A Method of Pretreatment and Bromine Recovery of PCB Incineration Ash
A method of pretreatment and bromine recovery of PCB Incineration ash is disclosed that relates to the field of comprehensive recovery of valuable metals by full wet method, especially relates to a method of valuable metals and bromine recovery, precious metals enrichment in pretreatment process of PCB Incineration ash. The major steps includes alkali leaching, Cu extraction back-extraction, neutralization-precipitation to separate, Bromine evaporative crystallization, regeneration, acid pickling, Zn evaporative crystallization, removal of Zn and Cu. Compared with the traditional comprehensive recovery process of ash, the invention can separate bromine from ash and recover valuable metals such as copper, zinc and lead with the maximum extent, at the same time, the enrichment of silver and other precious metals is beneficial to the subsequent recovery of precious metals. It has high added recovery value and no tailless discharge.
PROCESS FOR ACIDIC LEACHING OF PRECIOUS AND CHALCOPHILE METALS
A process for recovery of one or more elements, selected from precious metals and chalcophile metals as herein defined, from materials containing precious and/or chalcophile metal/s, said process including: (i) a leaching step comprising contacting the material with an acidic solution containing a lixiviant comprising an aqueous amino acid-thiourea compound formed from an amino acid (as herein defined) and thiourea (as herein defined), in order to form a leachate containing the precious metal and/or chalcophile metal; and (ii) a recovery step comprising recovering the precious metal and/or chalcophile metal from the leachate.
PROCESS FOR THE PURIFICATION OF WASTE MATERIALS OR INDUSTRIAL BY-PRODUCTS COMPRISING CHLORINE
The present application relates to a process for the purification of waste materials or industrial by-products, the process comprising the steps of: a) Preparing a composition (C) by blending or mixing waste materials or industrial by-products comprising chlorine (B) with one or more materials comprising heavy metals (HM) b) Reacting (B) and (HM) by thermal treatment of (C) c) Separating evaporated heavy metal chloride compounds (HMCC) d) Obtaining a solid material after the thermal treatment step.
PROCESS FOR THE PURIFICATION OF WASTE MATERIALS OR INDUSTRIAL BY-PRODUCTS COMPRISING CHLORINE
The present application relates to a process for the purification of waste materials or industrial by-products, the process comprising the steps of: a) Preparing a composition (C) by blending or mixing waste materials or industrial by-products comprising chlorine (B) with one or more materials comprising heavy metals (HM) b) Reacting (B) and (HM) by thermal treatment of (C) c) Separating evaporated heavy metal chloride compounds (HMCC) d) Obtaining a solid material after the thermal treatment step.
Acid digestion processes for recovery of rare earth elements from coal and coal byproducts
A system for recovering rare earth elements from coal ash includes a leaching reactor, an ash dryer downstream of the leaching reactor, and a roaster downstream of the ash dryer that is cooperatively connected to both the leaching reactor and the ash dryer. Coal ash is mixed with an acid stream such that rare earth elements present in the coal ash are dissolved in the acid stream, thereby creating (i) a leachate containing the rare earth elements and (ii) leached ash. The leachate is heated to obtain acid vapor and an acid-soluble rare earth concentrate. Mixing of the coal ash with the acid stream can occur in a leaching reactor and heating of the leachate can occur in a roaster. The acid-soluble rare earth concentrate can be fed to a hydrometallurgical process to separate and purify the rare earth elements.
Acid digestion processes for recovery of rare earth elements from coal and coal byproducts
A system for recovering rare earth elements from coal ash includes a leaching reactor, an ash dryer downstream of the leaching reactor, and a roaster downstream of the ash dryer that is cooperatively connected to both the leaching reactor and the ash dryer. Coal ash is mixed with an acid stream such that rare earth elements present in the coal ash are dissolved in the acid stream, thereby creating (i) a leachate containing the rare earth elements and (ii) leached ash. The leachate is heated to obtain acid vapor and an acid-soluble rare earth concentrate. Mixing of the coal ash with the acid stream can occur in a leaching reactor and heating of the leachate can occur in a roaster. The acid-soluble rare earth concentrate can be fed to a hydrometallurgical process to separate and purify the rare earth elements.
SYSTEMS FOR ACID DIGESTION PROCESSES
A system for recovering rare earth elements from coal ash includes a leaching reactor, an ash dryer downstream of the leaching reactor, and a roaster downstream of the ash dryer that is cooperatively connected to both the leaching reactor and the ash dryer. Coal ash is mixed with an acid stream such that rare earth elements present in the coal ash are dissolved in the acid stream, thereby creating (i) a leachate containing the rare earth elements and (ii) leached ash. The leachate is heated to obtain acid vapor and an acid-soluble rare earth concentrate. Mixing of the coal ash with the acid stream can occur in a leaching reactor and heating of the leachate can occur in a roaster. The acid-soluble rare earth concentrate can be fed to a hydrometallurgical process to separate and purify the rare earth elements.
METHODS FOR RECOVERY OF RARE EARTH ELEMENTS FROM COAL
Methods of recovering rare earth elements, vanadium, cobalt, or lithium from coal are described. The coal is dissolved in a first solvent to dissolve organic material in the coal and create a slurry containing coal ash enriched with rare earth elements, vanadium, cobalt, or lithium. The enriched coal ash is separated from the first solvent. Residual organic material is removed from the coal ash. The rare earth elements, vanadium, cobalt, or lithium can then be recovered from the coal ash. The coal ash is mixed with an acid stream that dissolves the rare earth elements, thereby creating (i) a leachate containing the rare earth elements and (ii) leached ash. The leachate is heated to obtain acid vapor and an acid-soluble rare earth concentrate. The acid-soluble rare earth concentrate can be fed to a hydrometallurgical process to separate and purify the rare earth elements.
ZINC RECOVERY METHOD
Dust Da containing zinc and iron is charged in a rotative cylindrical kiln base body 11 of an indirect-heating rotary kiln 10 and is subjected to heat treatment in the kiln base body so that zinc contained in the dust is volatilized. The volatilized zinc is guided to a treatment device 30 through an exhaust pipe 31 disposed at a discharge part 16 of the rotary kiln and is recovered. A residue Db resulting from the treatment in the kiln base body is transferred from a residue outlet 16b disposed at the discharge part 16 of the rotary kiln to a burner device 40, in which the residue is combusted and heated.
ZINC RECOVERY METHOD
Dust Da containing zinc and iron is charged in a rotative cylindrical kiln base body 11 of an indirect-heating rotary kiln 10 and is subjected to heat treatment in the kiln base body so that zinc contained in the dust is volatilized. The volatilized zinc is guided to a treatment device 30 through an exhaust pipe 31 disposed at a discharge part 16 of the rotary kiln and is recovered. A residue Db resulting from the treatment in the kiln base body is transferred from a residue outlet 16b disposed at the discharge part 16 of the rotary kiln to a burner device 40, in which the residue is combusted and heated.