stream is fed to a water wash column along with water to remove oxygenates and is subsequently treated with an adsorbent to effectively remove all the oxygenates from the crude hydrocarbon. A regenerant medium from a naphtha hydrotreating unit is used to regenerate the adsorbent.

Methods of regenerating aromatization catalysts with a decoking step between chlorine and fluorine addition

Methods for regenerating a spent catalyst in a metal reactor are disclosed. Such methods may employ a step of chlorinating the spent catalyst, followed by decoking the chlorinated spent catalyst, and then fluorinating the de-coked catalyst.

Methods of regenerating aromatization catalysts with a decoking step between chlorine and fluorine addition

Methods for regenerating a spent catalyst in a metal reactor are disclosed. Such methods may employ a step of chlorinating the spent catalyst, followed by decoking the chlorinated spent catalyst, and then fluorinating the de-coked catalyst.

CLUSTER SUPPORTED CATALYST AND METHOD FOR PRODUCING SAME

An improved cluster-supporting catalyst has heteroatom-removed zeolite particles, and catalyst metal clusters supported within the pores of the heteroatom-removed zeolite particles. A method for producing a cluster-supporting catalyst includes the following steps: providing a dispersion liquid containing a dispersion medium and the heteroatom-removed zeolite particles dispersed in the dispersion medium; and in the dispersion liquid, forming catalyst metal clusters having a positive charge, and supporting the catalyst metal clusters within the pores of the heteroatom-removed zeolite particles through an electrostatic interaction.

CLUSTER SUPPORTED CATALYST AND METHOD FOR PRODUCING SAME

An improved cluster-supporting catalyst has heteroatom-removed zeolite particles, and catalyst metal clusters supported within the pores of the heteroatom-removed zeolite particles. A method for producing a cluster-supporting catalyst includes the following steps: providing a dispersion liquid containing a dispersion medium and the heteroatom-removed zeolite particles dispersed in the dispersion medium; and in the dispersion liquid, forming catalyst metal clusters having a positive charge, and supporting the catalyst metal clusters within the pores of the heteroatom-removed zeolite particles through an electrostatic interaction.