Patent classifications
B29C66/7352
HEAT-SEALABLE PACKAGING MATERIAL
The present invention is directed to a packaging material free from aluminium in the form of a continuous foil or film, comprising a layer of microfibrillated cellulose (MFC), wherein the layer comprising MFC has been laminated or coated on at least one side with a heat-sealable material. The MFC layer contains at least 60% by weight of microfibrillated cellulose. The present invention is also directed to a method for induction sealing, wherein a packaging material to be heat-sealed by induction is placed against an induction heating surface.
Heat Sealer Provided with Interfacial Temperature Sensor
The embodiment provides a heat-sealing apparatus and a method of accurately controlling heat sealing temperature by measuring the temperature using a heat-sealing apparatus which heat-seals a pair of heat seal materials by nipping them between a pair of heating bodies. The method of heat-sealing includes mounting a cover material on the surface of at least one of the heating bodies to be in contact with the heat seal material, attaching a minute temperature sensor to the surface of the cover material on the side to be in contact with the heat seal material, and controlling temperature of welding face by the temperature detected by the minute temperature sensor, and an apparatus therefor.
LOCALIZED PANEL STIFFENER
A device (10) comprising a carrier material (14) and a matrix material (12) deposited onto the carrier material in a pattern that leaves a predetermined amount of space (18) between each deposition of matrix material.
PRE-TREATMENT COMPOSITION
The present disclosure relates to a pre-treatment composition for sealing polymeric film, said composition comprising: 0.5 to 10 weight % of a halogenated carboxylic acid, a surfactant, and a liquid solvent.
HIGH-SPEED POLYMER-TO-METAL DIRECT JOINING SYSTEM AND METHOD
A method of directly joining a polymer to a metal along a joint interface through the formation of CO-M chemical bonds, where M represents an element in the metal to be joined. The method includes heating the metal to a predetermined temperature above a glass transition temperature of the polymer and less than a flash ignition temperature of the polymer and less than a metal melting temperature of the metal; physically contacting at least one of the metal and the polymer; and applying compression pressure to the joint interface of the metal and the polymer when the metal is above the glass transition temperature of the polymer and less than the flash ignition temperature of the polymer and less than the metal melting temperature of the metal to generate intimate atomic contact between the metal and the polymer to create CO-M chemical bonds between the metal and the polymer.
Laser welding member, and molded article
A laser welding member that has a high laser transmittance at a welding region and exhibits an excellent laser welding processability, and a molded article obtained by laser welding using this laser welding member. The laser welding member is obtained by injection molding of a thermoplastic polyester resin material, wherein a region to be laser welded in the member is at a location separated by a distance of at least 15 mm from a gate of an injection molding mold and has at least 30% of a light transmittance of laser light with a wavelength of 940 nm.
INTERNAL TENSIONING STRUCTURE USEABLE WITH INFLATABLE DEVICES
An internal tensioning structure for use in an inflatable product fulfills the basic function of maintaining two adjacent inflatable surfaces in a desired geometric arrangement when the inflatable product is pressurized. The tensioning structure is formed by connecting a pair of plastic strips sheets via spaced-apart strands, such as strings or wires. When pulled taut, the strands provide a high tensile strength between the two opposed plastic strips. At the same time, the plastic strips facilitate a strong, long-lasting weld between the tensioning structure and the inflatable product.
METHOD FOR WELDING MEMBRANES
A process for welding porous membranes, the process containing i) providing first and second porous membranes; ii) at least partially superimposing the first and second porous membranes to obtain an at least partial superimposition region; iii) welding the first and second porous membranes at least in a portion of the at least one superimposition region at a temperature in the range from 100 to 300 C. to obtain an at least partially welded composite of the first and second porous membranes, wherein the first and second porous membranes are made of at least one thermoplastic elastomer selected from the group consisting of a polyurethane elastomer, a polyester elastomer, a polyetherester elastomer, a polyesterester elastomer, a polyamide elastomer, a polyetheramide elastomer, a polystyrene elastomer, and an ethylene-vinyl acetate elastomer, and wherein the first and second porous membranes have pores having an average pore diameter of less than 2000 nm.
Ultrasonic welding systems and methods using dual, synchronized horns on opposite sides of parts to be joined
An ultrasonic system and method for sealing a complex interface, such as a Gable top, having multiple and a variety of layers across the interface, or an oval or round spout having a complex geometry. The system includes two ultrasonic horns arranged opposite a gap between which the interface is provided. The frequency and phase of the ultrasonic energy are synchronized as the energy is applied simultaneously while the interface is pressed between a jaw and the energy is applied to both sides of the interface. Only one application of the frequency- and phase-synchronized ultrasonic energy is required to hermetically seal all the layers of the interface together.
Localized panel stiffener
A device (10) comprising a carrier material (14) and a matrix material (12) deposited onto the carrier material in a pattern that leaves a predetermined amount of space (18) between each deposition of matrix material.