Patent classifications
B23K20/1245
DEVICE AND METHOD FOR CHANGING THE WELDING DIRECTION OF THE WELDING SHOULDER OF A SYSTEM FOR A FRICTION STIR WELDING PROCESS VIRTUALLY WITHOUT DELAY
The invention relates to a device and a method for changing the welding direction of the welding shoulder of a system for a friction stir welding process virtually without delay when required by the geometric arrangement of the joint partners to be welded or by a material unevenness, having the following method features: a) a main part (1) with a horizontally movable bridge support (5) has a friction welding head (12) which can be vertically adjusted together therewith and which has a pin receiving area (13) for mounting and driving a welding pin tip (14), wherein the welding shoulder (18) has a welding shoulder receiving area (17) which is supported at multiple points, and b) the welding shoulder receiving area (17) can be adjusted to any angle of attack relative to the joint partners by means of different push-pull rods (16) during the welding process.
Solid State Extrusion and Bonding Tool
An extrusion and bonding tool for carrying out a hybrid metal extrusion and bonding process, the tool being for extruding an extrusion material and bonding the extrusion material to a substrate is provided. The tool may comprise a main body and a rotating die through which the extrusion material is extruded, wherein the rotating die moves relative to the main body of the tool, and wherein the extrusion material, in use, is extruded through the rotating die at a position that can vary about a circumferential path about a rotation axis of the tool. The tool may comprise an extrusion chamber; and a plurality of dies through which the extrusion material is extruded associated with the extrusion chamber, wherein the tool is arranged so that, in use, the extrusion material is received in the extrusion chamber and plasticised within the extrusion chamber before being extruded through one of the dies onto the substrate.
METHOD FOR MANUFACTURING LIQUID-COOLING JACKET
A method for manufacturing a liquid cooling jacket has a feature of using a primary joining rotary tool provided with a tip side pin and a base side pin having a taper angle larger than a taper angle of the tip side pin and comprising a first primary joining process in which inserting the tip side pin and the base side pin of the rotary tool that is rotating into the sealing body member and moving the rotary tool along the first abutted portion with an outer circumferential face of the base side pin being in contact with a front face of the sealing body member and with the outer circumferential face of the tip side pin being kept off a step side face of the peripheral wall step portion while having a second aluminum alloy of the sealing body member flow into the gap.
Double-Head Double-Sided High-Efficiency Friction Stir Welding Device and Welding Method Thereof
A double-head double-sided high-efficiency friction stir welding device includes a base (1), a pair of columns (2) arranged on the base (1), an upper beam (3), at least one worktable connected with a horizontal surface of the base (1), vision sensors (7) mounted on the upper head (5) and the lower head (6) and used for identifying the weld, and a CNC controller (8) used for controlling operations of the gantry, the upper head (5), the lower head (6), the worktable and the vision sensors (7).
REFILL FRICTION STIR SPOT WELDING METHOD AND REFILL FRICTION STIR SPOT WELDING DEVICE
A friction stir spot welding method performs friction stir spot welding of a pair of workpieces having a coating film formed on at least one welding surface by using a refill friction stir spot welding device including rotary tools. The method includes removing the coating film by plunging a distal end of the shoulder member into one workpiece up to a position closer to the surface than the welding surface, while rotating the shoulder member as a rotary tool around the axis, and rotating the shoulder member in a state in which the surface of one of the pair of workpieces, with the welding surfaces being overlaid on each other, is pressed by the end face of the clamp member and performing friction stir spot welding of the pair of workpieces after the coating film removal by using the pin member and the shoulder member as rotary tools.
Friction stir welding apparatus for structural steel
A friction stir welding apparatus that includes a rotary tool and a heating device. The heating device is placed in front of the rotary tool to heat steel sheets that are used as a workpiece. The rotary tool is moved in the welding direction so that steel sheet is softened by frictional heat. Additionally, the surface temperature, the area, and the position of the heated region during the heating process are strictly controlled. The heating of the steel sheets by the welding apparatus provides sufficient strength and good welding workability by advantageously eliminating plastic flow defects generated due to insufficient heating of workpieces.
REFILL FRICTION STIR SPOT WELDING METHOD, PRESSING TOOL SET, AND REFILL FRICTION STIR SPOT WELDING DEVICE
A friction stir spot welding method includes a welding step of performing friction stir spot welding of a workpiece by using a pin member and a shoulder member while the workpiece is supported and pressed by the end face of a clamp member and a pressing step of causing a friction stir spot welding device to press an obverse surface and a reverse surface of at least one of a friction-stirred region of the workpiece and an adjacent region adjacent to the friction-stirred region of the workpiece from a rotary tool side and an opposite side after the welding step while the pin member and the shoulder member are accommodated in an accommodation space of the clamp member.
DOUBLE-SIDED FRICTION STIR WELDING METHOD FOR METAL SHEETS AND DOUBLE-SIDED FRICTION STIR WELDING DEVICE
There is provided a friction stir welding method in which, when double-sided friction stir welding is performed, enough plastic flow to obtain a welded state uniform in the thickness direction of metal sheets can be obtained, in which an increase in welding speed is achieved while the occurrence of defects during welding is prevented, and in which sufficient strength and improvement in welding workability can be achieved. There is also provided a friction stir welding device suitable for the friction stir welding.
HOLDING JIG AND HOLDING JIG SET FOR DOUBLE-ACTING FRICTION STIR SPOT WELDING, DOUBLE-ACTING FRICTION STIR SPOT WELDING DEVICE, AND DOUBLE-ACTING FRICTION STIR SPOT WELDING METHOD
In a double-acting friction stir spot welding device or a double-acting friction stir spot welding method, a pin member and a cylindrical shoulder member that rotates around the axis of the pin member are used as rotary tools, and a clamp member that has a cylindrical shape positioned so as to surround the outside of the shoulder member and is configured to press a workpiece from an obverse surface with an annular pressing surface of the distal end is used as a holding jig. The clamp member has an inclined surface that is adjacent to the inner edge portion of the pressing surface and inclined so as to reduce the inner diameter of the clamp member toward the back side as viewed from the pressing surface.
CLAMP MEMBER FOR DOUBLE-ACTING FRICTION STIR SPOT WELDING DEVICE, DOUBLE-ACTING FRICTION STIR SPOT WELDING DEVICE, AND DOUBLE-ACTING FRICTION STIR SPOT WELDING METHOD
A clamp member, for a double-acting friction stir spot welding device, is provided for the double-acting friction stir spot welding device to perform friction stir spot welding of a workpiece by using a rotary tool, and presses a surface of the workpiece while the workpiece is supported. The rotary tool has a pin member and a shoulder member. The clamp member includes an end face that comes into surface contact with the surface of the workpiece to press the surface and a protruding portion protruding from the end face in an axial direction and extending around an axis. The protruding portion is configured to press the workpiece, the clamp member surrounding an outer periphery of the shoulder member.