C03B27/004

ENAMEL COMPOSITION, MANUFACTURING METHOD THEREFOR, AND COOKING UTENSILS
20210246067 · 2021-08-12 ·

The present invention relates to an enamel composition capable of removing sugars as well as poultry oils as contaminants at a low temperature by using a catalyst oxide, to a manufacturing method therefor, and cooking utensils. The present invention provides an enamel composition, a manufacturing method therefor, and cooking utensils, wherein the enamel composition is capable of removing sugars as well as poultry oils as contaminants at a low temperature by comprising: at least one of SiO.sub.2, B.sub.2O.sub.3, Li.sub.2O, Na.sub.2O, and K.sub.2O; and TiO.sub.2.

ENAMEL COMPOSITION, MANUFACTURING METHOD THEREFOR, AND COOKING UTENSILS
20210246067 · 2021-08-12 ·

The present invention relates to an enamel composition capable of removing sugars as well as poultry oils as contaminants at a low temperature by using a catalyst oxide, to a manufacturing method therefor, and cooking utensils. The present invention provides an enamel composition, a manufacturing method therefor, and cooking utensils, wherein the enamel composition is capable of removing sugars as well as poultry oils as contaminants at a low temperature by comprising: at least one of SiO.sub.2, B.sub.2O.sub.3, Li.sub.2O, Na.sub.2O, and K.sub.2O; and TiO.sub.2.

MANUFACTURE OF LAMINATED GLAZING
20210017807 · 2021-01-21 ·

A process for manufacturing a bent laminated glazing, includes manufacturing a first bent laminated glazing including at least two glass substrates locally comprising, in each of the at least two glass substrates and facing each other in all the at least two glass substrates, a zone including compressive stresses, and cutting the first bent laminated glazing through its entire thickness along a line included in the zone in order to form local cut edges and, after cutting, a second bent laminated glazing with the local cut edges having compressive edge stresses.

MANUFACTURE OF LAMINATED GLAZING
20210017807 · 2021-01-21 ·

A process for manufacturing a bent laminated glazing, includes manufacturing a first bent laminated glazing including at least two glass substrates locally comprising, in each of the at least two glass substrates and facing each other in all the at least two glass substrates, a zone including compressive stresses, and cutting the first bent laminated glazing through its entire thickness along a line included in the zone in order to form local cut edges and, after cutting, a second bent laminated glazing with the local cut edges having compressive edge stresses.

Manufacture of laminated glazing

A laminated includes two bent glass substrates, a polymer interlayer between the glass substrates, and a notch or orifice cut in an entire thickness of the glazing. The glazing includes a border of compressive edge stresses obtained by general controlled cooling of the substrates in a paired state so that compressive stresses are generated at the border, and a local compression zone, different from the border, and obtained by local controlled cooling of a local area of a main surface of the glazing so that compressive stresses are generated in theid local compression zone. The notch or orifice is located in the local compression zone and made in the substrates in a paired state after forming the local compression zone so that cut contours of the substrates in the notch or orifice have a perfect superposition. The compressive edge stresses of the cut contours are greater than 4 MPa.

Manufacture of laminated glazing

A laminated includes two bent glass substrates, a polymer interlayer between the glass substrates, and a notch or orifice cut in an entire thickness of the glazing. The glazing includes a border of compressive edge stresses obtained by general controlled cooling of the substrates in a paired state so that compressive stresses are generated at the border, and a local compression zone, different from the border, and obtained by local controlled cooling of a local area of a main surface of the glazing so that compressive stresses are generated in theid local compression zone. The notch or orifice is located in the local compression zone and made in the substrates in a paired state after forming the local compression zone so that cut contours of the substrates in the notch or orifice have a perfect superposition. The compressive edge stresses of the cut contours are greater than 4 MPa.

MANUFACTURE OF LAMINATED GLAZING
20170314321 · 2017-11-02 ·

A laminated includes two bent glass substrates, a polymer interlayer between the glass substrates, and a notch or orifice cut in an entire thickness of the glazing. The glazing includes a border of compressive edge stresses obtained by general controlled cooling of the substrates in a paired state so that compressive stresses are generated at the border, and a local compression zone, different from the border, and obtained by local controlled cooling of a local area of a main surface of the glazing so that compressive stresses are generated in theid local compression zone. The notch or orifice is located in the local compression zone and made in the substrates in a paired state after forming the local compression zone so that cut contours of the substrates in the notch or orifice have a perfect superposition. The compressive edge stresses of the cut contours are greater than 4 MPa.

MANUFACTURE OF LAMINATED GLAZING
20170314321 · 2017-11-02 ·

A laminated includes two bent glass substrates, a polymer interlayer between the glass substrates, and a notch or orifice cut in an entire thickness of the glazing. The glazing includes a border of compressive edge stresses obtained by general controlled cooling of the substrates in a paired state so that compressive stresses are generated at the border, and a local compression zone, different from the border, and obtained by local controlled cooling of a local area of a main surface of the glazing so that compressive stresses are generated in theid local compression zone. The notch or orifice is located in the local compression zone and made in the substrates in a paired state after forming the local compression zone so that cut contours of the substrates in the notch or orifice have a perfect superposition. The compressive edge stresses of the cut contours are greater than 4 MPa.

Manufacture of laminated glazing

A method for manufacturing a laminated glass panel, which includes at least two glass substrates and at least one intermediate layer made of a polymeric material arranged between the substrates, the method including in the following order: the bending of the substrates; the controlled cooling of the substrates; and the formation of a laminated assembly that includes the substrates and the intermediate layer; the cutting of the laminated assembly straight through the entire thickness thereof along a line on one of the main surfaces thereof, the controlled cooling including general controlled cooling and local controlled cooling of an area that includes the cutting line, the local controlled cooling being faster than the general controlled cooling.

Manufacture of laminated glazing

A method for manufacturing a laminated glass panel, which includes at least two glass substrates and at least one intermediate layer made of a polymeric material arranged between the substrates, the method including in the following order: the bending of the substrates; the controlled cooling of the substrates; and the formation of a laminated assembly that includes the substrates and the intermediate layer; the cutting of the laminated assembly straight through the entire thickness thereof along a line on one of the main surfaces thereof, the controlled cooling including general controlled cooling and local controlled cooling of an area that includes the cutting line, the local controlled cooling being faster than the general controlled cooling.