B29C66/73115
METHOD OF PRODUCTION OF FABRIC BAGS OR CONTAINERS USING HEAT FUSED SEAMS
A method of producing flexible polypropylene fabric bags with heat fused seams comprising providing fabric pieces, wherein each fabric piece has a coated side and an uncoated side; positioning fabric pieces so that a coated side of one fabric piece faces a coated side of another fabric piece; selecting an area of fabric to be joined for forming a seam or joint; applying heat to the area to be joined that is less than the melting point of the fabrics, for forming one or more seams or joints and wherein the heat fused seams or joints of a resulting polypropylene bag retains at least 85% of the fabric strength without using sewing machines.
IMPLANTABLE MEDICAL DEVICE WITH METAL AND POLYMER HOUSING
In some examples, manufacturing techniques for implantable medical devices are described. An example method may including positioning a metal housing component adjacent to a polymer housing component so that there is an interface between the metal housing component and the polymer housing component; and forming a seal at the interface between the metal housing component and the polymer housing component to join the metal housing component and the polymer housing component, wherein the joined metal housing component and the polymer housing component form at least a portion of housing for the implantable medical device, wherein the housing of the implantable medical device contains electronic circuitry.
ULTRASONIC WELDING METHOD, STRUCTURE WELDED BY ULTRASONIC WELDING METHOD, AND ULTRASONIC WELDING DEVICE
A pair of thermoplastic resin members are placed on an anvil. A pressing force of a tool horn vibrating ultrasonically in a direction not perpendicular to but along upper surfaces of the pair of thermoplastic resin members is applied to the upper surfaces. The application of the pressing force of the tool horn vibrating ultrasonically allows melting of a vicinity of the upper surfaces of the pair of thermoplastic resin members. A welded structure part is formed on an unwelded structure part, thereby welding the pair of thermoplastic resin members as an overlap structure including the welded structure part arranged on the unwelded structure part. The distance and positional relationship between the pair of thermoplastic resin members after the welding are unchanged before and after the welding. The surfaces, placed on the anvil, of the thermoplastic resin members are neither burned nor discolored.
Method of fabricating a miniature device having an acoustic diaphragm
A method of forming a device having a compliant member includes applying heat to a thermoplastic elastomer to maintain the thermoplastic elastomer in a softened state. The thermoplastic elastomer is extruded in the softened state as a film of thermoplastic elastomer. One or more of a bobbin and a housing, each having and end, is positioned such that the end extends at least partially into the film of thermoplastic elastomer. The positioning occurs when the thermoplastic elastomer is in the softened state and/or the bobbin and/or housing is at a temperature that is greater than a temperature of the film of thermoplastic elastomer. The film is cooled so that the bobbin and/or housing are secured to the film and so that the thermoplastic elastomer is in a state that exhibits rubber-like properties.
Device, in particular for closing a head region of a foodstuffs container made of a laminate having an edge region which is skived and partially folded over itself
The invention relates to a device comprising a first fixing element, a further fixing element and a folded planar composite; wherein the first fixing element comprises a first fixing surface and the further fixing element comprises a further fixing surface; wherein the folded planar composite is at least partially fixed between the first fixing surface and the further fixing surface; wherein the folded planar composite comprises a first composite region; wherein the first composite region comprises a first layer sequence comprising a first composite layer comprising a first carrier layer, a second composite layer comprising a second carrier layer, a third composite layer comprising a third carrier layer and a fourth composite layer comprising a fourth carrier layer; wherein in the first composite region the second composite layer is joined to the third composite layer and the third composite layer is joined to the fourth composite layer; wherein in the first composite region the third carrier layer is characterised by a smaller layer thickness than in each case one selected from the group consisting of the first carrier layer, the second carrier layer and the fourth carrier layer or a combination of at least two of these; wherein the first fixing surface or the further fixing surface or both comprises a recess comprising a first recess region; wherein the first composite region is located at least partially between the first recess region and the first fixing surface or the further fixing surface.
Method of production of fabric bags or containers using heat fused seams
A method of producing flexible polypropylene fabric bags with heat fused seams comprising providing fabric pieces, wherein each fabric piece has a coated side and an uncoated side; positioning fabric pieces so that a coated side of one fabric piece faces a coated side of another fabric piece; selecting an area of fabric to be joined for forming a seam or joint; applying heat to the area to be joined that is less than the melting point of the fabrics, for forming one or more seams or joints and wherein the heat fused seams or joints of a resulting polypropylene bag retains at least 85% of the fabric strength without using sewing machines.
Metal-clad laminate sheet manufacturing method, and metal-clad laminate sheet using the same
A method for manufacturing a metal-clad laminate sheet including forming a laminate sheet having the thermoplastic liquid crystal polymer film and the metal foil bonded together; and providing the laminate sheet with a heat treatment which satisfies conditions (1) and (2) below: (1) a heat treatment temperature ranges between 1° C. inclusive and 50° C. exclusive higher than a melting point of the thermoplastic liquid crystal polymer film. (2) a time for the heat treatment ranges from one second to 10 minutes.
LAMINATE AND METHOD FOR PRODUCING SAME
Disclosed are a method for producing a laminate including a step of laminating a resin impregnated fiber reinforced composition layer on a metal member, wherein the method includes a step of forming a resin coating on the metal member and a step of laminating a resin impregnated fiber reinforced composition layer containing a resin impregnated fiber reinforced composition containing (I) 20 to 80% by mass of a polymer having a melting point and/or a glass transition temperature of 50 to 300° C., and (C) 20 to 80% by mass of a reinforcing fiber
(provided that the sum of the component (I) and the component (C) is taken as 100% by mass) via the above resin coating; and a laminate obtained by the method.
Method and apparatus for welding a thermoset object to a further object via thermoplastic outer layers
A method and an apparatus for welding a first object to a second object, wherein the first object is produced from a thermoset and comprises a thermoplastic material outer layer, wherein the second object comprises at least one thermoplastic material outer layer. In addition, a layer of carbon nanotubes is applied to the thermoplastic material outer layer of the first object, and the second object is placed onto the first object. At least some of the thermoplastic material outer layer of the second object lies atop the applied layer of carbon nanotubes. In addition, a potential is applied to the layer of carbon nanotubes, such that an electrical current flows through the carbon nanotubes, wherein the thermoplastic material outer layer of the first object and the thermoplastic material outer layer of the second object are heated and are welded to one another.
POLYAMIDE RESIN COMPOSITION, MOLDED BODY THEREOF, AND METHOD FOR MANUFACTURING LASER-WELDED BODY
This polyamide resin composition contains: 30-89.9 parts by mass of a polyamide resin (A) having a melting point of at least 300 C.; 0-45 parts by mass of a polyamide resin (B) having substantially no melting point; 0.1-5 parts by mass of a light-transmitting pigment (C); and 10-55 parts by mass of a fibrous filler (D) (the total amount of (A), (B), (C), and (D) is 100 parts by mass). The polyamide resin (A) contains at least a terephthalic acid-derived component unit. In a molded body of the polyamide resin composition, the corrected heat of fusion (HR) is 10-70 J/g, and the transmittance of laser light having a wavelength of 940 nm is at least 15% at a thickness of 1.6 mm.