B01J29/085

Modified Y-type molecular sieve, preparation thereof and catalyst comprising the same

A modified Y-type molecular sieve has a rare earth oxide content of about 4% to about 12% by weight, a phosphorus content of about 0% to about 10% by weight, a sodium oxide content of no more than about 1.0% by weight, a total pore volume of about 0.36 to 0.48 mL/g, a percentage of the pore volume of secondary pores to the total pore volume of about 20% to about 40%, a lattice constant of about 2.440 nm to about 2.455 nm, a percentage of the non-framework aluminum content to the total aluminum content of no more than about 10%, a lattice collapse temperature of not lower than about 1060 C., and a ratio of Brnsted acid to Lewis acid of no less than about 3.50. The preparation of the molecular sieve includes ion-exchange with rare earth, hydrothermal roasting, gas phase ultra-stabilization, acid treatment, and an optional phosphorus modification.

Catalytic cracking catalyst and preparation thereof

A catalytic cracking catalyst has a rare earth modified Y-type molecular sieve, an additive-containing alumina binder, and a clay. The rare earth modified Y-type molecular sieve has a rare earth oxide content of about 4-12 wt %, a phosphorus content of about 0-10 wt %, a sodium oxide content of no more than about 1.0 wt %, a total pore volume of about 0.36-0.48 mL/g, a percentage of the pore volume of secondary pores having a pore size of 2-100 nm to the total pore volume of about 20-40%, a lattice constant of about 2.440-2.455 nm, a percentage of non-framework aluminum content to the total aluminum content of no more than about 10%, a lattice collapse temperature of not lower than about 1060 C., and a ratio of B acid to L acid in the total acid content of the modified Y-type molecular sieve of no less than about 3.50.

Aromatization Catalyst and Methods of Making and Using Same
20200338532 · 2020-10-29 ·

A process of making an aromatization catalyst comprising: (a) mixing a zeolite, a binder, and water to form a mixture; (b) extruding the mixture to form a green extrudate; (c) drying the green extrudate to form a dried green extrudate; (d) calcining the dried green extrudate to form a support, wherein calcining the dried green extrudate is the only calcination step in the process; (e) washing the support to form a washed support; (f) drying the washed support to form a dried washed support; (g) impregnating the dried washed support with a Group 8-10 transition metal compound and at least one halide-containing compound to form a metalized-halided material; and (h) vacuum drying the metalized-halided material to form a dried metalized-halided material which is the aromatization catalyst.

FCC CATALYST WITH ENHANCED MESOPOROSITY, ITS PREPARATION AND USE

Process for the preparation of a catalyst and a catalyst comprising enhanced mesoporosity is provided herein. Thus, in one embodiment, provided is a particulate FCC catalyst comprising 2 to 50 wt % of one or more ultra stabilized high Si02/A1203 ratio large pore faujasite zeolite or a rare earth containing USY, 0 to 50 wt % of one or more rare-earth exchanged large pore faujasite zeolite, 0 to 30 wt % of small to medium pore size zeolites, 5 to 45 wt % quasi-crystalline boehmite 0 to 35 wt % microcrystalline boehmite, 0 to 25 wt % of a first silica, 2 to 30 wt % of a second silica, 0.1 to 10 wt % one or more rare earth components showiomg enhanced mesoporosity in the range of 6-40 nm, the numbering of the silica corresponding to their orders of introduction in the preparation process.

PHOSPHORUS-CONTAINING MOLECULAR SIEVE, ITS PREPARATION AND APPLICATION THEREOF
20200338540 · 2020-10-29 ·

A phosphorus-containing molecular sieve has a phosphorus content of about 0.3-5 wt %, a pore volume of about 0.2-0.95 ml/g, and a ratio of B acid content to L acid content of about 2-10. The molecular sieve has a specific combination of characteristics, including a high ratio of B acid content to L acid content, thereby exhibiting higher hydrocracking activity and ring-opening selectivity when used in the preparation of a hydrocracking catalyst.

Production of Methyl-substituted Biphenyl Compounds
20200325086 · 2020-10-15 ·

In a process for producing a methyl-substituted biphenyl compound, at least one methyl-substituted cyclohexylbenzene compound of the formula:

##STR00001##

wherein each of m and n is independently 1, 2, or 3, is contacted with hydrogen in the presence of a hydrogenation catalyst to produce a hydrogenation reaction product comprising at least one methyl-substituted bicyclohexane compound, and the methyl-substituted bicyclohexane compound is then contacted with a dehydrogenation catalyst to produce a dehydrogenation reaction product comprising at least one methyl-substituted biphenyl compound.

Additive and a catalyst composition comprising the additive for FCC process

The present disclosure relates to an additive and a catalyst composition for a catalytic cracking process of vacuum gas oil for preparing cracked run naphtha having reduced liquid olefin content, and increased propylene and butylene yields in the LPG fraction. The process makes use of a catalyst composition which is a mixture of an FCC equilibrated catalyst and an additive comprising a zeolite, phosphorus and a combination of metal promoters. The process is successful in achieving high propylene and butylene yields in the LPG fraction along with a lower liquid olefin content and increased aromatic content with increase in RON unit in the resultant cracked run naphtha, as compared to that achieved using an FCC equilibrated catalyst alone.

Disproportionation and transalkylation of heavy aromatic hydrocarbons

Disclosed herein is a process for producing para-xylene comprising the steps of: (a) contacting a feedstock comprising toluene with a first catalyst under effective vapor phase toluene disproportionation conditions to disproportionate said toluene and produce a first product comprising benzene, unreacted toluene and greater than equilibrium amounts of para-xylene; and (b) contacting a feedstock comprising C.sub.9+ aromatic hydrocarbons and benzene with a second catalyst in the presence of 0 wt. % or more of hydrogen having a 0 to 10 hydrogen/hydrocarbon molar ratio under effective C.sub.9+ transalkylation conditions to transalkylate said C.sub.9+ aromatic hydrocarbons and produce a second product comprising xylenes.

CATALYST STRUCTURE AND METHOD OF UPGRADING HYDROCARBONS IN THE PRESENCE OF THE CATALYST STRUCTURE
20200261894 · 2020-08-20 ·

A catalyst structure includes a porous support structure, where the support structure includes an aluminosilicate material. Any two or more metals are loaded in the porous support structure, the two or more metals selected from the group consisting of Ga, Ag, Mo, Zn, Co and Ce, where each metal loaded in the porous support structure is present in an amount from about 0.1 wt % to about 20 wt %. In example embodiments, the catalyst structure includes three or more of the metals loaded in the porous support structure. The catalyst structure is used in a hydrocarbon upgrading process that is conducted in the presence of methane, nitrogen or hydrogen.

PREPARATION OF METAL-IN-HOLLOW-ZEOLITE-BASED CATALYST FOR SELECTIVE BENZENE ALKYLATION

The invention is directed to hollow zeolite encapsulated metal particle catalysts where the metal particle is contained in the hollow of the zeolite, their preparation method by depositing metal particle precursors and subsequent removal of said metal particle precursors from the surface of the hollow zeolite while retaining those in the cavity of the hollow zeolite, and the catalysts' use in selective benzene alkylation.