C04B14/38

METHOD FOR MANUFACTURING BUILDING MATERIAL

[Object] To provide a building material having excellent durability.

[Solution] A building material has a convex part formed on a surface thereof, the convex part including a first lateral surface part and a second lateral surface part corresponding to the first lateral surface part. The building material is formed from a mixture containing a hydraulic material, an admixture, and a plant-based reinforcing material, and the plant-based reinforcing material at least in the convex part is distributed in the mixture with the hydraulic material and the admixture attached to the plant-based reinforcing material. A distribution of the plant-based reinforcing material in the first lateral surface part and a distribution of the plant-based reinforcing material in the second lateral surface part are substantially the same. Desirably, the convex part includes a first edge part that is an edge part of the first lateral surface part and a second edge part that is an edge part of the second lateral surface part and that corresponds to the first edge part, and a distribution of holes formed in the first edge part and a distribution of holes formed in the second edge part are substantially the same.

METHOD FOR MANUFACTURING BUILDING MATERIAL

[Object] To provide a building material having excellent durability.

[Solution] A building material has a convex part formed on a surface thereof, the convex part including a first lateral surface part and a second lateral surface part corresponding to the first lateral surface part. The building material is formed from a mixture containing a hydraulic material, an admixture, and a plant-based reinforcing material, and the plant-based reinforcing material at least in the convex part is distributed in the mixture with the hydraulic material and the admixture attached to the plant-based reinforcing material. A distribution of the plant-based reinforcing material in the first lateral surface part and a distribution of the plant-based reinforcing material in the second lateral surface part are substantially the same. Desirably, the convex part includes a first edge part that is an edge part of the first lateral surface part and a second edge part that is an edge part of the second lateral surface part and that corresponds to the first edge part, and a distribution of holes formed in the first edge part and a distribution of holes formed in the second edge part are substantially the same.

Energy efficient cementitious mortars

Thermally conductive cementitious compositions for use in flooring installations that are applied over a heat radiating flooring system to increase the thermal conductance of the flooring system and increase the rate of heating the flooring system. The thermally conductive cementitious compositions include a cementitious composition, amorphous flake graphite carbon, and an aqueous solution suitable for use as a thermally conductive mortar, grout or adhesive for flooring installations. The thermally conductive cementitious compositions also include a cementitious composition, mesh fine aluminum oxide, mesh coarse aluminum oxide, and an aqueous solution that provides a thermally conductive mortar, grout or adhesive for use in flooring installations.

Energy efficient cementitious mortars

Thermally conductive cementitious compositions for use in flooring installations that are applied over a heat radiating flooring system to increase the thermal conductance of the flooring system and increase the rate of heating the flooring system. The thermally conductive cementitious compositions include a cementitious composition, amorphous flake graphite carbon, and an aqueous solution suitable for use as a thermally conductive mortar, grout or adhesive for flooring installations. The thermally conductive cementitious compositions also include a cementitious composition, mesh fine aluminum oxide, mesh coarse aluminum oxide, and an aqueous solution that provides a thermally conductive mortar, grout or adhesive for use in flooring installations.

Anti-blast concrete and method of fabricating anti-blast structure member using such anti-blast concrete

An anti-blast concrete and a method of fabricating an anti-blast structure member using such anti-blast concrete are disclosed. The composition of the anti-blast concrete according to the invention includes, in parts by weight, 1.0 part by weight of cement, 1.0 to 2.5 parts by weight of fine aggregates, 1.0 to 2.5 parts by weight of coarse aggregates, and a plurality of reinforcing fibers. The weight ratio of the reinforcing fibers to the cement ranges from 0.5% to 3%. The plurality of reinforcing fibers are a plurality of carbon fibers or a plurality of aramid fibers. A test body, made of the anti-blast concrete of the invention, has an average number of times of repeated impacts at an impact energy of 49.0 Joules equal to or larger than 41 times at 28 days of age.

Inorganic fiber toughened inorganic composite artificial stone panel and preparation method thereof

An inorganic fiber toughened inorganic composite artificial stone panel and a preparation method thereof are disclosed. The panel includes a surface layer and a toughened base layer. The surface layer includes the the following components in parts by weight: 40-70 parts of quartz sand, 10-30 parts of quartz powder, 20-45 parts of inorganic active powder, 0.5-4 parts of pigment, 0.3-1 parts of water reducing agent and 3-10 parts of water. The toughened base layer includes the following components in parts by weight: 40-60 parts of inorganic active powder, 45-65 parts of sand, 0.8-1.5 parts of water reducing agent, 6-14 parts of water, 0.4-2 parts of inorganic fiber and 0.8-2.5 parts of toughener.

Inorganic fiber toughened inorganic composite artificial stone panel and preparation method thereof

An inorganic fiber toughened inorganic composite artificial stone panel and a preparation method thereof are disclosed. The panel includes a surface layer and a toughened base layer. The surface layer includes the the following components in parts by weight: 40-70 parts of quartz sand, 10-30 parts of quartz powder, 20-45 parts of inorganic active powder, 0.5-4 parts of pigment, 0.3-1 parts of water reducing agent and 3-10 parts of water. The toughened base layer includes the following components in parts by weight: 40-60 parts of inorganic active powder, 45-65 parts of sand, 0.8-1.5 parts of water reducing agent, 6-14 parts of water, 0.4-2 parts of inorganic fiber and 0.8-2.5 parts of toughener.

Inorganic fiber toughened inorganic composite artificial stone panel and preparation method thereof

An inorganic fiber toughened inorganic composite artificial stone panel and a preparation method thereof are disclosed. The panel includes a surface layer and a toughened base layer. The surface layer includes the the following components in parts by weight: 40-70 parts of quartz sand, 10-30 parts of quartz powder, 20-45 parts of inorganic active powder, 0.5-4 parts of pigment, 0.3-1 parts of water reducing agent and 3-10 parts of water. The toughened base layer includes the following components in parts by weight: 40-60 parts of inorganic active powder, 45-65 parts of sand, 0.8-1.5 parts of water reducing agent, 6-14 parts of water, 0.4-2 parts of inorganic fiber and 0.8-2.5 parts of toughener.

Eco-Friendly, Crack-Resistant Cementitious Materials

Provided herein are cementitious materials, for example, a crack-resistant cementitious mortar. The cementitious materials are a mixture of cement, at least one recycled fiber reinforcement material, a recycled aggregate material, and water. Also provided is a method for increasing the crack-resistance of a cementitious material by replacing the sand in a cement mortar with a recycled aggregate material and adding at least one recycled fiber reinforcement material and a volume of water.

IMPROVED FIBER CEMENT PRODUCTS AND METHODS FOR THE PRODUCTION THEREOF
20220332643 · 2022-10-20 ·

The present invention relates to fiber cement products comprising an inner core material, which inner core material is covered by at least one outer surface layer, characterized in that: —said inner core material has a density of between about 0.4 and about 0.9 g/cm.sup.3 inclusive, and at least comprises cement and between 1 wt % and 70 wt % (with respect to the total dry weight of said inner core material) of a lightweight filler, and—said at least one outer surface layer has a density of between about 0.9 and about 1.4 g/cm.sup.3 inclusive, and at least comprises fibers and cement.