C04B35/71
Compliant layer for ceramic components and methods of forming the same
An apparatus includes a ceramic matrix composite (CMC) component and an interface coating on the CMC component, wherein the interface coating includes a layer of at least one of the following compositions: 40-50 wt % Nb, 28-42 wt % Al, 4-15 wt % Cr, 1-2 wt % Si; 90-92 wt % Mo, 4-5 wt % Si, 4-5 wt % B; or 60-80 wt % V, 20-30 wt % Cr, 2-15 wt % Ti.
Discontinuous Molded Tape Wear Interface for Composite Components
Composite components that include features that provide improved wear characteristics at the interface between the composite component and a second component are provided. As one example, a composite component can include an integrally formed discontinuous molded tape (DMT) that defines a wear interface between the component and a second component. The wear interface defined by the DMT may provide improved durability of the composite component and may facilitate more uniform wear at the interface, among other benefits. Methods for manufacturing composite components having discontinuous molded tape wear interfaces are also provided.
Discontinuous Molded Tape Wear Interface for Composite Components
Composite components that include features that provide improved wear characteristics at the interface between the composite component and a second component are provided. As one example, a composite component can include an integrally formed discontinuous molded tape (DMT) that defines a wear interface between the component and a second component. The wear interface defined by the DMT may provide improved durability of the composite component and may facilitate more uniform wear at the interface, among other benefits. Methods for manufacturing composite components having discontinuous molded tape wear interfaces are also provided.
REFRACTORY CONTAINER MADE OF A CERAMIC MATERIAL, GREEN BODY FOR SUCH A CONTAINER, AND METHOD FOR THE MANUFACTURE OF A REFRACTORY CONTAINER MADE OF A CERAMIC MATERIAL AND OF A GREEN BODY PROVIDED FOR THIS PURPOSE
The invention relates to a refractory container 1 for use in a furnace for heat treatment of workpieces, comprising a mat 5 of long fibers that are embedded in a ceramic shell, with the mat 5 being shaped into a container that forms a receiving space for workpieces, and to a green body of such a container 1. Furthermore, advantageous uses of the container 1 as well as a method for manufacturing a green body or container 1 according to the invention are specified.
REFRACTORY CONTAINER MADE OF A CERAMIC MATERIAL, GREEN BODY FOR SUCH A CONTAINER, AND METHOD FOR THE MANUFACTURE OF A REFRACTORY CONTAINER MADE OF A CERAMIC MATERIAL AND OF A GREEN BODY PROVIDED FOR THIS PURPOSE
The invention relates to a refractory container 1 for use in a furnace for heat treatment of workpieces, comprising a mat 5 of long fibers that are embedded in a ceramic shell, with the mat 5 being shaped into a container that forms a receiving space for workpieces, and to a green body of such a container 1. Furthermore, advantageous uses of the container 1 as well as a method for manufacturing a green body or container 1 according to the invention are specified.
COMPOSITIONS FOR EROSION AND MOLTEN DUST RESISTANT ENVIRONMENTAL BARRIER COATINGS
Coating systems are provided for positioning on a surface of a substrate, along with the resulting coated components and methods of their formation. The coating system may include a layer having a compound of the formula: A.sub.1bB.sub.bZ.sub.1dD.sub.dMO.sub.6 where: A is Al, Ga, In, Sc, Y, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, Fe, Cr, Co, Mn, Bi, or a mixture thereof; b is 0 to about 0.5; Z is Hf, Ti, or a mixture thereof; D is Zr, Ce, Ge, Si, or a mixture thereof; d is 0 to about 0.5; and M is Ta, Nb, or a mixture thereof.
COMPOSITIONS FOR EROSION AND MOLTEN DUST RESISTANT ENVIRONMENTAL BARRIER COATINGS
Coating systems are provided for positioning on a surface of a substrate, along with the resulting coated components and methods of their formation. The coating system may include a layer having a compound of the formula: A.sub.1bB.sub.bZ.sub.1dD.sub.dMO.sub.6 where: A is Al, Ga, In, Sc, Y, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, Fe, Cr, Co, Mn, Bi, or a mixture thereof; b is 0 to about 0.5; Z is Hf, Ti, or a mixture thereof; D is Zr, Ce, Ge, Si, or a mixture thereof; d is 0 to about 0.5; and M is Ta, Nb, or a mixture thereof.
Carbon composites
A carbon composite comprises: at least two carbon microstructures; and a binding phase disposed between the at least two carbon microstructures; wherein the binding phase includes a binder comprising one or more of the following SiO.sub.2; Si; B; B.sub.2O.sub.3; a metal; or an alloy of the metal, and the metal is at least one of aluminum; copper; titanium; nickel; tungsten; chromium; iron; manganese; zirconium; hafnium; vanadium; niobium; molybdenum; tin; bismuth; antimony; lead; cadmium; or selenium.
Carbon composites
A carbon composite comprises: at least two carbon microstructures; and a binding phase disposed between the at least two carbon microstructures; wherein the binding phase includes a binder comprising one or more of the following SiO.sub.2; Si; B; B.sub.2O.sub.3; a metal; or an alloy of the metal, and the metal is at least one of aluminum; copper; titanium; nickel; tungsten; chromium; iron; manganese; zirconium; hafnium; vanadium; niobium; molybdenum; tin; bismuth; antimony; lead; cadmium; or selenium.
Methods to fabricate needled preforms with randomly oriented short length carbon fibers
A method and apparatus for fabricating a short length carbon fiber preform with a through thickness reinforcement is disclosed herein. The starting media for fabricating a net shape (e.g., annular disc) may meet specific requirements including a sufficient fiber volume and a binding mechanism compatible with the needle-punching process.