B01J29/26

Catalyst for converting alkylaromatic hydrocarbon and preparation method thereof

Disclosed are a bifunctional catalyst and a preparation method therefor, the bifunctional catalyst being suitable to produce high-value aromatic hydrocarbons by subjecting alkylaromatic hydrocarbons to a disproportionation/transalkylation/dealkylation reaction while suppressing aromatic loss or subjecting C8 aromatic hydrocarbons to an isomerization reaction while suppressing xylene loss.

COATED HYDROPROCESSING CATALYST
20220241760 · 2022-08-04 · ·

Embodiments of the present disclosure are directed to a coated hydroprocessing catalyst comprising: a hydroprocessing catalyst comprising a porous support and at least one metal supported on the porous support; wherein the porous support comprising silica, alumina, titania, or combinations thereof; and the at least one metal selected from IUPAC Groups 6, 9 and 10 metals; a catalyst activation agent, a catalyst deactivation agent, or both loaded onto pores of the porous support, the catalyst activation agent comprising at least one sulfur compound and the catalyst deactivation agent comprising at least one nitrogen compound; and a coating layer on a surface of the hydroprocessing catalyst, the coating layer encapsulating the catalyst activation agent, the catalyst deactivation agent, or both within the hydroprocessing catalyst, wherein the 3coating layer comprises a polymer, or a paraffinic oil.

CARBONYLATION-DEHYDRATION DUAL-FUNCTIONAL CATALYST PRECURSOR, PREPARATION METHOD THEEOF, CARBONYLATION-DEHYDRATION DUAL-FUNCTIONAL CATALYST AND USE THEREOF

A carbonylation-dehydration dual-functional catalyst precursor, a preparation method thereof, a carbonylation-dehydration dual-functional catalyst and use thereof are provided. The carbonylation-dehydration dual-functional catalyst precursor includes a modified silica-aluminum molecular sieve having an 8-member ring channel structure; a modified metal oxie loaded on the modified silica-aluminum molecular sieve having an 8-member ring channel structure by coupling, the coupling being performed using a silane coupling agent, wherein a modified component in the modified silica-aluminum molecular sieve having an 8-member ring channel structure includes at least one selected from the group consisting of copper oxide, zing oxide and iron oxide, and has a loading amount of 0.5-5 wt %, based on a metal mass of the modified component; and the modified metal oxie is prepared by modifying a composite metal oxide with an acid solution or an alkali solution, wherein the composite metal oxide is prepared based on a co-precipitation-calcination method.

Three stage catalytic process for pyrolysis oil upgrading to xylenes

A method for upgrading pyrolysis oil includes contacting a pyrolysis oil feed with hydrogen in the presence of a mixed metal oxide catalyst in a slurry reactor to produce an intermediate stream comprising light aromatic compounds comprising mono-aromatic compounds, di-aromatic compounds, or both, passing the intermediate stream to a hydrocracking reactor, contacting the intermediate stream with hydrogen in the presence of a hydrocracking catalyst in a hydrocracking reactor to produce a hydrocracking effluent comprising aromatic compounds having six to nine carbon atoms, passing the hydrocracking effluent to a transalkylation reactor, and contacting the hydrocracking effluent with hydrogen in the presence of a transalkylation catalyst in the transalkylation reactor to produce a transalkylation effluent comprising xylenes.

Hydrocracking catalyst for preparing light aromatic hydrocarbon, method for preparing same and method for preparing light aromatic hydrocarbon by using same

The present disclosure relates to a hydrocracking catalyst for preparing a C.sub.6-C.sub.9 light aromatic hydrocarbons having an increased BTX content from a polycyclic aromatic hydrocarbon, a method for preparing the same and a method for preparing a C.sub.6-C.sub.9 light aromatic hydrocarbons having an increased BTX content by using the same. More specifically, an effect of obtaining a C.sub.6-C.sub.9 light aromatic hydrocarbons having an increased BTX content with a high yield from the byproducts of oil refining and petrochemical processes, which contain polycyclic aromatic hydrocarbons such as naphthalene, alkylnaphthalene, etc., can be achieved by using a catalyst in which one or more metal selected from group VIII and one or more metal selected from group VIB are supported on a composite zeolite support of zeolite beta and zeolite ZSM-5.

Methods of heavy reformate conversion into aromatic compounds

Method of making BTX compounds including benzene, toluene, and xylene, including feeding heavy reformate to a reactor containing a composite zeolite catalyst. The composite zeolite catalyst includes a mixture of layered mordenite (MOR-L) comprising a layered or rod-type morphology with a layer thickness less than 30 nm and ZSM-5. The MOR-L, the ZSM-5, or both include one or more impregnated metals. The method further includes producing the BTX compounds by simultaneously performing transalkylation and dealkylation of the heavy reformate in the reactor. The composite zeolite catalyst is able to simultaneously catalyze both the transalkylation and dealkylation reactions.

Methods of heavy reformate conversion into aromatic compounds

Method of making BTX compounds including benzene, toluene, and xylene, including feeding heavy reformate to a reactor containing a composite zeolite catalyst. The composite zeolite catalyst includes a mixture of layered mordenite (MOR-L) comprising a layered or rod-type morphology with a layer thickness less than 30 nm and ZSM-5. The MOR-L, the ZSM-5, or both include one or more impregnated metals. The method further includes producing the BTX compounds by simultaneously performing transalkylation and dealkylation of the heavy reformate in the reactor. The composite zeolite catalyst is able to simultaneously catalyze both the transalkylation and dealkylation reactions.

Composite hierarchical zeolite catalyst for heavy reformate conversion to xylenes

A method of producing a hierarchical zeolite composite catalyst. The method including dissolving, in an alkaline solution and in the presence of a surfactant, a catalyst precursor comprising mesoporous zeolite to yield a dissolved zeolite solution, where the mesoporous zeolite comprises large pore mordenite and medium pore ZSM-5. The method also including condensing the dissolved zeolite solution to yield a solid zeolite composite from the dissolved zeolite solution and heating the solid zeolite composite to remove the surfactant. The method further including impregnating the solid zeolite composite with one or more active metals selected from the group consisting of molybdenum, platinum, rhenium, nickel, and combinations thereof to yield impregnated solid zeolite composite and calcining the impregnated solid zeolite composite to produce the hierarchical zeolite composite catalyst. The hierarchical zeolite composite catalyst has a mesostructure comprising at least one disordered mesophase and at least one ordered mesophase.

Composite hierarchical zeolite catalyst for heavy reformate conversion to xylenes

A method of producing a hierarchical zeolite composite catalyst. The method including dissolving, in an alkaline solution and in the presence of a surfactant, a catalyst precursor comprising mesoporous zeolite to yield a dissolved zeolite solution, where the mesoporous zeolite comprises large pore mordenite and medium pore ZSM-5. The method also including condensing the dissolved zeolite solution to yield a solid zeolite composite from the dissolved zeolite solution and heating the solid zeolite composite to remove the surfactant. The method further including impregnating the solid zeolite composite with one or more active metals selected from the group consisting of molybdenum, platinum, rhenium, nickel, and combinations thereof to yield impregnated solid zeolite composite and calcining the impregnated solid zeolite composite to produce the hierarchical zeolite composite catalyst. The hierarchical zeolite composite catalyst has a mesostructure comprising at least one disordered mesophase and at least one ordered mesophase.

Heavy Aromatics Conversion Processes and Catalyst Compositions Used Therein

Disclosed are processes for conversion of a feedstock comprising C.sub.8+ aromatic hydrocarbons to lighter aromatic products in which the feedstock and optionally hydrogen are contacted in the presence of the catalyst composition under conversion conditions effective to dealkylate and transalkylate said C.sub.8+ aromatic hydrocarbons to produce said lighter aromatic products comprising benzene, toluene and xylene. The catalyst composition comprises a zeolite, a first metal, and a second metal, and is treated with a source of sulfur and/or a source of steam.