C04B5/06
Mineralizer Composition and Pidgeon Silicothermic Process for Smelting Magnesium
A mineralizer composition for Pidgeon silicothermic process for smelting magnesium consists of fluorite and a boron-containing compound. Amounts of the fluorite and the boron-containing compound meet the following equation:
M.sub.fluo-original=(1−x)M.sub.fluo+(m)(x)M.sub.B,
where, M.sub.fluo-original is a mass of the fluorite required in a conventional Pidgeon silicothermic process in which no boron-containing compound is introduced to replace a fraction or all of the total fluorite, M.sub.fluo is a mass of the fluorite in the composition, M.sub.B is a mass of the boron-containing compound in the composition, 0.5≤x≤1, and 2≤m≤8. A Pidgeon silicothermic process for smelting magnesium is also provided, which employs the mineralizer composition. The composition and process of the disclosure enable reduction and even avoidance of dust pollution caused by fluorite-containing magnesium slag.
Method for preparing a cementing material using smelting industrial waste slag after utilizing the simultaneous removal of S02 and NOx in flue gas and application of the cementing material obtained by the same
The invention belongs to the technical field of the resource treatment of industrial wastes, and particularly relates to a method for preparing a cementing material using smelting industrial waste slag after utilizing the simultaneous removal of SO.sub.2 and NO.sub.x in flue gas and an application of the cementing material obtained by the same. According to the invention, SO.sub.2 and NO.sub.x in the flue gas can be treated with the smelting industrial waste slag, meeting requirement of flue gas desulfurization and denitration; moreover, the smelting industrial waste slag can be purified and separated by means of waste gas resources to obtain a cementing material, realizing the resource utilization of the smelting industrial waste slag and waste gas.
METHOD FOR PREPARING A CEMENTING MATERIAL USING SMELTING INDUSTRIAL WASTE SLAG AFTER UTILIZING THE SIMULTANEOUS REMOVAL OF SO2 AND NOx IN FLUE GAS AND APPLICATION OF THE CEMENTING MATERIAL OBTAINED BY THE SAME
The invention belongs to the technical field of the resource treatment of industrial wastes, and particularly relates to a method for preparing a cementing material using smelting industrial waste slag after utilizing the simultaneous removal of SO.sub.2 and NO.sub.x in flue gas and an application of the cementing material obtained by the same. According to the invention, SO.sub.2 and NO.sub.x in the flue gas can be treated with the smelting industrial waste slag, meeting requirement of flue gas desulfurization and denitration; moreover, the smelting industrial waste slag can be purified and separated by means of waste gas resources to obtain a cementing material, realizing the resource utilization of the smelting industrial waste slag and waste gas.
CONSTRUCTION ELEMENTS WITH SLAG FROM NON-FERROUS METAL PRODUCTION
Disclosed is a method of fabricating a construction element, the method comprising the manufacturing of a construction element including a slag, wherein the slag is comprising, on a dry basis and whereby the presence of a metal is expressed as the total of the metal present as elemental metal and the presence of the metal in an oxidized state, a) at least 7% wt and at most 49% wt of iron, Fe, b) at most 1.3% wt of copper, Cu, c) at least 24% wt and at most 44% wt of silicon dioxide, SiO.sub.2, d) at least 1.0% wt and at most 20% wt of calcium oxide, CaO, e) at least 0.10% wt and at most 1.50% wt of zinc, Zn, f) at least 0.10% wt and at most 2.5% wt of magnesium oxide, MgO, and g) at most 0.100% wt of lead, Pb.
Further disclosed are improved construction elements comprising the slag.
CONSTRUCTION ELEMENTS WITH SLAG FROM NON-FERROUS METAL PRODUCTION
Disclosed is a method of fabricating a construction element, the method comprising the manufacturing of a construction element including a slag, wherein the slag is comprising, on a dry basis and whereby the presence of a metal is expressed as the total of the metal present as elemental metal and the presence of the metal in an oxidized state, a) at least 7% wt and at most 49% wt of iron, Fe, b) at most 1.3% wt of copper, Cu, c) at least 24% wt and at most 44% wt of silicon dioxide, SiO.sub.2, d) at least 1.0% wt and at most 20% wt of calcium oxide, CaO, e) at least 0.10% wt and at most 1.50% wt of zinc, Zn, f) at least 0.10% wt and at most 2.5% wt of magnesium oxide, MgO, and g) at most 0.100% wt of lead, Pb.
Further disclosed are improved construction elements comprising the slag.
Steel product, cement manufacturing process and cement
The present invention relates to a novel cementitious product produced from steelworks slag additivation to obtain material having properties suitable for use in the partial or total clinker replacement for the production of different types of cement. The process, which is also object of this invention, aims to adapt the properties of steelworks slag, by means of thermochemical treatment, including and preferably, but not only, still in the liquid steelworks slag pot, taking advantage of the thermal input of steel processing, to form a greater amount of alite (essential compound to increase pozzolanicity), under controlled conditions. After additivation, preferably, but not exclusively, the additivated steelworks slag is subjected to quenching, comminution and concentration to stabilize the alite fraction, to release the present phases and to remove any excess contaminants, such as metallic iron.
Steel product, cement manufacturing process and cement
The present invention relates to a novel cementitious product produced from steelworks slag additivation to obtain material having properties suitable for use in the partial or total clinker replacement for the production of different types of cement. The process, which is also object of this invention, aims to adapt the properties of steelworks slag, by means of thermochemical treatment, including and preferably, but not only, still in the liquid steelworks slag pot, taking advantage of the thermal input of steel processing, to form a greater amount of alite (essential compound to increase pozzolanicity), under controlled conditions. After additivation, preferably, but not exclusively, the additivated steelworks slag is subjected to quenching, comminution and concentration to stabilize the alite fraction, to release the present phases and to remove any excess contaminants, such as metallic iron.
Steel product, cement manufacturing process and cement
The present invention relates to a novel cementitious product produced from steelworks slag additivation to obtain material having properties suitable for use in the partial or total clinker replacement for the production of different types of cement. The process, which is also object of this invention, aims to adapt the properties of steelworks slag, by means of thermochemical treatment, including and preferably, but not only, still in the liquid steelworks slag pot, taking advantage of the thermal input of steel processing, to form a greater amount of alite (essential compound to increase pozzolanicity), under controlled conditions. After additivation, preferably, but not exclusively, the additivated steelworks slag is subjected to quenching, comminution and concentration to stabilize the alite fraction, to release the present phases and to remove any excess contaminants, such as metallic iron.
Slag from non-ferrous metal production
Disclosed is a slag comprising, on a dry basis and expressed as the total of the metal present as elemental metal and the presence of the metal in an oxidized state, a) at least 7% wt and at most 49% wt of Fe, b) at most 1.3% wt of Cu, c) at least 24% wt and at most 44% wt of SiO.sub.2, and d) at least 2.0% wt and at most 20% wt of CaO, characterised in that the slag comprises, on the same basis, e) at least 0.10% wt and at most 1.00% wt of Zn, f) at least 0.10% wt and at most 2.5% wt of MgO, and g) at most 0.100% wt of Pb. Further disclosed are an improved object comprising the slag, a process for the production of the slag, and a number of uses of the slag, whereby the slag may comprise up to at most 1.50% wt of zinc and down to 1.0% wt of CaO.
Slag from non-ferrous metal production
Disclosed is a slag comprising, on a dry basis and expressed as the total of the metal present as elemental metal and the presence of the metal in an oxidized state, a) at least 7% wt and at most 49% wt of Fe, b) at most 1.3% wt of Cu, c) at least 24% wt and at most 44% wt of SiO.sub.2, and d) at least 2.0% wt and at most 20% wt of CaO, characterised in that the slag comprises, on the same basis, e) at least 0.10% wt and at most 1.00% wt of Zn, f) at least 0.10% wt and at most 2.5% wt of MgO, and g) at most 0.100% wt of Pb. Further disclosed are an improved object comprising the slag, a process for the production of the slag, and a number of uses of the slag, whereby the slag may comprise up to at most 1.50% wt of zinc and down to 1.0% wt of CaO.