B22F3/1025

Manufacturing method for three-dimensional structure and manufacturing apparatus therefor

A manufacturing method for three-dimensional structure has a layer forming step of supplying a flowable composition containing a powder and an organic material to form a unit layer, an organic material removing step of performing a treatment of removing the organic material on the unit layer, and an energy applying step of applying energy to the unit layer after the organic material removing step to form a molten layer or sintered layer, wherein the layer forming step, the organic material removing step, and the energy applying step are repeated with respect to the molten layer or sintered layer in a stacking direction as appropriate.

Poppet valve and method of its manufacture

A method for manufacturing a poppet valve or mushroom valve includes providing a mixture of metal powder and a binder, filling and pressing said mixture in a mold, to obtain a green product, removing the binder from the green product, and thermally sintering the green product to a poppet valve blank, by hot isostatic pressing. A poppet valve is also provided that is manufactured with this method.

Poppet valve and method of its manufacture

A method for manufacturing a poppet valve or mushroom valve includes providing a mixture of metal powder and a binder, filling and pressing said mixture in a mold, to obtain a green product, removing the binder from the green product, and thermally sintering the green product to a poppet valve blank, by hot isostatic pressing. A poppet valve is also provided that is manufactured with this method.

Method for manufacturing three-dimensional shaped object
11759856 · 2023-09-19 · ·

A method for manufacturing a three-dimensional shaped object includes a structure shaping step (step S140) of shaping a structure with a shaping material including a metal powder or a ceramic powder, a support shaping step (step S130) of shaping a support T that supports a structure S with a support material including a resin, and a deresining step (step S210) of deresining the support T supporting the structure S.

Method for manufacturing three-dimensional shaped object
11759856 · 2023-09-19 · ·

A method for manufacturing a three-dimensional shaped object includes a structure shaping step (step S140) of shaping a structure with a shaping material including a metal powder or a ceramic powder, a support shaping step (step S130) of shaping a support T that supports a structure S with a support material including a resin, and a deresining step (step S210) of deresining the support T supporting the structure S.

Polymer ammunition and cartridge primer insert
11231258 · 2022-01-25 · ·

The present invention provides a polymer ammunition cartridge having a primer insert having: a top surface; a bottom surface opposite the top surface; a coupling element that extends from the bottom surface, wherein the coupling element comprises an interior surface and an exterior surface, wherein the interior surface comprises: a transition region that transitions from the bottom surface to a second segment wherein the transition region has a radius of from 0.02 to 0.2; a first segment extending from the second segment and terminates at a tip, wherein the first segment has a first segment distance from 0.02 to 0.18 inches and the second segment has a second segment distance from 0.02 to 0.18 inches, wherein the second segment has a second segment angle from +3 to −3 degrees relative to the first segment angle and the first segment has a first segment angle from +6 to −6 degrees from perpendicular to the top surface; a primer recess in the top surface that extends toward the bottom surface; a primer flash aperture positioned in the primer recess through the bottom surface; and a flash aperture groove in the primer recess and positioned around the primer flash aperture and adapted to receive a polymer overmolding through the primer flash aperture.

Polymer ammunition and cartridge primer insert
11231258 · 2022-01-25 · ·

The present invention provides a polymer ammunition cartridge having a primer insert having: a top surface; a bottom surface opposite the top surface; a coupling element that extends from the bottom surface, wherein the coupling element comprises an interior surface and an exterior surface, wherein the interior surface comprises: a transition region that transitions from the bottom surface to a second segment wherein the transition region has a radius of from 0.02 to 0.2; a first segment extending from the second segment and terminates at a tip, wherein the first segment has a first segment distance from 0.02 to 0.18 inches and the second segment has a second segment distance from 0.02 to 0.18 inches, wherein the second segment has a second segment angle from +3 to −3 degrees relative to the first segment angle and the first segment has a first segment angle from +6 to −6 degrees from perpendicular to the top surface; a primer recess in the top surface that extends toward the bottom surface; a primer flash aperture positioned in the primer recess through the bottom surface; and a flash aperture groove in the primer recess and positioned around the primer flash aperture and adapted to receive a polymer overmolding through the primer flash aperture.

Polymer Cartridge Having a Primer Insert With a Primer Pocket Groove
20220018639 · 2022-01-20 · ·

The present invention provides an ammunition cartridge having a primer insert having a top surface opposite a bottom surface and a extraction flange that extends circumferentially about an outer edge of the top surface; a coupling element that extends from the bottom surface, wherein the substantially cylindrical coupling element is adapted to receive a polymer overmolding; a primer recess in the top surface that extends toward the bottom surface, wherein the primer recess comprises a recess bottom and a circular recess side wall; a primer flash aperture through the recess bottom that extends through the bottom surface, wherein the primer flash aperture is adapted to receive a polymer overmolding to form a flash hole; and a groove in the primer recess positioned around the primer flash aperture adapted to receive a polymer overmolding, wherein the groove extends at least partially over the bottom surface and the circular recess side wall and the groove is adapted to receive polymer through the primer flash aperture and over the bottom surface and the circular recess side wall.

Polymer ammunition and cartridge primer insert
11226179 · 2022-01-18 · ·

The present invention provides a polymer ammunition cartridge having a primer insert having: a top surface; a bottom surface opposite the top surface; a coupling element that extends from the bottom surface, wherein the coupling element comprises an interior surface and an exterior surface, wherein the interior surface comprises: a transition region that transitions from the bottom surface to a second segment wherein the transition region has a radius of from 0.02 to 0.2; a first segment extending from the second segment and terminates at a tip, wherein the first segment has a first segment distance from 0.02 to 0.18 inches and the second segment has a second segment distance from 0.02 to 0.18 inches, wherein the second segment has a second segment angle from +3 to −3 degrees relative to the first segment angle and the first segment has a first segment angle from +6 to −6 degrees from perpendicular to the top surface; a primer recess in the top surface that extends toward the bottom surface; a primer flash aperture positioned in the primer recess through the bottom surface; and a flash aperture groove in the primer recess and positioned around the primer flash aperture and adapted to receive a polymer overmolding through the primer flash aperture.

Polymer ammunition and cartridge primer insert
11226179 · 2022-01-18 · ·

The present invention provides a polymer ammunition cartridge having a primer insert having: a top surface; a bottom surface opposite the top surface; a coupling element that extends from the bottom surface, wherein the coupling element comprises an interior surface and an exterior surface, wherein the interior surface comprises: a transition region that transitions from the bottom surface to a second segment wherein the transition region has a radius of from 0.02 to 0.2; a first segment extending from the second segment and terminates at a tip, wherein the first segment has a first segment distance from 0.02 to 0.18 inches and the second segment has a second segment distance from 0.02 to 0.18 inches, wherein the second segment has a second segment angle from +3 to −3 degrees relative to the first segment angle and the first segment has a first segment angle from +6 to −6 degrees from perpendicular to the top surface; a primer recess in the top surface that extends toward the bottom surface; a primer flash aperture positioned in the primer recess through the bottom surface; and a flash aperture groove in the primer recess and positioned around the primer flash aperture and adapted to receive a polymer overmolding through the primer flash aperture.