Patent classifications
B01J41/14
Amorphous inorganic anion exchanger, resin composition for electronic component sealing, and process for producing amorphous bismuth compound
The amorphous inorganic anion exchanger of the present invention is represented by Formula (1) and has an average primary particle size observed with an electron microscope of at least 1 nm but no greater than 500 nm and an NO.sub.3 content of no greater than 1 wt % of the whole:
BiO(OH) Formula (1).
Amorphous inorganic anion exchanger, resin composition for electronic component sealing, and process for producing amorphous bismuth compound
The amorphous inorganic anion exchanger of the present invention is represented by Formula (1) and has an average primary particle size observed with an electron microscope of at least 1 nm but no greater than 500 nm and an NO.sub.3 content of no greater than 1 wt % of the whole:
BiO(OH) Formula (1).
CHARGE REVERSIBLE ION EXCHANGE RESINS, CHROMATOGRAPHY COLUMN, METHOD, AND SYSTEM THEREOF
An ion exchange chromatographic packing material is described that includes a copolymer grafted to support resin particles. The copolymer includes an ion exchange group, an ionic crosslinking group configured to ionically bind to the ion exchange group, and an adjustable ionization state group having at least a first net charge at the first pH and a second net charge at the second pH. An overall first net charge of the chromatographic packing material at the first pH is opposite in polarity to the overall second net charge of the chromatographic packing material. This allows impurities to be removed from the chromatographic packing material at the second pH.
Method for producing monodisperse, amido-methylated vinyl-aromatic bead polymers
The invention relates to a method of producing monodisperse amidomethylated vinylaromatic bead polymers, to ion exchangers prepared from these monodisperse amidomethylated vinylaromatic bead polymers by alkaline hydrolysis, to the method of using said monodisperse amidomethylated vinylaromatic bead polymers in the manufacture of ion exchangers and chelating resins, and also to the method of using these ion exchangers in the removal of heavy metals and noble metals from aqueous solutions or gases.
Method for producing monodisperse, amido-methylated vinyl-aromatic bead polymers
The invention relates to a method of producing monodisperse amidomethylated vinylaromatic bead polymers, to ion exchangers prepared from these monodisperse amidomethylated vinylaromatic bead polymers by alkaline hydrolysis, to the method of using said monodisperse amidomethylated vinylaromatic bead polymers in the manufacture of ion exchangers and chelating resins, and also to the method of using these ion exchangers in the removal of heavy metals and noble metals from aqueous solutions or gases.
SEPARATION MATERIAL
The present invention provides a separation material comprising porous polymer particles that comprise a styrene-based monomer as a monomer unit; and a coating layer that comprises a macromolecule having hydroxyl groups and covers at least a portion of the surface of the porous polymer particles, wherein the rupture strength is 10 mN or higher.
SEPARATION MATERIAL
The present invention provides a separation material comprising porous polymer particles that comprise a styrene-based monomer as a monomer unit; and a coating layer that comprises a macromolecule having hydroxyl groups and covers at least a portion of the surface of the porous polymer particles, wherein the rupture strength is 10 mN or higher.
Composite ion exchange membrane and method of making same
An anion exchange membrane is made by mixing 2 trifluoroMethyl Ketone [nominal] (1.12 g, 4.53 mmol), 1 BiPhenyl (0.70 g, 4.53 mmol), methylene chloride (3.0 mL), trifluoromethanesulfonic acid (TFSA) (3.0 mL) to produce a pre-polymer. The pre-polymer is then functionalized to produce an anion exchange polymer. The pre-polymer may be functionalized with trimethylamine in solution with water. The pre-polymer may be imbibed into a porous scaffold material, such as expanded polytetrafluoroethylene to produce a composite anion exchange membrane.
Composite ion exchange membrane and method of making same
An anion exchange membrane is made by mixing 2 trifluoroMethyl Ketone [nominal] (1.12 g, 4.53 mmol), 1 BiPhenyl (0.70 g, 4.53 mmol), methylene chloride (3.0 mL), trifluoromethanesulfonic acid (TFSA) (3.0 mL) to produce a pre-polymer. The pre-polymer is then functionalized to produce an anion exchange polymer. The pre-polymer may be functionalized with trimethylamine in solution with water. The pre-polymer may be imbibed into a porous scaffold material, such as expanded polytetrafluoroethylene to produce a composite anion exchange membrane.
AGROCHEMICAL RESINATES FOR AGRICULTURAL APPLICATIONS
The invention encompasses resinate formulations comprising an agricultural active ingredient and an ion exchange resin, wherein the agricultural active ingredient is imbibed upon the ion exchange resin; and methods of treating an agricultural surface. The invention also encompasses methods of manufacturing an agricultural formulation comprising a resinate, comprising: providing an agricultural active ingredient and an ion exchange resin; and mixing the agricultural active ingredient and the ion exchange resin to imbibe the agricultural active ingredient upon the ion exchange resin, thereby forming the resinate.