Patent classifications
C01G51/10
PROCESSES FOR RECYCLING SPENT CATALYSTS, RECYCLING RECHARGEABLE BATTERIES, AND INTEGRATED PROCESSES THEREOF
Integrated recycling method and processes including recycling spent catalyst to produce one or more water-soluble metal salts and one or more water-insoluble tail byproducts, and recycling rechargeable batteries to produce one or more battery-grade metals and one or more pure metallic byproducts, wherein the water insoluble tail byproduct is a feedstock in recycling the rechargeable batteries, the impure metallic byproduct is a feedstock in recycling the spent catalyst, or both.
BINDER FOR AN AGGLOMERATION PROCESS
A binder for use in leaching a heap of a low-permeability ore containing at least one of the following: copper ore, copper/cobalt ore, nickel laterite ore and uranium ore, wherein the binder comprises an acid-proof cement formed by modifying ordinary Portland cement (OPC) with a supplementary cementitious material (SCM).
BINDER FOR AN AGGLOMERATION PROCESS
A binder for use in leaching a heap of a low-permeability ore containing at least one of the following: copper ore, copper/cobalt ore, nickel laterite ore and uranium ore, wherein the binder comprises an acid-proof cement formed by modifying ordinary Portland cement (OPC) with a supplementary cementitious material (SCM).
METHOD FOR PREPARING COBALT SULFATE SALT
In a method for preparing a cobalt sulfate salt, a feeding solution comprising cobalt sulfate and a sulfuric acid aqueous solution is prepared. A first solution is produced by evaporation-crystallizing the feeding solution. A first cobalt sulfate salt is produced by filtering the first solution together with first purging. A second solution is produced by cooling-crystallizing an aqueous solution comprising the first cobalt sulfate salt. A second cobalt sulfate salt is produced by filtering the second solution together with second purging.
METHOD FOR PREPARING COBALT SULFATE SALT
In a method for preparing a cobalt sulfate salt, a feeding solution comprising cobalt sulfate and a sulfuric acid aqueous solution is prepared. A first solution is produced by evaporation-crystallizing the feeding solution. A first cobalt sulfate salt is produced by filtering the first solution together with first purging. A second solution is produced by cooling-crystallizing an aqueous solution comprising the first cobalt sulfate salt. A second cobalt sulfate salt is produced by filtering the second solution together with second purging.
Method for preparing nickel/manganese/lithium/cobalt sulfate and tricobalt tetraoxide from battery wastes
A method for preparing nickel/manganese/lithium/cobalt sulfate and tricobalt tetraoxide from battery wastes adopts the following process: dissolving battery wastes with acid, removing iron and aluminum, removing calcium, magnesium and copper, carrying extraction separation, and carrying out evaporative crystallization to prepare nickel sulfate, manganese sulfate, lithium sulfate, cobalt sulfate or/and tricobalt tetraoxide. By using the method, multiple metal elements, such as nickel, manganese, lithium and cobalt, can be simultaneously recovered from the battery wastes, the recovered products are high in purity and can reach battery grade, battery-grade tricobalt tetraoxide can also be directly produced. The method is simple in process, low in energy consumption and free in exhaust gas pollution, and can realize zero release of wastewater.
Method for preparing nickel/manganese/lithium/cobalt sulfate and tricobalt tetraoxide from battery wastes
A method for preparing nickel/manganese/lithium/cobalt sulfate and tricobalt tetraoxide from battery wastes adopts the following process: dissolving battery wastes with acid, removing iron and aluminum, removing calcium, magnesium and copper, carrying extraction separation, and carrying out evaporative crystallization to prepare nickel sulfate, manganese sulfate, lithium sulfate, cobalt sulfate or/and tricobalt tetraoxide. By using the method, multiple metal elements, such as nickel, manganese, lithium and cobalt, can be simultaneously recovered from the battery wastes, the recovered products are high in purity and can reach battery grade, battery-grade tricobalt tetraoxide can also be directly produced. The method is simple in process, low in energy consumption and free in exhaust gas pollution, and can realize zero release of wastewater.
METHOD FOR SEPARATING COPPER FROM NICKEL AND COBALT
Provided is a method for separating copper from nickel and cobalt with which it is possible to selectively and efficiently separate copper, as well as nickel and cobalt, from an alloy including copper, nickel, and cobalt such as an alloy having high corrosion resistance that includes copper, nickel, and cobalt obtained by dry treatment of waste lithium ion cells. An alloy including copper, nickel, and cobalt is brought into contact with sulfuric acid in the joint presence of a sulfurizing agent, and a solid containing copper and a leachate containing nickel and cobalt are obtained.
Method for producing solutions containing nickel or cobalt
Provided is a method for producing solutions, by which two solutions, namely a high-purity nickel sulfate solution and a mixed solution of nickel sulfate and cobalt sulfate are able to be obtained at the same time from a sulfuric acid solution containing nickel, cobalt and calcium. A method for producing solutions according to the present invention uses a sulfuric acid solution containing nickel, cobalt and calcium and performs a first step S1 for producing a mixed solution of nickel sulfate and cobalt sulfate from the sulfuric acid solution and a second step S2 for producing a solution of nickel sulfate from the sulfuric acid solution in parallel. In the first step, the sulfuric acid solution is subjected to solvent extraction by an extractant, thereby obtaining a first organic solvent after extraction. In the second step, the sulfuric acid solution is subjected to solvent extraction by means of an extractant.
Method for producing solutions containing nickel or cobalt
Provided is a method for producing solutions, by which two solutions, namely a high-purity nickel sulfate solution and a mixed solution of nickel sulfate and cobalt sulfate are able to be obtained at the same time from a sulfuric acid solution containing nickel, cobalt and calcium. A method for producing solutions according to the present invention uses a sulfuric acid solution containing nickel, cobalt and calcium and performs a first step S1 for producing a mixed solution of nickel sulfate and cobalt sulfate from the sulfuric acid solution and a second step S2 for producing a solution of nickel sulfate from the sulfuric acid solution in parallel. In the first step, the sulfuric acid solution is subjected to solvent extraction by an extractant, thereby obtaining a first organic solvent after extraction. In the second step, the sulfuric acid solution is subjected to solvent extraction by means of an extractant.