C01D3/04
SODIUM ANTI-PEROVSKITE SOLID ELECTROLYTE COMPOSITIONS
Na-rich electrolyte compositions provided herein can be used in a variety of devices, such as sodium ionic batteries, capacitors and other electrochemical devices. Na-rich electrolyte compositions provided herein can have a chemical formula of Na.sub.3OX, Na.sub.3SX, Na .sub.(3-δ) M.sub.δ/2OX and Na .sub.(3-δ) M.sub.δ/2SX wherein 0<δ<0.8, wherein X is a monovalent anion selected from fluoride, chloride, bromide, iodide, H.sup.−, CN.sup.−, BF.sub.4.sup.−, BH.sub.4.sup.−, ClO.sub.4.sup.−, CH.sub.3.sup.−, NO.sub.2.sup.−, NH.sub.2.sup.− and mixtures thereof, and wherein M is a divalent metal selected from the group consisting of magnesium, calcium, barium, strontium and mixtures thereof. Na-rich electrolyte compositions provided herein can have a chemical formula of Na .sub.(3-δ) M.sub.δ/3OX and/or Na .sub.(3-δ) M.sub.δ/3SX; wherein 0<δ<0.5, wherein M is a trivalent cation M.sup.3, and wherein X is selected from fluoride, chloride, bromide, iodide, H.sup.−, CN.sup.−, BF.sub.4.sup.−, BH.sub.4.sup.−, ClO.sub.4.sup.−, CH.sub.3.sup.−, NO.sub.2.sup.−, NH.sup.2− and mixtures thereof. Synthesis and processing methods of NaRAP compositions for battery, capacitor, and other electrochemical applications are also provided.
Non-caking salt composition, preparation process and use thereof
The present invention relates to a sodium chloride composition comprising an iron complex of tartaric acid wherein between 55 and 90% by weight of the tartaric acid is meso-tartaric acid. The present invention furthermore relates to a process to prepare such a sodium chloride composition and to the use of such a sodium chloride composition.
Non-caking salt composition, preparation process and use thereof
The present invention relates to a sodium chloride composition comprising an iron complex of tartaric acid wherein between 55 and 90% by weight of the tartaric acid is meso-tartaric acid. The present invention furthermore relates to a process to prepare such a sodium chloride composition and to the use of such a sodium chloride composition.
PRODUCTION OF LITHIUM HYDROXIDE
A process (10) for the production of lithium hydroxide, the process comprising the steps of: (i) Causticising lithium chloride (12) with sodium hydroxide (16) to produce a lithium hydroxide product; (ii) Collecting the solids resulting from the causticisation of step (i) and filtering (22) same; (iii) The filtered solids from step (ii) are passed to a heating step (32) in which anhydrous lithium hydroxide is produced; (iv) Filtering (34) the anhydrous lithium hydroxide product of step (iii); and (v) Quenching the anhydrous lithium hydroxide of step (iv) with water to produce lithium hydroxide monohydrate crystals.
METHOD FOR THE PRODUCTION OF SULPHATE OF POTASH GRANULATES, SULPHATE OF POTASH GRANULATE OBTAINED THEREBY, AND USE THEREOF
The invention relates to a method for producing sulphate of potash granulates, wherein 0.1 to 7.5 wt % of a sodium salt selected from among sodium chloride, sodium sulphate, sodium sulphate hydrates, sodium hydroxide and mixtures thereof are added to the sulphate of potash during the granulation process, the percentage by weight being in relation to the sulphate of potash used. In addition, 0.1 to 2.5 wt % of water are added prior to or during the granulation process. The invention also relates to the granulates obtained by said method as well as the use of sodium salts and glaserite and mixtures thereof for improving the mechanical properties of sulfate of potash granulates. The sulphate of potash granulates produced by the method of the invention have significantly greater bursting strength and significantly greater abrasion resistance than granulates known from the prior art.
METHOD FOR THE PRODUCTION OF SULPHATE OF POTASH GRANULATES, SULPHATE OF POTASH GRANULATE OBTAINED THEREBY, AND USE THEREOF
The invention relates to a method for producing sulphate of potash granulates, wherein 0.1 to 7.5 wt % of a sodium salt selected from among sodium chloride, sodium sulphate, sodium sulphate hydrates, sodium hydroxide and mixtures thereof are added to the sulphate of potash during the granulation process, the percentage by weight being in relation to the sulphate of potash used. In addition, 0.1 to 2.5 wt % of water are added prior to or during the granulation process. The invention also relates to the granulates obtained by said method as well as the use of sodium salts and glaserite and mixtures thereof for improving the mechanical properties of sulfate of potash granulates. The sulphate of potash granulates produced by the method of the invention have significantly greater bursting strength and significantly greater abrasion resistance than granulates known from the prior art.
HIMALAYAN SALT CRYSTAL PURIFICATION PROCESS
The disclosure provides a process for obtaining the purest form of Himalayan pink salt. The purest form of Himalayan pink salt is preferably in crystal in form and is substantially clear and colorless. The disclosure provides a purification process that identifies and removes solid impurities affording the purest form of Himalayan pink salt. The system may machine vision algorithms that process feedback from one or more sensors to detect and identify color or clarity, and may use one or more host controllers to remove solid impurities. The controller may identify the color or clarity and ensure consistent removal of the solid impurities.
HIMALAYAN SALT CRYSTAL PURIFICATION PROCESS
The disclosure provides a process for obtaining the purest form of Himalayan pink salt. The purest form of Himalayan pink salt is preferably in crystal in form and is substantially clear and colorless. The disclosure provides a purification process that identifies and removes solid impurities affording the purest form of Himalayan pink salt. The system may machine vision algorithms that process feedback from one or more sensors to detect and identify color or clarity, and may use one or more host controllers to remove solid impurities. The controller may identify the color or clarity and ensure consistent removal of the solid impurities.
AGENTS AND METHODS FOR THE TEMPORARY SHAPING OF KERATIN-CONTAINING FIBERS
The invention relates to a cosmetic product, comprising a) a cosmetic preparation, including, in relation to its total weight, a1) 65 to 96 wt % of at least one polar solvent; a2) 0.1 to 34 wt % of at least one inorganic salt; b) a device for flash evaporation of the cosmetic preparation a), and to a method using corresponding products and to the use of the cosmetic preparation a) as process material in a device for flash evaporation.
Method for producing hexagonal plate-shaped zinc oxide
The present invention provides a method capable of producing hexagonal plate-shaped zinc oxide having a small thickness and a small variation in the particle size. The present invention relates to a method for producing hexagonal plate-shaped zinc oxide, the method including: a step (1) of preparing a slurry mixture containing starting particulate zinc oxide, a zinc acetate solution, and a chloride; and a step (2) of heat aging the slurry mixture obtained in the step (1) at 60° C. to 100° C.