Patent classifications
C21D9/22
Drill component
The present disclosure relates to a drill component having a martensitic stainless steel which has good corrosion resistance in combination with optimized and well-balanced mechanical properties, such as high hardness, resistance against wear and abrasion, high tensile strength and high impact toughness.
Martensitic stainless steel
The present disclosure relates to a martensitic stainless steel suitable for rock drill steel rods. Furthermore, the present disclosure also relates to the use of the martensitic stainless steel and to products manufactured thereof, especially drill rods.
Martensitic stainless steel
The present disclosure relates to a martensitic stainless steel suitable for rock drill steel rods. Furthermore, the present disclosure also relates to the use of the martensitic stainless steel and to products manufactured thereof, especially drill rods.
Drill bit for drilling and method for manufacturing same
Disclosed are a drill bit for drilling and a method for manufacturing same, in which the hardness of a body part of a shank can be selectively improved by performing rapid cooling in a forced cooling method after performing rapid heating selectively only on the body part of the shank in a high-frequency induction heating method after completing infiltration.
Drill bit for drilling and method for manufacturing same
Disclosed are a drill bit for drilling and a method for manufacturing same, in which the hardness of a body part of a shank can be selectively improved by performing rapid cooling in a forced cooling method after performing rapid heating selectively only on the body part of the shank in a high-frequency induction heating method after completing infiltration.
Compressive residual stress-hardened downhole tool shaft region
The disclosure provides downhole tools with shaft regions that are hardened by a compressive residual stress created when an allotropic material in a precursor region transforms from a first allotrope to a second allotrope in response to heat, while continuing to occupy the same physical space. The disclosure further provides methods of forming such downhole tools.
Compressive residual stress-hardened downhole tool shaft region
The disclosure provides downhole tools with shaft regions that are hardened by a compressive residual stress created when an allotropic material in a precursor region transforms from a first allotrope to a second allotrope in response to heat, while continuing to occupy the same physical space. The disclosure further provides methods of forming such downhole tools.
BORING BIT COMPONENT WITH HARD FACE WEAR RESISTANCE MATERIAL WITH SUBSEQUENT HEAT TREATMENT
A boring bit or other component for horizontal directional drilling is provided which includes a hard faced layer that is preferably made by a laser cladding bead. A subsequent or post heat treatment is applied to modify the heat affected zone (HAZ) to eliminate or reduce the hard brittle regions and/or softer regions in the base iron or steel material of the HAZ. Further, the hard faced layer may be applied in combination with carbide insert teeth that are embedded within the steel base of the boring bit body, such as by press fitting.
BORING BIT COMPONENT WITH HARD FACE WEAR RESISTANCE MATERIAL WITH SUBSEQUENT HEAT TREATMENT
A boring bit or other component for horizontal directional drilling is provided which includes a hard faced layer that is preferably made by a laser cladding bead. A subsequent or post heat treatment is applied to modify the heat affected zone (HAZ) to eliminate or reduce the hard brittle regions and/or softer regions in the base iron or steel material of the HAZ. Further, the hard faced layer may be applied in combination with carbide insert teeth that are embedded within the steel base of the boring bit body, such as by press fitting.
High-speed tool steel, material for tools, and method for producing material for tools
Provided are a high-speed tool steel having excellent hot workability, and excellent damage resistance when made into various tools; a material for tools, and a method for producing the same. The high-speed tool steel contains, in mass %, 0.9-1.2% of C, 0.1-1.0% of Si, 1.0% or less of Mn, 3.0-5.0% of Cr, 2.1-3.5% of W, 9.0-10.0% of Mo, 0.9-1.2% of V, 5.0-10.0% of Co, 0.020% or less of N, and the remainder being Fe and impurities, wherein an M value calculated by a formula satisfies 1.5M value1.5. Formula: M value=9.500+9.334[% C]0.275[% Si]0.566[% W]0.404[% Mo]+3.980[% V]+0.166[% Co], where the characters in brackets [ ] indicate the contained amounts (mass %) of the respective elements. The present invention also pertains to: a material for tools, which is obtained by using the high-speed tool steel; and a method for producing the material for tools.