METHOD FOR PRODUCING STRETCHED FILM

In a method for producing a stretched film by stretching a film web containing a poly(3-hydroxybutyrate) resin, the film web is stretched under conditions where a film surface maximum temperature is within a temperature range represented by the following inequality:

Tm-60film surface maximum temperature ( C.)Tm-5, where the Tm is a melting point ( C.) of the film web.