C04B2103/10

SYSTEM FOR MANUFACTURING CEMENTITIOUS PRODUCT WITH SECONDARY DISCHARGE CONDUIT HAVING ADDITIVE INJECTION SYSTEM

An additive injection system can be a part of a cementitious slurry mixing and dispensing assembly. The additive injection system can be used to inject an additive into an auxiliary slurry discharge conduit carrying a secondary flow of cementitious slurry produced in the assembly such that the secondary slurry stream is different from a main slurry stream discharged from a main slurry discharge conduit.

Methods of Making and Using a Cementitious Composition with Ultra-Low Portland Cement

Disclosed herein is a method of servicing a wellbore penetrating a subterranean formation, comprising: placing a cementitious composition of the type disclosed herein into the wellbore. The cementitious composition comprises a cement blend and water, wherein the cement blend comprises Portland cement and pozzolan, wherein the Portland cement is present in an amount of from equal to or greater than about 0.01 wt. % to equal to or less than about 25.0 wt. % based on the total weight of the cement blend.

Methods of Making and Using a Cementitious Composition with Ultra-Low Portland Cement

Disclosed herein is a method of servicing a wellbore penetrating a subterranean formation, comprising: placing a cementitious composition of the type disclosed herein into the wellbore. The cementitious composition comprises a cement blend and water, wherein the cement blend comprises Portland cement and pozzolan, wherein the Portland cement is present in an amount of from equal to or greater than about 0.01 wt. % to equal to or less than about 25.0 wt. % based on the total weight of the cement blend.

METHOD FOR MANUFACTURING COAL-BASED GEOPOLYMER FOAM INCLUDING SILICA FUME
20230202923 · 2023-06-29 · ·

Disclosed herein are a lightweight geopolymer foam with low thermal conductivity and a manufacturing method therefor in which coal bottom ash and fly ash are used together as materials for the geopolymer foam and silica fume is added to a mixed solution of an alkali activator and sodium hydroxide. The geopolymer foam can be utilized for improving insulation performance and safety for a structure constructed with eco-friendly cement.

Coated fibre and concrete composition comprising the same

A coated fiber comprising a fiber comprising polyester, and a coating on the fiber, said coating comprising a cross-linked silicone prepared by cross-linking on the fiber one or more silicon-containing compounds selected from an organosilane and organosilicone resin, wherein at least one of said silicon-containing compounds has at least three cross-linking groups is provided, together with a method of preparing such a fiber, a concrete composition comprising such coated fibers, and a method of preparing such a concrete composition.

Coated fibre and concrete composition comprising the same

A coated fiber comprising a fiber comprising polyester, and a coating on the fiber, said coating comprising a cross-linked silicone prepared by cross-linking on the fiber one or more silicon-containing compounds selected from an organosilane and organosilicone resin, wherein at least one of said silicon-containing compounds has at least three cross-linking groups is provided, together with a method of preparing such a fiber, a concrete composition comprising such coated fibers, and a method of preparing such a concrete composition.

Voltage source with an electrolyte containing ash, and method for manufacturing the voltage source
11688859 · 2023-06-27 · ·

A voltage source includes two electrically conductive terminals (101, 102) with an electrolyte (103) between them. Said electrolyte (103) is a mixture in which the main component is ash produced in a power plant or an incineration plant.

GYPSUM FIBER BOARD AND METHOD FOR PRODUCING GYPSUM FIBER BOARDS

A gypsum fiber board produced in a Siempelkamp dry-process, comprising 75 wt % to 90 wt % (relative to the total dry mix) of calcium sulfate hemi-hydrate and 10 wt % to 25 wt % (relative to the total dry mix) paper fibers, wherein the calcium sulfate hemi-hydrate is a mixture of α-calcium sulfate hemi-hydrate and β-calcium sulfate hemi-hydrate, wherein the content of α-calcium sulfate hemi-hydrate in the mixture is at least 5 wt % (relative to the total calcium sulfate hemi-hydrate) is disclosed. Also disclosed is a method for producing a gypsum fiber board of a thickness of 23 mm in a Siempelkamp dry-process.

Composition for manufacturing artificial marble
11685692 · 2023-06-27 · ·

The present invention relates to a composition for manufacturing artificial marble including a first preliminary composition and a second preliminary composition which include an acrylic-based monomer, an acrylic-based resin, a polymerization initiator, a crosslinking agent, a coloring agent, and a gelling agent and have a viscosity of 100,000 Ps to 5,000,000 Ps and/or a storage modulus of 100,000 Pa to 1,000,000 Pa. A viscosity of the second preliminary composition is higher than a viscosity of the first preliminary composition. Coloring agents of the first preliminary composition and the second preliminary composition have different colors. A weight ratio of the first preliminary composition to the second preliminary composition is in a range of 1:1 to 500:1. According to the present invention, artificial marble having a dashed pattern similar to that of natural marble is provided by increasing viscoelasticity to prepare semi-solid preliminary compositions for manufacturing artificial marble, having excellent workability and machinability, preparing a composition for manufacturing artificial marble by mixing two or more of the semi-solid preliminary compositions, and performing various molding and machining processes on the composition.

GYPSUM WALLBOARD AND RELATED METHODS AND SLURRIES
20170362124 · 2017-12-21 ·

Disclosed is a gypsum board comprising a set gypsum core disposed between two cover sheets. The set gypsum core is formed from a slurry comprising stucco, water, and at least one pregelatinized starch having a viscosity of from about 20 cP to about 300 cP as measured according to the VMA method described herein. The starch is present in an amount of greater than 10% by weight of the stucco. In preferred embodiments, the board has good strength properties even at lower densities, such as about 31 pcf or less. Also disclosed are a related method of making a gypsum wallboard and a slurry.