C08F8/42

Organic polymeric bi-metallic composites

Organic polymeric bi-metallic alkoxide or aryloxide composites are used as dielectric materials in various devices with improved properties such as improved mobility. These composites comprise a poly(meth)acrylate or polyester having metal coordination sites, and the same or different bi-metallic alkoxide or aryloxide molecules that are coordinated with the organic polymer. The bi-metallic alkoxide or aryloxide molecules can be represented by Structure (I) shown herein. Such composites are generally soluble at room temperature in various organic solvents and be provided in homogeneous organic solvent solutions that can be suitably applied to a substrate to form dielectric materials.

Process for Producing Conjugated Diene Polymer
20170260301 · 2017-09-14 · ·

The present invention provides a process for producing a conjugated diene polymer, the process including a production step of producing a conjugated diene polymer solution containing a conjugated diene polymer and a solvent, and a devolatilization step of heating the conjugated diene polymer solution while conveying the conjugated diene polymer solution with an apparatus having rotary twin screws, thereby devolatilizing the solvent, in which a motor current value of the screw in the devolatilization step and a motor current value of the screw under no load satisfy a predetermined relational expression.

Process for Producing Conjugated Diene Polymer
20170260301 · 2017-09-14 · ·

The present invention provides a process for producing a conjugated diene polymer, the process including a production step of producing a conjugated diene polymer solution containing a conjugated diene polymer and a solvent, and a devolatilization step of heating the conjugated diene polymer solution while conveying the conjugated diene polymer solution with an apparatus having rotary twin screws, thereby devolatilizing the solvent, in which a motor current value of the screw in the devolatilization step and a motor current value of the screw under no load satisfy a predetermined relational expression.

BLOCK COPOLYMER INTERMEDIATE, BLOCK COPOLYMER, AND PRODUCTION METHODS FOR SAME
20220235167 · 2022-07-28 · ·

Provided are a block copolymer having a narrow molecular weight distribution such that the copolymer can be used in a DSA technique, a block copolymer intermediate thereof, and methods for producing the same. A block copolymer intermediate represented by the general formula (1) or (2) is used:

##STR00001##

wherein, in the general formulae (1) and (2), each of R.sup.1 and R.sup.3 independently represents a polymerization initiator residue, each of R.sup.2 and R.sup.4 independently represents an aromatic group or an alkyl group, Y.sup.1 represents a polymer block of (a)an (meth)acrylic acid ester, Y.sup.2 represents a polymer block of styrene or a derivative thereof, L represents an alkylene group having 1 to 6 carbon atoms, X represents a halogen atom, and each of m and n independently represents an integer of 1 to 5.

BLOCK COPOLYMER INTERMEDIATE, BLOCK COPOLYMER, AND PRODUCTION METHODS FOR SAME
20220235167 · 2022-07-28 · ·

Provided are a block copolymer having a narrow molecular weight distribution such that the copolymer can be used in a DSA technique, a block copolymer intermediate thereof, and methods for producing the same. A block copolymer intermediate represented by the general formula (1) or (2) is used:

##STR00001##

wherein, in the general formulae (1) and (2), each of R.sup.1 and R.sup.3 independently represents a polymerization initiator residue, each of R.sup.2 and R.sup.4 independently represents an aromatic group or an alkyl group, Y.sup.1 represents a polymer block of (a)an (meth)acrylic acid ester, Y.sup.2 represents a polymer block of styrene or a derivative thereof, L represents an alkylene group having 1 to 6 carbon atoms, X represents a halogen atom, and each of m and n independently represents an integer of 1 to 5.

Block Copolymer, Method for Preparting the Same, and Asphalt Composition Comprising the Same
20220235166 · 2022-07-28 · ·

The present invention relates to a block copolymer, and to a block copolymer including an aromatic vinyl-based polymer block, a conjugated diene-based polymer block and a coupling agent linking group, wherein the conjugated diene-based polymer block includes a hydroxyl group, and the hydroxyl group content is 0.5 mol % to 12.0 mol % based on the double bond content of a conjugated diene-based monomer unit, a method for preparing the same, and an asphalt composition including the same.

Block Copolymer, Method for Preparting the Same, and Asphalt Composition Comprising the Same
20220235166 · 2022-07-28 · ·

The present invention relates to a block copolymer, and to a block copolymer including an aromatic vinyl-based polymer block, a conjugated diene-based polymer block and a coupling agent linking group, wherein the conjugated diene-based polymer block includes a hydroxyl group, and the hydroxyl group content is 0.5 mol % to 12.0 mol % based on the double bond content of a conjugated diene-based monomer unit, a method for preparing the same, and an asphalt composition including the same.

Process for preparation of semi-crystalline functionalized olefin copolymer

The present invention relates to a semi-crystalline functionalized olefin copolymer composition and a process for the preparation of a semi-crystalline functionalized olefin copolymer composition.

Process for preparation of semi-crystalline functionalized olefin copolymer

The present invention relates to a semi-crystalline functionalized olefin copolymer composition and a process for the preparation of a semi-crystalline functionalized olefin copolymer composition.

Hot melt composition, hot melt composition production method, seal material, electronic device, and lamp
11208578 · 2021-12-28 · ·

One aspect of the present invention is a hot melt composition containing a silane coupling agent, a thermoplastic polymer, a softener, and a catalyst, wherein the silane coupling agent is hydrolyzed to a compound having a boiling point of 70 to 180° C.