C03C4/14

Glass powder and silver paste comprising same

A glass powder is a glass powder comprising vanadium-tellurium-silver, which has a softening temperature of 230-330° C. and a median particle size of 1-2 μm; when the glass powder is applied to the silver paste, the requirement that the silver paste is sintered at the temperature of 230-400° C. can be met, and a firm three-dimensional network structure can be formed in the glass system after the silver paste is sintered, and the welding tension of a front silver electrode can be improved; the addition of other metal elements to the glass powder can enable the network structure of the glass powder to be more compact and complete and ensure the stability of the glass powder; the prepared silver paste can be sintered at a temperature of 230-400° C.

SOLID-STATE LITHIUM ION CONDUCTOR

The disclosure relates to a method for producing a solid-state lithium ion conductor material in which the use of water and/or steam is a medium when the obtained intermediate product is cooled or quenched and, if needed, comminution of the intermediate product and/or carrying out of a cooling process with the production of a powder in one comminution step or in a plurality of comminution steps leads or lead to especially advantageous production products. The subject of the disclosure is also the solid-state lithium ion conductor material that has an ion conductivity of at least 10.sup.−5 S/cm at room temperature as well as a water content of <1.0 wt %. The disclosure further relates to the use of the solid-state lithium ion conductor material in the form of a powder in batteries or rechargeable batteries, preferably lithium batteries or rechargeable lithium batteries, in particular, separators, cathodes, anodes, or solid-state electrolytes.

Conductive composition, method for producing conductor, and method for forming wire of electronic component

A conductive composition has excellent adhesiveness to a substrate and conductivity. For example, a conductive composition contains copper powder, cuprous oxide, a lead-free glass frit, and a carboxylic acid-based additive. The cuprous oxide is contained in an amount of at least 5.5 parts by mass and up to 25 parts by mass relative to 100 parts by mass of the copper powder. The lead-free glass frit contains a borosilicate zinc-based glass frit and a vanadium zinc-based glass frit. The borosilicate zinc-based glass frit contains boron oxide, silicon oxide, zinc oxide, and optional other components, among which boron oxide, silicon oxide, and zinc oxide serve as top-three oxide components in terms of content. The vanadium zinc-based glass frit contains vanadium oxide, zinc oxide, and optional other components, among which vanadium oxide and zinc oxide serve as top-two oxide components in terms of content.

Conductive composition, method for producing conductor, and method for forming wire of electronic component

A conductive composition has excellent adhesiveness to a substrate and conductivity. For example, a conductive composition contains copper powder, cuprous oxide, a lead-free glass frit, and a carboxylic acid-based additive. The cuprous oxide is contained in an amount of at least 5.5 parts by mass and up to 25 parts by mass relative to 100 parts by mass of the copper powder. The lead-free glass frit contains a borosilicate zinc-based glass frit and a vanadium zinc-based glass frit. The borosilicate zinc-based glass frit contains boron oxide, silicon oxide, zinc oxide, and optional other components, among which boron oxide, silicon oxide, and zinc oxide serve as top-three oxide components in terms of content. The vanadium zinc-based glass frit contains vanadium oxide, zinc oxide, and optional other components, among which vanadium oxide and zinc oxide serve as top-two oxide components in terms of content.

ELECTRICALLY CONDUCTIVE, POROUS SINTERING BODY
20230284342 · 2023-09-07 · ·

An evaporator is provided that includes a porous sintered body. The porous sintered body is formed by a composite of at least one electrically conductive material and at least one dielectric material. The sintered body has an open porosity in a range from 10 to 90% and an electrical conductivity in a range from 0.1 to 105 S/m. The fraction of electrically conductive material in the sintered body is a maximum of 90 wt. %.

ELECTRICALLY CONDUCTIVE, POROUS SINTERING BODY
20230284342 · 2023-09-07 · ·

An evaporator is provided that includes a porous sintered body. The porous sintered body is formed by a composite of at least one electrically conductive material and at least one dielectric material. The sintered body has an open porosity in a range from 10 to 90% and an electrical conductivity in a range from 0.1 to 105 S/m. The fraction of electrically conductive material in the sintered body is a maximum of 90 wt. %.

CAPACITOR COMPONENT AND PASTE FOR EXTERNAL ELECTRODE

A capacitor component includes a body, including a dielectric layer and an internal electrode layer, and an external electrode disposed on one surface of the body. The external electrode includes a conductive base and a glass disposed in the conductive base, and the glass includes 0.01 wt % or more to 5.8 wt % or less of nitrogen (N) based on a total weight of the glass.

CAPACITOR COMPONENT AND PASTE FOR EXTERNAL ELECTRODE

A capacitor component includes a body, including a dielectric layer and an internal electrode layer, and an external electrode disposed on one surface of the body. The external electrode includes a conductive base and a glass disposed in the conductive base, and the glass includes 0.01 wt % or more to 5.8 wt % or less of nitrogen (N) based on a total weight of the glass.

COMPLIANT SOLID-STATE IONICALLY CONDUCTIVE COMPOSITE MATERIALS AND METHOD FOR MAKING SAME

Provided herein are ionically conductive solid-state compositions that include ionically conductive inorganic particles in a matrix of an organic material. The resulting composite material has high ionic conductivity and mechanical properties that facilitate processing. In particular embodiments, the ionically conductive solid-state compositions are compliant and may be cast as films. In some embodiments of the present invention, solid-state electrolytes including the ionically conductive solid-state compositions are provided. In some embodiments of the present invention, electrodes including the ionically conductive solid-state compositions are provided. The present invention further includes embodiments that are directed to methods of manufacturing the ionically conductive solid-state compositions and batteries incorporating the ionically conductive solid-state compositions.

COMPLIANT SOLID-STATE IONICALLY CONDUCTIVE COMPOSITE MATERIALS AND METHOD FOR MAKING SAME

Provided herein are ionically conductive solid-state compositions that include ionically conductive inorganic particles in a matrix of an organic material. The resulting composite material has high ionic conductivity and mechanical properties that facilitate processing. In particular embodiments, the ionically conductive solid-state compositions are compliant and may be cast as films. In some embodiments of the present invention, solid-state electrolytes including the ionically conductive solid-state compositions are provided. In some embodiments of the present invention, electrodes including the ionically conductive solid-state compositions are provided. The present invention further includes embodiments that are directed to methods of manufacturing the ionically conductive solid-state compositions and batteries incorporating the ionically conductive solid-state compositions.