B29C48/67

Extruder screw with alternately-arranged conveyance portions and extruders and extrusion methods using the extruder screw

A conveyance portion, a barrier portion, and a path are provided at places of a screw main body in which a kneading portion is provided. In at least one of the places, the path is provided inside the screw main body, and includes an entrance and an exit. The entrance is opened to urge the raw materials having the conveyance limited by the barrier portion to increase pressure on the raw materials, to flow in the entrance. The raw materials flowing from the entrance flow through the path in the same direction as a conveyance direction of the conveyance portion.

Extruder screw including conveyance portions and paths within the conveyance portions, extruder, and extrusion method

At a part of the screw main body at which the kneading portion is provided, conveyance portions, a barrier portion and a path are provided at a plurality of places. At least one of the places, the path is provided inside the screw main body, and includes an entrance and an exit. The entrance is opened in such a manner that the raw material whose pressure is enhanced by being restricted in conveyance by the barrier portion flows into the entrance. The path is formed in such a manner that the raw material flowing into the path from the entrance flows toward the exit in a direction opposite to the direction of conveyance.

Extruder screw including conveyance portions and paths within the conveyance portions, extruder, and extrusion method

At a part of the screw main body at which the kneading portion is provided, conveyance portions, a barrier portion and a path are provided at a plurality of places. At least one of the places, the path is provided inside the screw main body, and includes an entrance and an exit. The entrance is opened in such a manner that the raw material whose pressure is enhanced by being restricted in conveyance by the barrier portion flows into the entrance. The path is formed in such a manner that the raw material flowing into the path from the entrance flows toward the exit in a direction opposite to the direction of conveyance.

In Situ Exfoliation Method to Fabricate a Graphene-Reinforced Polymer Matrix Composite

A method for forming a graphene-reinforced polymer matrix composite is disclosed. The method includes distributing graphite microparticles into a molten thermoplastic polymer phase; and applying a succession of shear strain events to the molten polymer phase so that the molten polymer phase exfoliates the graphite successively with each event until at least 50% of the graphite is exfoliated to form a distribution in the molten polymer phase of single- and multi-layer graphene nanoparticles less than 50 nanometers thick along the c-axis direction.

In Situ Exfoliation Method to Fabricate a Graphene-Reinforced Polymer Matrix Composite

A method for forming a graphene-reinforced polymer matrix composite is disclosed. The method includes distributing graphite microparticles into a molten thermoplastic polymer phase; and applying a succession of shear strain events to the molten polymer phase so that the molten polymer phase exfoliates the graphite successively with each event until at least 50% of the graphite is exfoliated to form a distribution in the molten polymer phase of single- and multi-layer graphene nanoparticles less than 50 nanometers thick along the c-axis direction.

Continuous methods of making fiber reinforced concrete panels

Continuous method including mixing water and cementitous powder to form slurry; mixing the slurry and reinforcement fibers in a single pass horizontal continuous mixer to form fiber-slurry mixture, the mixer including an elongated mixing chamber having a reinforcement fiber inlet port, and upstream of the fiber inlet port is an inlet port to introduce water and cementitous powder together as one stream or at least two inlet ports to introduce water and dry cementitous powder separately as separate streams into the chamber, a rotating horizontal shaft/s within the chamber, part of the chamber for mixing the fibers and slurry and moving the fiber-slurry mixture to a mixture outlet; discharging the fiber-slurry mixture from the mixer outlet; forming and setting the fiber-slurry mixture on a moving surface; cutting the set mixture into fiber reinforced concrete panels and removing the panels from the moving surface.

Continuous methods of making fiber reinforced concrete panels

Continuous method including mixing water and cementitous powder to form slurry; mixing the slurry and reinforcement fibers in a single pass horizontal continuous mixer to form fiber-slurry mixture, the mixer including an elongated mixing chamber having a reinforcement fiber inlet port, and upstream of the fiber inlet port is an inlet port to introduce water and cementitous powder together as one stream or at least two inlet ports to introduce water and dry cementitous powder separately as separate streams into the chamber, a rotating horizontal shaft/s within the chamber, part of the chamber for mixing the fibers and slurry and moving the fiber-slurry mixture to a mixture outlet; discharging the fiber-slurry mixture from the mixer outlet; forming and setting the fiber-slurry mixture on a moving surface; cutting the set mixture into fiber reinforced concrete panels and removing the panels from the moving surface.

EXTRUDER SCREW HAVING PATHS WITHIN THE SCREW, EXTRUDER, AND EXTRUSION METHOD

A conveyance portion, a barrier portion, and a path are provided at places of a portion of a screw main body in which a kneading portion is provided. In at least one of the places, an entrance is opened to cause raw materials, conveyance of which is limited by a barrier portion to increase pressure on the raw materials, to flow in. The raw materials flowing in from the entrance flow through the path in the opposite direction to a conveyance direction of the conveyance portion. An exit is opened in an outer circumferential surface of the screw main body at a position outside the conveyance portion in which the entrance is opened.

EXTRUDER SCREW HAVING PATHS WITHIN THE SCREW, EXTRUDER, AND EXTRUSION METHOD

A conveyance portion, a barrier portion, and a path are provided at places of a portion of a screw main body in which a kneading portion is provided. In at least one of the places, an entrance is opened to cause raw materials, conveyance of which is limited by a barrier portion to increase pressure on the raw materials, to flow in. The raw materials flowing in from the entrance flow through the path in the opposite direction to a conveyance direction of the conveyance portion. An exit is opened in an outer circumferential surface of the screw main body at a position outside the conveyance portion in which the entrance is opened.

Liquid Crystalline Polymer Composition
20220025153 · 2022-01-27 ·

A compact camera module that contains a generally planar base on which is mounted a lens barrel is provided. The base, barrel, or both are molded from a polymer composition that includes a thermotropic liquid crystalline polymer and a plurality of mineral fibers (also known as “whisker”). The mineral fibers have a median width of from about 1 to about 35 micrometers and constitute from about 5 wt. % to about 60 wt. % of the polymer composition.