B29C48/91

HIGH STRENGTH 3D-PRINTED POLYMER STRUCTURES AND METHODS OF FORMATION
20230015346 · 2023-01-19 ·

A polymer body includes a first thermoplastic polymer, and a second thermoplastic polymer. The first thermoplastic polymer and the second thermoplastic polymer form a continuous solid structure. The first thermoplastic polymer forms an external supporting structure that at least partially envelops the second thermoplastic polymer. A first flow temperature of the first thermoplastic polymer is at least 10° C. higher than a second flow temperature of the second thermoplastic polymer. The first thermoplastic polymer may be removable by exposure to a selective solvent.

HIGH STRENGTH 3D-PRINTED POLYMER STRUCTURES AND METHODS OF FORMATION
20230015346 · 2023-01-19 ·

A polymer body includes a first thermoplastic polymer, and a second thermoplastic polymer. The first thermoplastic polymer and the second thermoplastic polymer form a continuous solid structure. The first thermoplastic polymer forms an external supporting structure that at least partially envelops the second thermoplastic polymer. A first flow temperature of the first thermoplastic polymer is at least 10° C. higher than a second flow temperature of the second thermoplastic polymer. The first thermoplastic polymer may be removable by exposure to a selective solvent.

Flexible medical article and method of making the same
11697001 · 2023-07-11 · ·

A method of making a flexible medical article or tube, for example, a sheath for a vascular access device, is provided. The method can include extruding a polymer, for example, a polycarbonate-urethane copolymer, to form a tube and annealing the extruded polymer. The method can further include cutting the extruded tube to a desired length before or after annealing, flaring one end of the annealed tube and over-molding the flared portion onto a hub, and forming the other end of the tube into a tip. A sheath formed by such a method is also provided.

Flexible medical article and method of making the same
11697001 · 2023-07-11 · ·

A method of making a flexible medical article or tube, for example, a sheath for a vascular access device, is provided. The method can include extruding a polymer, for example, a polycarbonate-urethane copolymer, to form a tube and annealing the extruded polymer. The method can further include cutting the extruded tube to a desired length before or after annealing, flaring one end of the annealed tube and over-molding the flared portion onto a hub, and forming the other end of the tube into a tip. A sheath formed by such a method is also provided.

Blown-Form Identification in a Blown Film System
20230211540 · 2023-07-06 ·

The invention relates to a blown film system for producing a film tube made of plastics material, comprising: an annular nozzle, out of which a plastic melt having a closed cross-section can be brought; a take-up device, by means of which the plastic melt can be drawn up from the direction of the annular nozzle so as to form the film tube; an air-provision device, which is downstream of the annular nozzle when viewed in the transport direction of the film tube and by means of which an amount of air can be provided; and a calibration device, which is downstream of the annular nozzle when viewed in the transport direction of the film tube and surrounds the film tube and by means of which the outer circumference of the film tube can be delimited. At least one detector is contained that has a plurality of detection elements, by means of which electromagnetic radiation emitted or reflected at various points of the film tube can be detected, such that at least one planar region and/or contoured region of the film tube can be detected with regard to characteristic properties, wherein the detector comprises at least 32 detection elements.

Continuous press-molding method and heating machine therefor
11548203 · 2023-01-10 · ·

A strip-shape softened resin sheet (S) which is continuously extruded from a molten resin extruder is cut to a unit resin sheet and a press molded product is manufactured by press-molding the unit resin sheet in a press-molding machine 20. Prior to press-molding the unit resin sheet (U) by the press-molding machine, the unit resin sheet (U) is heated by a heating machine 16. The heating machine 16 comprises a first heating furnace 84 and a second heating furnace 86. The first heating furnace 84 includes a series of heaters 84-3 and 84-4 whose heat source is infrared ray in a far-infrared region and the second heating furnace 86 includes a series of heaters 86-3 and 86-4 whose heat source is the infrared ray in a middle-infrared region. In the first furnace 84, the unit resin sheet (U) is continuously conveyed with a low velocity and is gradually heated by the far-infrared ray up to temperature which is slightly lower than the temperature which is suitable for press-molding the unit resin sheet (U). In the second furnace 86, the unit resin sheet (U) is stopped and is rapidly heated by the middle-infrared ray. By efficiently heating the unit resin sheet (U), a cycle time can be shortened and the production speed can be improved.

Crosslinked polyolefin separator and manufacturing method thereof
11545718 · 2023-01-03 · ·

A method for manufacturing a crosslinked polyolefin separator and a separator are provided. The method includes putting a polyolefin and a polyolefin elastomer into an extruder first, and putting an alkoxy silane containing a carbon-carbon double bond functional group, an initiator and a crosslinking catalyst to form the separator. The crosslinked polyolefin separator has high meltdown temperature and low shutdown temperature.

Crosslinked polyolefin separator and manufacturing method thereof
11545718 · 2023-01-03 · ·

A method for manufacturing a crosslinked polyolefin separator and a separator are provided. The method includes putting a polyolefin and a polyolefin elastomer into an extruder first, and putting an alkoxy silane containing a carbon-carbon double bond functional group, an initiator and a crosslinking catalyst to form the separator. The crosslinked polyolefin separator has high meltdown temperature and low shutdown temperature.

METHOD FOR MANUFACTURING LCP FILM FOR CIRCUIT SUBSTRATE AND T-DIE MELT-EXTRUDED LCP FILM FOR CIRCUIT SUBSTRATE
20220418111 · 2022-12-29 · ·

Provided is a method for manufacturing an LCP film for a circuit substrate capable of achieving an LCP film for a circuit substrate having a low coefficient of linear thermal expansion and excellent dimensional stability, without excessively impairing excellent basic performance possessed by the liquid crystal polyester, such as mechanical characteristics, electrical characteristics, and heat resistance. The method for manufacturing an LCP film for a circuit substrate at least comprising: a composition provision step of providing an LCP resin composition at least containing 100 parts by mass of a liquid crystal polyester and 1 to 20 parts by mass of a polyarylate; a film forming step of T-die melt-extruding the LCP resin composition to form a T-die melt-extruded LCP film having a coefficient of linear thermal expansion (α2) in a TD direction of 50 ppm/K or more; and a pressurizing and heating step of subjecting the T-die melt-extruded LCP film to pressure and heat treatment to obtain an LCP film for a circuit substrate having a coefficient of linear thermal expansion (α2) in the TD direction of 16.8±12 ppm/K.

METHOD FOR MANUFACTURING LCP FILM FOR CIRCUIT SUBSTRATE AND T-DIE MELT-EXTRUDED LCP FILM FOR CIRCUIT SUBSTRATE
20220418111 · 2022-12-29 · ·

Provided is a method for manufacturing an LCP film for a circuit substrate capable of achieving an LCP film for a circuit substrate having a low coefficient of linear thermal expansion and excellent dimensional stability, without excessively impairing excellent basic performance possessed by the liquid crystal polyester, such as mechanical characteristics, electrical characteristics, and heat resistance. The method for manufacturing an LCP film for a circuit substrate at least comprising: a composition provision step of providing an LCP resin composition at least containing 100 parts by mass of a liquid crystal polyester and 1 to 20 parts by mass of a polyarylate; a film forming step of T-die melt-extruding the LCP resin composition to form a T-die melt-extruded LCP film having a coefficient of linear thermal expansion (α2) in a TD direction of 50 ppm/K or more; and a pressurizing and heating step of subjecting the T-die melt-extruded LCP film to pressure and heat treatment to obtain an LCP film for a circuit substrate having a coefficient of linear thermal expansion (α2) in the TD direction of 16.8±12 ppm/K.