C04B40/0089
HIGH TOUGHNESS INORGANIC COMPOSITE ARTIFICIAL STONE PANEL AND PREPARATION METHOD THEREOF
A high toughness inorganic composite artificial stone panel and preparation method are disclosed. The panel includes a surface layer, an intermediate metal fiber toughening layer and a substrate toughening layer. The surface layer includes the following components: 40-70 parts of quartz sand, 10-30 parts of quartz powder, 20-45 parts of inorganic active powder, 0.5-4 parts of pigment, 0.3-1 part of water reducer and 3-10 parts of water. The intermediate metal fiber toughening layer includes the following components: 40-60 parts of inorganic active powder, 45-65 parts of sand, 0.8-1.5 parts of water reducer, 6-14 parts of water and 4-8 parts of metal fiber. The substrate toughening layer includes the following components: 30-50 parts of inorganic active powder, 30-55 parts of quartz sand, 15-20 parts of quartz powder, 0.5-1.2 parts of water reducer, 4-8 parts of water and 0.8-2.5 parts of toughening agent.
Inorganic fiber toughened inorganic composite artificial stone panel and preparation method thereof
An inorganic fiber toughened inorganic composite artificial stone panel and a preparation method thereof are disclosed. The panel includes a surface layer and a toughened base layer. The surface layer includes the the following components in parts by weight: 40-70 parts of quartz sand, 10-30 parts of quartz powder, 20-45 parts of inorganic active powder, 0.5-4 parts of pigment, 0.3-1 parts of water reducing agent and 3-10 parts of water. The toughened base layer includes the following components in parts by weight: 40-60 parts of inorganic active powder, 45-65 parts of sand, 0.8-1.5 parts of water reducing agent, 6-14 parts of water, 0.4-2 parts of inorganic fiber and 0.8-2.5 parts of toughener.
Inorganic fiber toughened inorganic composite artificial stone panel and preparation method thereof
An inorganic fiber toughened inorganic composite artificial stone panel and a preparation method thereof are disclosed. The panel includes a surface layer and a toughened base layer. The surface layer includes the the following components in parts by weight: 40-70 parts of quartz sand, 10-30 parts of quartz powder, 20-45 parts of inorganic active powder, 0.5-4 parts of pigment, 0.3-1 parts of water reducing agent and 3-10 parts of water. The toughened base layer includes the following components in parts by weight: 40-60 parts of inorganic active powder, 45-65 parts of sand, 0.8-1.5 parts of water reducing agent, 6-14 parts of water, 0.4-2 parts of inorganic fiber and 0.8-2.5 parts of toughener.
Organic fiber toughened inorganic composite artificial stone panel and preparation method thereof
An organic fiber toughened inorganic composite artificial stone panel and a preparation method thereof are disclosed. The panel includes a surface layer, an intermediate organic fiber toughened layer and a toughened base layer. The surface layer includes the following components: 40-70 parts of quartz sand, 20-30 parts of quartz powder, 20-45 parts of inorganic active powder, 0.5-4 parts of pigment, 0.1-3 part of water reducing agent and 3-10 parts of water. The intermediate organic fiber toughened layer includes the following components: 40-60 parts of inorganic active powder, 45-65 parts of sand, 0.8-1.5 parts of water reducing agent, 6-14 parts of water and 4-8 parts of organic fiber. The toughened base layer includes the following components: 30-50 parts of inorganic active powder, 30-55 parts of quartz sand, 15-20 parts of quartz powder, 0.5-1.2 parts of water reducing agent, 4-8 parts of water and 0.8-2.5 parts of toughener.
Organic fiber toughened inorganic composite artificial stone panel and preparation method thereof
An organic fiber toughened inorganic composite artificial stone panel and a preparation method thereof are disclosed. The panel includes a surface layer, an intermediate organic fiber toughened layer and a toughened base layer. The surface layer includes the following components: 40-70 parts of quartz sand, 20-30 parts of quartz powder, 20-45 parts of inorganic active powder, 0.5-4 parts of pigment, 0.1-3 part of water reducing agent and 3-10 parts of water. The intermediate organic fiber toughened layer includes the following components: 40-60 parts of inorganic active powder, 45-65 parts of sand, 0.8-1.5 parts of water reducing agent, 6-14 parts of water and 4-8 parts of organic fiber. The toughened base layer includes the following components: 30-50 parts of inorganic active powder, 30-55 parts of quartz sand, 15-20 parts of quartz powder, 0.5-1.2 parts of water reducing agent, 4-8 parts of water and 0.8-2.5 parts of toughener.
Synthetic stone
A synthetic stone for decorative purposes, countertops, flooring, and the like comprises, as a major component, magnesium compounds, and includes diamond or quartz sand. It is formed via a vibro-compression process that is conducted under vacuum and at ambient temperature. The synthetic stone slab is very hard, waterproof, mildew-proof, insect-proof, environmentally friendly, and low cost.
Synthetic stone
A synthetic stone for decorative purposes, countertops, flooring, and the like comprises, as a major component, magnesium compounds, and includes diamond or quartz sand. It is formed via a vibro-compression process that is conducted under vacuum and at ambient temperature. The synthetic stone slab is very hard, waterproof, mildew-proof, insect-proof, environmentally friendly, and low cost.
METHOD FOR MANUFACTURING ARTICLES IN THE FORM OF A SLAB OR BLOCK WITH A HARDENING BINDER, AND ARTICLES THUS OBTAINED
In a method for manufacturing articles in the form of a slab or block, obtained by means of a procedure during which an initial mix comprising aggregates and a binder undergo vacuum vibro-compression followed by a step involving hardening of the binder, the aggregates comprise synthetic aggregates and fillers with a hardness greater than or equal to 5 Mohs, which contain silicon dioxide substantially only in amorphous form.
Environment-friendly Artificial Stone with Low Cost and High Strength and A Preparation Method Thereof
The invention relates to an environment-friendly artificial stone with low cost and high strength and a preparation method thereof, the artificial stone comprises the following raw materials in parts by mass: 60-80 parts of fritted sand; 10-30 parts of quartz powder; 9-14 parts of terephthalic unsaturated polyester resin; 0.6-1 parts of curing agent; 0.8-1 parts of coupling agent; 0.5-1 parts of pigment paste; 0.1-1 parts of pigment powder. The invention has advantages of: (1) using mine solid waste or waste materials as raw materials, and using blast-furnace gas and coke-oven gas recovered and purified in the productive process of the steel plant and coking plant as fuel, the production process is green and environment-friendly, which can recycle waste materials. (2) high strength, natural stripe, elegance appearance, green and environmental protection, and being recognized by global customers and promising in worldwide market.
DECORATIVE COATING METHODS, SYSTEMS, AND DEVICES
A decorative coatings method, system, device, and composition, wherein the initial part may be the blending of several materials to create the face coat. The next step may be the application of this face coat into a mold. Then the backfilling of this mold with another blended material that is not usually associated with the face coat. The method ensures the adhesion of the backfill to the face coat. The specific mixtures allow the materials to bond and form a solid product when removed from the mold.