B01J29/084

ACRYLIC ACID PRODUCTION PROCESS

Provided herein are methods of producing acrylic acid from bPL. Such methods involve the use of a heterogeneous catalyst, such as a zeolite at vapor phase conditions. The method may use a fixed bed, moving bed or fluidized contacting zone as the reactor configurations.

Control of fluid catalytic cracking process for minimizing additive usage in the desulfurization of petroleum feedstocks

A method and apparatus for the cracking of a petroleum oil feedstock to produce a desulfurized full-range gasoline product. The petroleum oil feedstock is contacted with a base cracking catalyst and an FCC additive in an FCC unit, wherein the catalyst includes a stable Y-type zeolite and a rare-earth metal oxide and the additive includes a shape selective zeolite. The catalyst, additive and petroleum oil feedstock can be contacted in a down-flow or riser fluid catalytic cracking unit, that can also include a regeneration zone, a separation zone, and a stripping zone. The FCC unit includes an integrated control and monitoring system that monitors at least one parameter selected from FCC operating parameters, feed rate, feedstock properties, and product stream properties, and adjusts at least one parameter in response to the measured parameter to increase production of desulfurized products.

Catalysts containing nano-materials and methods of making and using same

A method of making a catalyst containing nanosize zeolite particles supported on a support material is disclosed. A process for making styrene or ethylbenzene by reacting toluene with a C.sub.1 source over a catalyst containing nanosize zeolite particles supported on a support material is disclosed.

MODIFIED USY ZEOLITIC CATALYST FOR ISOMERIZATION OF ALKYLATED AROMATICS, AND METHOD FOR ISOMERIZATION OF ALKYLATED AROMATICS
20220234033 · 2022-07-28 ·

The present invention relates to a catalyst for isomerization of alkylated aromatics such as mixed xylenes, using xylene isomerization catalyst particles including post-framework modified USY zeolite in which zirconium atoms and/or titanium atoms and/or hafnium atoms form a part of a framework of an ultra-stable Y-type zeolite.

Catalytic cracking process and catalyst system therefor

A catalytic cracking process includes a step of contacting a cracking feedstock with a catalytic cracking catalyst in the presence of a radical initiator for reaction under catalytic cracking conditions. The radical initiator contains a dendritic polymer and/or a hyperbranched polymer. The dendritic polymer and the hyperbranched polymer each independently has a degree of branching of about 0.3-1, and each independently has a weight average molecular weight of greater than about 1000. The catalytic cracking process is beneficial to enhancing and accelerating the free radical cracking of petroleum hydrocarbon and promoting the regulation of cracking activity and product distribution; by using the process disclosed herein, the conversion of catalytic cracking can be improved, the yields of ethylene and propylene can be increased, and the yield of coke can be reduced.

LIQUID-SOLID AXIAL MOVING BED REACTION AND REGENERATION DEVICE, AND SOLID ACID ALKYLATION METHOD

A liquid-solid axial moving bed reaction and regeneration apparatus and a solid acid alkylation process by using the liquid-solid axial moving bed reaction and regeneration apparatus. the liquid-solid axial moving bed reaction and regeneration apparatus comprise:

An axial moving bed reactor (1), a spent catalyst receiver (5), a catalyst regenerator (4) and a regenerated catalyst receiver (6) that are successively connected, wherein, a catalyst outlet of the regenerated catalyst receiver (6) is communicated with a catalyst inlet of the axial moving bed reactor (1);

Wherein, the axial moving bed reactor (1) is provided with at least two catalyst beds (3) arranged up and down, the axial moving bed reactor (1) is provided with a feed inlet (2) above each catalyst bed (3);

A catalyst delivery pipe (16) is arranged between two adjacent catalyst beds (3) so that the catalyst can move from top to bottom in the axial moving bed reactor (1);

A separation component (10) is provided between two adjacent catalyst beds (3), the inside space of the separation component (10) is communicated with the catalyst delivery pipe (16), the separation component (10) is for separating the stream after the reaction in the upstream catalyst bed from the catalyst, the catalyst obtained by the separation with the separation component (10) moves down through the catalyst delivery pipe (16).

Phosphorus-containing high-silica molecular sieve, its preparation and application thereof

Disclosed are a phosphorus-containing high-silica molecular sieve, its preparation and application thereof, wherein the molecular sieve comprises about 86.5-99.8 wt % of silicon, about 0.1-13.5 wt % of aluminum and about 0.01-6 wt % of phosphorus, calculated as oxides and based on the dry weight of the molecular sieve, the molecular sieve has an XRD pattern with at least three diffraction peaks, the first strong peak is present at a diffraction angle of about 5.9-6.9°, the second strong peak is present at a diffraction angle of about 10.0-11.0°, and the third strong peak is present at a diffraction angle of about 15.6-16.7°. The phosphorus-containing high-silica molecular sieve shows an improved hydrocracking activity in the presence of nitrogen-containing species when used in the preparation of hydrocracking catalysts.

Process for producing BTX by catalytic pyrolysis from biomass with injection of oxygenated compounds

A process is described for producing a BTX cut from biomass comprising at least one step of catalytic pyrolysis of said biomass in a fluidized-bed reactor in which a stream comprising at least one oxygenated compound selected from alcohols having 2 to 12 carbon atoms, alcohol acids having 2 to 12 carbon atoms, diols having 2 to 12 carbon atoms, carboxylic acids having 2 to 12 carbon atoms, ethers having 2 to 12 carbon atoms, aldehydes having 2 to 12 carbon atoms, esters having 2 to 12 carbon atoms and glycerol, alone or mixed, is fed into the catalytic pyrolysis reactor.

MFI STRUCTURE MOLECULAR SIEVE RICH IN MESOPORE, PREPARATION METHOD THEREFOR, AND CATALYST CONTAINING SAME AND APPLICATION THEREOF

A molecular sieve of MFI structure has a ratio of n(SiO2)/n(Al2O3) of more than 15 and less than 70. It has a content of phosphorus of 1-15 wt %, calculated as P.sub.2O.sub.5 and based on the dry weight of the molecular sieve and a content of the supported metal in the molecular sieve 1-10 wt % based on the oxide of the supported metal and the dry weight of the molecular sieve. The supported metal is one or two selected from lanthanum and cerium. The volume of mesopores in the molecular sieve represents 40-70% by volume of the total pore volume of the molecular sieve by volume, measured by a nitrogen adsorption BET specific surface area method, and the volume of mesopores means the pore volume of the pores having a diameter of more than 2 nm and less than 100 nm.

Catalytic composition and structures made thereof

A catalytic composition is built up from a ceramic material including a catalytic material and a first inorganic binder and a second inorganic binder and a catalytic structure made thereof. Preferably, the structure is made by a colloidal ceramic shaping technique. The structure is usable for catalytic or ion exchange applications as well. It is demonstrated that the catalytic structures have excellent mechanical, physicochemical and catalytic properties.