GLASS PRODUCTION METHOD AND INDUSTRIAL GLASS-MAKING FACILITY
The invention relates to a glass production method comprising charging a glass furnace with solid-state raw materials, said raw materials comprising granular glassy sodium silicate and having a moisture content of less than 1%, preferably 0%, by weight, and powdered calcium oxide.
Preparation of carbon-doped silicon dioxide granulate as an intermediate in the preparation of quartz glass
One aspect relates to a process for the preparation of a quartz glass body. The process includes providing a silicon dioxide granulate I prepared from a pyrogenically produced silicon dioxide powder, treating the silicon dioxide granulate I with a reactant at a temperature in a range from 1000 to 1300° C., and making a glass melt out of the silicon dioxide granulate. A quartz glass body is made out of at least a part of the glass melt. Furthermore, one aspect relates to a quartz glass body obtainable by this process. Furthermore, one aspect relates to a light guide, an illuminant, and a formed body, each of which is obtainable by further processing of the quartz glass body. One aspect additionally relates to a process for the preparation of a silicon dioxide granulate II.
Glass Redox Control in Submerged Combustion Melting
A method of producing glass using submerged combustion melting includes supplying a combustible gas mixture to one or more submerged burners of a submerged combustion melter, combusting the combustible gas mixture supplied to the submerged burner(s) to produce combustion products, and discharging the combustion products from the submerged burner(s) directly into a glass melt contained within the submerged combustion melter to agitate and heat the glass melt. The glass melt is comprised of soda-lime-silica glass and has a redox ratio. Additionally, the disclosed method involves controlling one or more operating conditions of the submerged combustion melter selected from (1) an oxygen-to-fuel ratio of the combustible gas mixture supplied to each of the submerged burners, (2) a residence time of the glass melt, and (3) a gas flux through the glass melt.
Glass Redox Control in Submerged Combustion Melting
A method of producing glass using submerged combustion melting includes supplying a combustible gas mixture to one or more submerged burners of a submerged combustion melter, combusting the combustible gas mixture supplied to the submerged burner(s) to produce combustion products, and discharging the combustion products from the submerged burner(s) directly into a glass melt contained within the submerged combustion melter to agitate and heat the glass melt. The glass melt is comprised of soda-lime-silica glass and has a redox ratio. Additionally, the disclosed method involves controlling one or more operating conditions of the submerged combustion melter selected from (1) an oxygen-to-fuel ratio of the combustible gas mixture supplied to each of the submerged burners, (2) a residence time of the glass melt, and (3) a gas flux through the glass melt.
Production of glass from a mixture comprising calcium oxide, and glass furnace
The invention relates to a glass production method comprising the production of a glass precursor mixture for a glass furnace, in which water, sand and sodium carbonate are mixed in weight proportions of between 0 and 5%, 40 and 65%, and greater than 0 and at most 25% respectively, and, after at least 10 minutes, calcium oxide is added in a weight proportion of between 1 and 20% of the total. The invention relates to a method for producing glass using a mixture containing, in particular, calcium oxide, and a glass melting furnace, said method and furnace using a burner with a flame directed at the glass batch.
FLUORITE SYNTHETIC STONES AND METHOD OF MAKING FLUORITE SYNTHETIC STONES
A fluorite synthetic stone comprises: (a) a glass matrix comprising Ca, Si and O, and having a predetermined weight ratio of Ca to Si; and (b) CaF.sub.2 crystals dispersed in the glass matrix at a concentration of at least about 70 wt.%. A method of making fluorite synthetic stones includes formulating a particulate mixture comprising: CaF.sub.2 crystals at a concentration of at least about 70 wt.%; and an excipient having a predetermined weight ratio of Ca to Si. Aggregates are prepared from the particulate mixture. The aggregates are heat treated to form a plurality of fluorite synthetic stones, where each synthetic stone comprises: a glass matrix comprising Ca, Si and O; and CaF.sub.2 crystals dispersed in the glass matrix at a concentration of at least about 70 wt.%.
Recycling of smart windows
The present invention relates to the methods of recycling electrochromic devices and also designing such devices while keeping recyclability in perspective. Recyclability includes recovering of certain materials for re-use within the same application or other applications. Using recycling reduces or eliminates waste stream quantities to be disposed of and/or reduces toxicity of these waste streams.
OPTICAL GLASS, PREPARATION METHOD THEREOF, BACKLIGHT MODULE AND DISPLAY MODULE
Optical glass, a preparation method thereof, a backlight module and a display module. The optical glass comprises a glass substrate and optical masterbatches, which are dispersed in the glass substrate, each optical masterbatch comprises a quantum dot fluorescent agent inner core and an encapsulation shell which encloses the quantum dot fluorescent agent inner core. A quantum dot fluorescent agent is protected by the encapsulation shell and the luminous efficiency is high; when the optical glass is applied to a display module, the color gamut may be improved; moreover, the glass is capable of preventing against the invasion of water vapor, even the quantum dot fluorescent agent at an edge of the glass rarely fails, and an edge failure size is basically avoided; meanwhile, the expansion coefficient is small, and an expansion space reserved during assembly is extremely small.
Doped bismuth silicate crystals via devitrification of glass forming liquids
This technology is directed to the preparation of doped-bismuth-silicate seed crystals through controlled crystallization (e.g. dimensionality of growth and nucleation mechanism) and the method of forming high purity single seed (particle size ranges from micrometers to millimeters) for various uses. These seed crystals have a nominal stoichiometry of Bi.sub.2-xA.sub.xSiO.sub.5, Bi.sub.2-xA.sub.xSi.sub.3O.sub.9, Bi.sub.4-xA.sub.xSi.sub.3O.sub.9, and Bi.sub.12-xA.sub.xSiO.sub.20, where A is a rare earth dopant selected from La, Ce, Nd, Pr, and/or Sm.
METHOD FOR PRODUCING MIXED RAW MATERIAL, METHOD FOR PRODUCING MOLTEN GLASS, METHOD FOR PRODUCING GLASS ARTICLE, APPARATUS FOR PRODUCING MOLTEN GLASS, AND APPARATUS FOR PRODUCING GLASS ARTICLE
A mixed raw material producing method for producing a mixed raw material includes preparing a glass raw material and an aqueous solution of sodium hydroxide; causing the aqueous solution to absorb carbon dioxide gas, to deposit sodium hydrogen carbonate in the aqueous solution; and mixing the sodium hydrogen carbonate with the glass raw material, to obtain a mixed raw material to be charged into a melting furnace.