C04B9/02
Curable formulations for structural and non-structural applications
According to some embodiments, a curable mixture configured to set in the presence of water, wherein the mixture comprises magnesium oxide, a primary cementitious component and at least one accelerant. A proportion by weight of the primary cementitious component is 80% to 120% of a proportion of magnesium oxide by weight.
Curable formulations for structural and non-structural applications
According to some embodiments, a curable mixture configured to set in the presence of water, wherein the mixture comprises magnesium oxide, a primary cementitious component and at least one accelerant. A proportion by weight of the primary cementitious component is 80% to 120% of a proportion of magnesium oxide by weight.
Method to make ultra stable structural laminate
A method to make an ultra-stable structural laminate of a cementitious material with a nano-molecular veneer and a foam component catalytically reacted into an expanded closed cell foam having a thickness from .sup.th inch to 8 inches, a density from 1.5 pounds/cubic foot to 3 pounds/cubic foot that inter-engages the cementitious material forming a matrix creating the ultra-stable structural laminate with fire resistance; a lateral nail pull strength from 44 pounds to 300 pounds of force; an insulation R value from 1 to 40; a resistance to seismic impact for earthquakes over 3.1 on the Richter Scale; a break point from 7 lbs/inch to 100 lbs/inch; and a resistance to wind shear equivalent to a 15 mph downburst.
Method to make ultra stable structural laminate
A method to make an ultra-stable structural laminate of a cementitious material with a nano-molecular veneer and a foam component catalytically reacted into an expanded closed cell foam having a thickness from .sup.th inch to 8 inches, a density from 1.5 pounds/cubic foot to 3 pounds/cubic foot that inter-engages the cementitious material forming a matrix creating the ultra-stable structural laminate with fire resistance; a lateral nail pull strength from 44 pounds to 300 pounds of force; an insulation R value from 1 to 40; a resistance to seismic impact for earthquakes over 3.1 on the Richter Scale; a break point from 7 lbs/inch to 100 lbs/inch; and a resistance to wind shear equivalent to a 15 mph downburst.
Building with ultra stable cementitious material formulation
A building with ultra-stable cementitious material with nano-molecular veneer has 29 wt % to 40 wt % of a magnesium oxide dry powder containing 80 wt % to 98 wt % of magnesium oxide based on a final total weight of the cementitious material, 14 wt % to 18 wt % of a magnesium chloride dissolved in water and reacting to form a liquid suspension, a phosphorus-containing material, and wherein the mixture forms a liquid suspension that reacts into an amorphous phase cementitious material, wherein a portion of the amorphous phase cementitious material grows a plurality of crystals. The plurality of crystals are encapsulated by the amorphous phase cementitious material forming a nano-molecular veneer and a wall material that is affixed to a frame of a building.
Building with ultra stable cementitious material formulation
A building with ultra-stable cementitious material with nano-molecular veneer has 29 wt % to 40 wt % of a magnesium oxide dry powder containing 80 wt % to 98 wt % of magnesium oxide based on a final total weight of the cementitious material, 14 wt % to 18 wt % of a magnesium chloride dissolved in water and reacting to form a liquid suspension, a phosphorus-containing material, and wherein the mixture forms a liquid suspension that reacts into an amorphous phase cementitious material, wherein a portion of the amorphous phase cementitious material grows a plurality of crystals. The plurality of crystals are encapsulated by the amorphous phase cementitious material forming a nano-molecular veneer and a wall material that is affixed to a frame of a building.
CURABLE FORMULATIONS FOR STRUCTURAL AND NON-STRUCTURAL APPLICATIONS
According to some embodiments, a curable mixture configured to set in the presence of water, wherein the mixture comprises magnesium oxide, a primary cementitious component and at least one accelerant. A proportion by weight of the primary cementitious component is 80% to 120% of a proportion of magnesium oxide by weight.
CURABLE FORMULATIONS FOR STRUCTURAL AND NON-STRUCTURAL APPLICATIONS
According to some embodiments, a curable mixture configured to set in the presence of water, wherein the mixture comprises magnesium oxide, a primary cementitious component and at least one accelerant. A proportion by weight of the primary cementitious component is 80% to 120% of a proportion of magnesium oxide by weight.
Curable formulations for structural and non-structural applications
According to some embodiments, a curable mixture configured to set in the presence of water, wherein the mixture comprises magnesium oxide, a primary cementitious component (e.g., slag cement) and at least one accelerant. A proportion by weight of the primary cementitious component is 80% to 120% of a proportion of magnesium oxide by weight.
Curable formulations for structural and non-structural applications
According to some embodiments, a curable mixture configured to set in the presence of water, wherein the mixture comprises magnesium oxide, a primary cementitious component (e.g., slag cement) and at least one accelerant. A proportion by weight of the primary cementitious component is 80% to 120% of a proportion of magnesium oxide by weight.