C08L97/02

NON-POLYMERIC COUPLING AGENT FORMULATIONS FOR WOOD POLYMER COMPOSITES

Non-polymeric coupling agent formulation for producing wood-polymer composites include at least one organic peroxide and a non-polymeric bio-based additive that includes at least one of a bio-based oil or a bio-based acid or derivatives of bio-based oils or acid is provided. The coupling agent formulations are capable of producing polymer matrix composites having improved strength and aging characteristics. The improved strength may be related to physical properties such as improved stiffness, toughness or tensile strength. A masterbatch utilizing the non-polymeric coupling agent formulation is provided, as well as a method making the masterbatch.

Process for obtaining citrus fiber from citrus pulp

A process is disclosed for obtaining citrus fiber from citrus pulp. Citrus fiber is obtained having a c* close packing concentration value of less than 3.8. The citrus fiber can be obtained having a viscosity of at least 1000 mPa.s, wherein said citrus fiber is dispersed in standardized water at a mixing speed of from 800 rpm to 1000 rpm, to a 3 w/w% citrus fiber/standardized water solution, and wherein said viscosity is measured at a shear rate of 5 s-1 at 20° C. Citrus fiber can be obtained having a CIELAB L* value of at least 90. The citrus fiber can be used in food products, feed products, beverages, personal care products, pharmaceutical products or detergent products.

Process for obtaining citrus fiber from citrus pulp

A process is disclosed for obtaining citrus fiber from citrus pulp. Citrus fiber is obtained having a c* close packing concentration value of less than 3.8. The citrus fiber can be obtained having a viscosity of at least 1000 mPa.s, wherein said citrus fiber is dispersed in standardized water at a mixing speed of from 800 rpm to 1000 rpm, to a 3 w/w% citrus fiber/standardized water solution, and wherein said viscosity is measured at a shear rate of 5 s-1 at 20° C. Citrus fiber can be obtained having a CIELAB L* value of at least 90. The citrus fiber can be used in food products, feed products, beverages, personal care products, pharmaceutical products or detergent products.

HEMP POLYMER MATERIALS AND METHODS OF MAKING SAME
20220332926 · 2022-10-20 ·

The present invention relates to polymer compounds containing hemp and/or components of hemp, and methods for producing such polymer compounds.

HEMP POLYMER MATERIALS AND METHODS OF MAKING SAME
20220332926 · 2022-10-20 ·

The present invention relates to polymer compounds containing hemp and/or components of hemp, and methods for producing such polymer compounds.

Method to valorize 2G bioethanol waste streams

An integrated approach for utilizing waste products of 2G bio-refineries to fractionate the lignin of high purity. The present invention also provides a method of recycling of two waste products (2-G ethanol residue as the substrate (LRBR) and fusel oil/synthetic fusel oil (SFO) as one of the solvent) of the biorefineries in a beneficial manner to fractionate the lignin of high purity. The present method of separating high purity lignin comprises fractioning extractive-free lignin rich residue with a solvent, wherein the solvent is a mixture of SFO/Fusel oil and Formic acid. An optimized ratio of waste fusel oil and formic acid gave more than >85% yields of high purity lignin.

Flame-retardant waterproof formaldehyde-free board and method of manufacture
11623991 · 2023-04-11 ·

A flame-retardant, waterproof and formaldehyde-free board is disclosed. The board includes raw material and a coagulant agent. The mass ratio of the raw material to the coagulant agent is 1:1-5. The coagulant includes Agent (A), Agent (B) and magnesium oxide at a mass ratio of 15:2:8-12. In addition, a method of manufacturing the flame-retardant, waterproof and formaldehyde-free board is disclosed.

Flame-retardant waterproof formaldehyde-free board and method of manufacture
11623991 · 2023-04-11 ·

A flame-retardant, waterproof and formaldehyde-free board is disclosed. The board includes raw material and a coagulant agent. The mass ratio of the raw material to the coagulant agent is 1:1-5. The coagulant includes Agent (A), Agent (B) and magnesium oxide at a mass ratio of 15:2:8-12. In addition, a method of manufacturing the flame-retardant, waterproof and formaldehyde-free board is disclosed.

A BIODEGRADABLE BIOCOMPOSITE AND A PROCESS FOR ITS PREPARATION

The present invention relates to biodegradable composites based on blends of a thermoplastic polymer material with cellulosic materials, useful for several industrial and packaging applications, in particular for the manufacture of biodegradable films and articles of complex shape, having improved mechanical properties, oxygen barrier properties, biodegradation and heat resistance; and to a process for the manufacture of these biodegradable composites.

A BIODEGRADABLE BIOCOMPOSITE AND A PROCESS FOR ITS PREPARATION

The present invention relates to biodegradable composites based on blends of a thermoplastic polymer material with cellulosic materials, useful for several industrial and packaging applications, in particular for the manufacture of biodegradable films and articles of complex shape, having improved mechanical properties, oxygen barrier properties, biodegradation and heat resistance; and to a process for the manufacture of these biodegradable composites.