Patent classifications
B22F3/1021
Hybrid solid-state cell with a sealed anode structure
An electrochemical cell is provided which includes a cathode, an anode, an electrolyte separator, and an anode current collector located on the anode. The anode is a three-dimensional (3D) porous anode including ionically conducting electrolyte strands and pores which extend through the anode from the anode current collector to the electrolyte separator. The anode also includes electronically conducting networks extending on sidewall surfaces of the pores from the anode current collector to the electrolyte separator.
Hybrid solid-state cell with a sealed anode structure
An electrochemical cell is provided which includes a cathode, an anode, an electrolyte separator, and an anode current collector located on the anode. The anode is a three-dimensional (3D) porous anode including ionically conducting electrolyte strands and pores which extend through the anode from the anode current collector to the electrolyte separator. The anode also includes electronically conducting networks extending on sidewall surfaces of the pores from the anode current collector to the electrolyte separator.
STEEL, STEEL MECHANICAL PART, ELECTRONIC DEVICE, AND PREPARATION METHOD FOR STEEL MECHANICAL PART
A steel, a steel mechanical part, an electronic device, and a preparation method for a steel mechanical part are provided. The steel includes components of the following mass percentages: chromium: 7% to 11%, nickel: 2% to 7.5%, cobalt: 6% to 15%, molybdenum: 4% to 7%, oxygen: a trace to 0.4%, carbon: a trace to 0.35%, and iron: 50% to 80%. The steel provided in this application has relatively high mechanical strength and is not easily deformed, and therefore a risk of fracture caused when an electronic device using the steel falls off from a height is reduced.
STEEL, STEEL MECHANICAL PART, ELECTRONIC DEVICE, AND PREPARATION METHOD FOR STEEL MECHANICAL PART
A steel, a steel mechanical part, an electronic device, and a preparation method for a steel mechanical part are provided. The steel includes components of the following mass percentages: chromium: 7% to 11%, nickel: 2% to 7.5%, cobalt: 6% to 15%, molybdenum: 4% to 7%, oxygen: a trace to 0.4%, carbon: a trace to 0.35%, and iron: 50% to 80%. The steel provided in this application has relatively high mechanical strength and is not easily deformed, and therefore a risk of fracture caused when an electronic device using the steel falls off from a height is reduced.
Nickel alloy composition with boron and nitrogen
An alloy composition includes, by weight: 20% to 23% of Cr; 8% to 10% of Mo; 3.15% to 4.15% of Nb+Ta; 0.25% to 1.5% of B; 0.35% to 1.75% of N; and a balance of Ni.
Nickel alloy composition with boron and nitrogen
An alloy composition includes, by weight: 20% to 23% of Cr; 8% to 10% of Mo; 3.15% to 4.15% of Nb+Ta; 0.25% to 1.5% of B; 0.35% to 1.75% of N; and a balance of Ni.
Extruder for a system for the additive manufacture of metal parts using the composite extrusion modeling (CEM) method
It is provided an extruder for a system for the additive manufacture of freely formable metal parts with or without a supporting structure by means of an extrusion method from a composite material, which is arranged on a three-dimensionally movable kinematic mechanism, with a building platform. The extruder consists of a housing and a screw arranged in the housing. The extruder is provided with a mechanical drive for the composite material to be extruded, with an exchangeable nozzle, arranged on the housing, and the housing is connected to the mechanical drive by way of suitable means for transporting the composite material.
METHOD OF EXTRUDING A POWDER METALLURGICAL COMPONENT
The invention relates to a method of manufacturing a component (21) from metal-containing powder. A paste is prepared by mixing at least a powder (11) comprising metal, a binder (12) in an amount of 2 to 8 weight % of the paste (10), and liquid (13), such as water, in an amount of 5 to 25 weight % of the paste (10). The paste is transferred to an extruder (31), and the paste is extruded into a green body (20) by using an extrusion pressure (P) of more than 50 bar. Then the green body (20) is dried and sintered or oxidized to obtain the final component.
Method for making a metal part with a complex geometry with a thin wall
A method for producing a thin-walled metal part with complex geometry includes mixing a metal powder with a polymer binder in order to obtain a composite mixture, producing a flexible composite sheet from the composite mixture, cutting, in the flexible composite sheet, a preform based on a contour of the metal part, applying the preform in a mold having a surface configured with a relief of the metal part, and debinding and sintering the preform in order to obtain the metal part.
Method for making a metal part with a complex geometry with a thin wall
A method for producing a thin-walled metal part with complex geometry includes mixing a metal powder with a polymer binder in order to obtain a composite mixture, producing a flexible composite sheet from the composite mixture, cutting, in the flexible composite sheet, a preform based on a contour of the metal part, applying the preform in a mold having a surface configured with a relief of the metal part, and debinding and sintering the preform in order to obtain the metal part.