C04B2111/00431

MATERIAL, APPARATUS, AND METHOD FOR REFRACTORY CASTINGS
20220111434 · 2022-04-14 ·

Provided herein is a system, apparatus, and method for producing refractory products, and more particularly, to producing heated refractories, passive refractories, transition plates, moldable refractories, and accessories such as heated spouts, heated pins, thimbles, and dams. A heated refractory channel as disclosed herein may include a working surface to contain molten metal within the channel; a core adjacent to the working surface; one or more heating elements disposed within the core; and insulation, where the core is disposed between the working surface and the insulation. The one or more heating elements may be molded into the core. The heating elements may be electrical resistance heating elements.

Method of making a refractory article

A method of making a refractory article is provided. The method includes: a) mixing a binder system, a refractory charge, and a second colloidal binder to form an aqueous slurry; b) casting the aqueous slurry into a mold; c) subjecting the mold containing the aqueous slurry to a temperature that is lower than a slurry casting temperature for a time sufficient to form a green strength article; and d) firing the green strength article at a temperature of at least 450° C. for a time sufficient to achieve thermal homogeneity, thereby forming a refractory article. Refractory articles made in accordance with the method have a unique combination of pore structure and mechanical properties.

KR desulfurization stirring paddle casting material and preparation method therefor

Provided are a Kanbara Reactor (KR) desulfurization stirring paddle casting material and a preparation method therefor. The casting material consists of a base material and an additive; the base material consists of the following raw materials in weight percentages: M70 sintered mullite 60-80%, flint clay 5-20%, fine powder 5-20%, and pure calcium aluminate cement 1-5%. The percentages of each component of the additive based on the weight of the base material are as follows: water reducing agent 0.05-0.2%, and heat-resistant stainless steel fiber 1-5%. The main raw materials are M70 sintered mullite and a small amount of flint clay so as to ensure good thermal shock resistance; the medium temperature and high temperature strength are controlled at 100-180 MPa so as to ensure good erosion resistance; the content of Al.sub.2O.sub.3 in the casting material is 60-70% so as to ensure good corrosion resistance; the ratio of high temperature strength to medium temperature strength is controlled at 1-1.2, which further improves the thermal shock resistance and peeling resistance of the casting material, thereby extending the service life of the stirring paddle. The casting material is lower in cost and has a good practical furnace usage effect; in addition, a paddle blade has less chance of cracking and peeling, while a bottom portion of the stirring paddle is less eroded, thus the frequency of paddle blade repair is low, and service life is significantly improved.

Insulating, refractory molded body, especially plate, and process for its manufacture and its usage

An unfired, refractory molded body (1), especially a plate, especially for thermal insulation of molten metal and/or an ingot solidifying from molten metal, that includes a binding agent matrix (2) of a set binder and aggregate grains (3) of biogenic silicic acid, preferably of rice husk ash, which are incorporated into the binding agent matrix (2), wherein the binding agent matrix (2) consists of silica gel, as well as a process for its production and its usage.

Self-bonding refractories for investment casting slurries and molds derived therefrom
11135644 · 2021-10-05 · ·

A self-bonding refractory powder product for use in making a slurry for investment casting molds comprising a coarse refractory powder; a Nano-sized powder; and an organic polymer powder, wherein it does not require aqueous colloidal silica to produce slurries used to build investment casting molds. The Nano-sized powder comprises fumed alumina, boehmite, fumed silica, or fumed titanium oxide or combinations thereof. The coarse refractory powder comprises milled zircon, tabular alumina or fused alumina, fused silica, alumino-silicate, zirconia, and yttria or combinations thereof. The organic polymer powder comprises a cellulose-based material.

Castable refractory compositions comprising zeolithic microstructures and uses thereof

The present invention relates to a dry refractory particulate composition comprising a zeolithic microstructure, to a green body and to a refractory lining formed therefrom, and to uses thereof.

CERAMIC HONEYCOMB BODY FOR LIGHTWEIGHT STRUCTURES AND CORRESPONDING PRODUCTION METHOD

A honeycomb body made of a composite material for fire-resistant lightweight structures including honeycomb cells having a cross section is provided. The cell walls of the honeycomb cells are produced from a composite material. The composite material has at least one carrier, for example a woven fabric or a laid fabric made of fibers, and a matrix into which the carrier is embedded. The matrix includes a silicon-based ceramic material, of which the proportion by mass in the matrix along the cell walls is at least 30 wt. %. A method for producing such a ceramic honeycomb body and a honeycomb tube as an intermediate product for the same are also provided. A flat semi-finished product as a curable intermediate product for the production of fire-resistant fiber composite lightweight structures, which has a matrix mixture including dispersed silicon particles, is also provided.

MINERAL FIBER BASED COMPOSITES
20210179791 · 2021-06-17 ·

The present disclosure provides for binder compositions comprising cellulose ethers, as well as insulation articles and products comprising the same.

SPIN CASTING DEVICE AND METHOD

A spin caster for spraying a surfacing material upon an interior surface of a vessel includes a spin head configured to rotate about an axis, the spin head including an input port, and a supply line coupled to the input port and configured to convey a first material to the spin head and a second material to the spin head. The supply line comprises a first channel configured to convey the first material to the spin head and a second, different channel configured to convey the second material to the spin head.

METHOD OF MAKING A REFRACTORY ARTICLE
20210047240 · 2021-02-18 ·

A method of making a refractory article is provided. The method includes: a) mixing a binder system, a refractory charge, and a second colloidal binder to form an aqueous slurry; b) casting the aqueous slurry into a mold; c) subjecting the mold containing the aqueous slurry to a temperature that is lower than a slurry casting temperature for a time sufficient to form a green strength article; and d) firing the green strength article at a temperature of at least 450 C. for a time sufficient to achieve thermal homogeneity, thereby forming a refractory article. Refractory articles made in accordance with the method have a unique combination of pore structure and mechanical properties.