B29C48/43
Methods for manufacturing bulked continuous filament
A method of manufacturing bulked continuous carpet filament which, in various embodiments, comprises: (A) washing a plurality of flakes of recycled PET; (B) providing a PET crystallizer; (C) after the step of washing the plurality of flakes, passing the plurality of flakes of recycled PET through the PET crystallizer; (D) at least partially melting the plurality of flakes into a polymer melt; (E) providing a multi-rotating screw (MRS) extruder having an MRS section; and a vacuum pump in communication with the MRS section; (F) using the vacuum pump to reduce a pressure within the MRS Section; (G) after the step of passing the plurality of flakes through the PET crystallizer, passing the polymer melt through the MRS Section; and (H) after the step of passing the polymer melt through the MRS extruder, forming the polymer melt into bulked continuous carpet filament.
METHODS FOR MANUFACTURING BULKED CONTINUOUS CARPET FILAMENT
A method of manufacturing bulked continuous carpet filament from recycled polymer. In various embodiments, the method includes: (1) reducing recycled polymer material into polymer flakes; (2) cleansing the polymer flakes; (3) melting the flakes into a polymer melt; (4) removing water and contaminants from the polymer melt by dividing the polymer melt into a plurality of polymer streams and exposing those streams to pressures below 5 millibars; (5) recombining the streams; and (6) using the resulting purified polymer to produce bulked continuous carpet filament.
METHODS FOR MANUFACTURING BULKED CONTINUOUS CARPET FILAMENT
A method of manufacturing bulked continuous carpet filament from recycled polymer. In various embodiments, the method includes: (1) reducing recycled polymer material into polymer flakes; (2) cleansing the polymer flakes; (3) melting the flakes into a polymer melt; (4) removing water and contaminants from the polymer melt by dividing the polymer melt into a plurality of polymer streams and exposing those streams to pressures below 5 millibars; (5) recombining the streams; and (6) using the resulting purified polymer to produce bulked continuous carpet filament.
Polyester Fiber Blends and Methods of Manufacturing Same
This application is directed to polymer blends of polyethylene naphthalate, polytrimethylene terephthalate, and polyethylene naphthalate, for use in fibers, such as carpet fibers, and other applications. This application is also directed to methods of producing such polymer blends and fibers.
Oxygen scavenging compositions, articles containing same, and methods of their use
The disclosure relates to oxygen scavenging compositions, methods of making the compositions, articles prepared from the compositions, and methods of making the articles. This abstract is intended as a scanning tool for purposes of searching in the particular art and is not intended to be limiting of the present invention.
SYSTEMS AND METHODS FOR MANUFACTURING BULKED CONTINUOUS FILAMENT
A method for manufacturing pellets from polymer, comprising: (1) melting polymer flakes in a first section of a melt processing unit to create a first single stream of polymer melt; (2) separating the first single stream of polymer melt into multiple streams of polymer melt by means of a separation element; (3) passing the multiple streams through a multiple stream section of said melt processing unit and exposing the multiple streams to a pressure within the multiple stream section of the melt processing unit as the multiple streams pass through the multiple stream section; (4) recombining the multiple streams into at least one combined stream of polymer melt; and (5) cooling the polymer melt and forming said pellets from the at least one combined stream. The intrinsic viscosity of the at least one combined stream may be determined and, in response, the chamber pressure within the multiple stream section adjusted.
SYSTEMS AND METHODS FOR MANUFACTURING BULKED CONTINUOUS FILAMENT
A method for manufacturing pellets from polymer, comprising: (1) melting polymer flakes in a first section of a melt processing unit to create a first single stream of polymer melt; (2) separating the first single stream of polymer melt into multiple streams of polymer melt by means of a separation element; (3) passing the multiple streams through a multiple stream section of said melt processing unit and exposing the multiple streams to a pressure within the multiple stream section of the melt processing unit as the multiple streams pass through the multiple stream section; (4) recombining the multiple streams into at least one combined stream of polymer melt; and (5) cooling the polymer melt and forming said pellets from the at least one combined stream. The intrinsic viscosity of the at least one combined stream may be determined and, in response, the chamber pressure within the multiple stream section adjusted.
Polyester fiber blends and methods of manufacturing same
This application is directed to polymer blends of polyethylene naphthalate, polytrimethylene terephthalate, and polyethylene naphthalate, for use in fibers, such as carpet fibers, and other applications. This application is also directed to methods of producing such polymer blends and fibers.
Polyester fiber blends and methods of manufacturing same
This application is directed to polymer blends of polyethylene naphthalate, polytrimethylene terephthalate, and polyethylene naphthalate, for use in fibers, such as carpet fibers, and other applications. This application is also directed to methods of producing such polymer blends and fibers.
Methods for manufacturing bulked continuous carpet filament
A method of manufacturing bulked continuous carpet filament from recycled polymer. In various embodiments, the method includes: (1) reducing recycled polymer material into polymer flakes; (2) cleansing the polymer flakes; (3) melting the flakes into a polymer melt; (4) removing water and contaminants from the polymer melt by dividing the polymer melt into a plurality of polymer streams and exposing those streams to pressures below 25 millibars or another predetermined pressure; (5) recombining the streams; and (6) using the resulting purified polymer to produce bulked continuous carpet filament.