C01G45/006
MANGANESE OXIDES AND CATHODE ACTIVE MATERIALS
Aspects of the present disclosure generally relate to battery technology, and more specifically relate to manganese oxides and cathode active materials. In an aspect, a cathode active material is provided. The cathode active material includes a composition comprising a manganese oxide represented by Formula (I): Li.sub.aNa.sub.b(M.sup.1).sub.cMn.sub.dO.sub.e, a manganese oxide represented by Formula (II): Na.sub.w(M.sup.2).sub.xMn.sub.yO.sub.z (II), or combinations thereof, wherein: each of M.sup.1 and M.sup.2 is, individually, Ni, Cu, Zn, Mg, Fe, Co, Li, Al, Cr, LiAl, LiCr, LiCo, or combinations thereof, a, b, c, d, and e represent molar ratios of respective elements in Formula (I); and w, x, y, and z represent molar ratios of respective elements in Formula (II). Batteries and articles comprising a manganese oxide described herein are provided. Processes for forming manganese oxides are also provided.
Precursor For Preparation Of Lithium Composite Transition Metal Oxide, Method For Preparing The Same And Lithium Composite Transition Metal Oxide Obtained From The Same
Disclosed are a precursor for preparation of a lithium composite transition metal oxide, a method for preparing the same and a lithium composite transition metal oxide obtained from the same. More particularly, the transition metal precursor which has a composition represented by Formula 1 below and is prepared in an aqueous transition metal solution, mixed with a transition metal-containing salt, including an alkaline material, the method for preparing the same and the lithium composite transition metal oxide obtained from the same are disclosed.
Mn.sub.aM.sub.b(OH.sub.1-x).sub.2-yA.sub.y (1) wherein M is at least one selected form the group consisting of Ni, Ti, Co, Al, Cu, Fe, Mg, B, Cr, Zr, Zn and Period II transition metals; A is at least one selected form the group consisting of anions of PO.sub.4, BO.sub.3, CO.sub.3, F and NO.sub.3, and 0.5a1.0; 0b0.5; a+b=1; 0<x<1.0; and 0y0.02.
MANUFACTURING METHOD OF COMPOSITE OXIDE AND MANUFACTURING METHOD OF POWER STORAGE DEVICE
An object is to reduce variation in shape of crystals that are to be formed. Solutions containing respective raw materials are made in an environment where an oxygen concentration is lower than that in air, the solutions containing the respective raw materials are mixed in an environment where an oxygen concentration is lower than that in air to form a mixture solution, and with use of the mixture solution, a composite oxide is formed by a hydrothermal method.
Precursor for preparation of lithium composite transition metal oxide, method for preparing the same and lithium composite transition metal oxide obtained from the same
Disclosed are a precursor for preparation of a lithium composite transition metal oxide, a method for preparing the same and a lithium composite transition metal oxide obtained from the same. More particularly, the transition metal precursor which has a composition represented by Formula 1 below and is prepared in an aqueous transition metal solution, mixed with a transition metal-containing salt, including an alkaline material, the method for preparing the same and the lithium composite transition metal oxide obtained from the same are disclosed.
Mn.sub.aM.sub.b(OH.sub.1-x).sub.2-yA.sub.y(1) wherein M is at least one selected form the group consisting of Ni, Ti, Co, Al, Cu, Fe, Mg, B, Cr, Zr, Zn and Period II transition metals; A is at least one selected form the group consisting of anions of PO.sub.4, BO.sub.3, CO.sub.3, F and NO.sub.3, and 0.5a1.0; 0b0.5; a+b=1; 0<x<1.0; and 0y0.02.
POSITIVE-ELECTRODE ACTIVE MATERIAL AND BATTERY INCLUDING POSITIVE-ELECTRODE ACTIVE MATERIAL
A positive-electrode active material contains a compound represented by the following composition formula (1):
Li.sub.xMe.sub.yA.sub.zO.sub.F.sub.(1) where Me denotes one or more elements selected from the group consisting of Mn, Co, Ni, Fe, Al, Cu, Nb, Mo, Ti, Cr, Zr, Zn, Na, K, Ca, Mg, Pt, Au, Ru, and W, A denotes one or more elements selected from the group consisting of B, Si, and P, and the following conditions: 1.3x2.1, 0.8y1.3, 0<z0.2, 1.82.9, and 0.11.2 are satisfied. A crystal structure of the compound belongs to a space group Fm-3m.
POSITIVE ELECTRODE ACTIVE MATERIAL AND BATTERY USING POSITIVE ELECTRODE ACTIVE MATERIAL
A positive-electrode active material contains a compound represented by the following composition formula (1):
Li.sub.xMe.sub.yO.sub.X.sub.(1) where Me denotes one or more elements selected from the group consisting of Mn, Ni, Co, Fe, Al, Sn, Cu, Nb, Mo, Bi, Ti, V, Cr, Y, Zr, Zn, Na, K, Ca, Mg, Pt, Au, Ag, Ru, Ta, W, La, Ce, Pr, Sm, Eu, Dy, and Er, X denotes two or more elements selected from the group consisting of F, Cl, Br, I, N, and S, and x, y, , and satisfy 0.75x2.25, 0.75y1.50, 1<3, and 0<2, respectively. A crystal structure of the compound belongs to a space group Fm-3m.
Hexafluoromanganate (IV), complex fluoride phosphor, and methods respectively for producing said products
The present invention relates to a method for producing a hexafluoromanganate(IV), said method being characterized by comprising: inserting an anode and a cathode into a reaction solution that contains a compound containing manganese having an atomic valence of less than 4 and/or manganese having an atomic valence of more than 4 and hydrogen fluoride; and then applying an electric current having an electric current density of 100 to 1000 A/m.sup.2 between the anode and the cathode. According to the present invention, it becomes possible to produce a hexafluoromanganate(IV) in which the content ratio of manganese having an atomic valence of 4 is high and the contamination with oxygen is reduced and which has high purity. When a complex fluoride red phosphor is produced using the hexafluoromanganate(IV) as a raw material, the phosphor produced has high luminescence properties, particularly high internal quantum efficiency.
Cathode active materials having improved particle morphologies
Mixed-metal oxides and lithiated mixed-metal oxides are disclosed that involve compounds according to, respectively, Ni.sub.xMn.sub.yCo.sub.zMe.sub.O.sub. and Li.sub.1+Ni.sub.xMn.sub.yCo.sub.zMe.sub.O.sub.. In these compounds, Me is selected from B, Na, Mg, Al, Si, K, Ca, Sc, Ti, V, Cr, Fe, Cu, Zn, Ga, Ge, Zr, Nb, Mo, Ru, Ag, In, and combinations thereof; 0x1; 0y1; 0z<1; x+y+z>0; 00.5; and x+y+>0. For the mixed-metal oxides, 15. For the lithiated mixed-metal oxides, 0.11.0 and 1.93. The mixed-metal oxides and the lithiated mixed-metal oxides include particles having an average density greater than or equal to 90% of an ideal crystalline density.
Lithium-ion battery
A lithium-ion battery includes: a cathode; an anode; and a non-aqueous electrolyte solution, in which the cathode includes a current collector and a cathode mixture applied on at least one side of the current collector, the cathode mixture includes a lithium transition metal oxide as a cathode active material, the anode includes a lithium titanium complex oxide as an anode active material, and the non-aqueous electrolyte solution includes a fluorine-containing boric acid ester.
Manufacturing method of composite oxide and manufacturing method of power storage device
An object is to reduce variation in shape of crystals that are to be formed. Solutions containing respective raw materials are made in an environment where an oxygen concentration is lower than that in air, the solutions containing the respective raw materials are mixed in an environment where an oxygen concentration is lower than that in air to form a mixture solution, and with use of the mixture solution, a composite oxide is formed by a hydrothermal method.