C22B13/04
Treated Geothermal Brine Compositions With Reduced Concentrations Of Silica, Iron and Manganese
This invention relates to treated geothermal brine compositions containing reduced concentrations of iron, silica, and manganese compared to the untreated brines. Exemplary compositions contain a concentration of manganese less than 10 mg/kg, a concentration of silica ranging from less than 10 mg/kg, and a concentration of iron less than 10 mg/kg, and the treated geothermal brine is derived from a Salton Sea geothermal reservoir.
METHOD FOR PREPARING LEAD DIRECTLY FROM LEAD-CONTAINING MATERIAL BY SOLID PHASE REACTION
A method for preparing lead directly from a lead-containing material by a solid phase reaction, includes: step 1, adding the lead-containing material to be processed to the grinder, and adding a metal substance and water to the grinder, wherein an activity of the metal substance is larger than that of lead; the solid phase reaction between the lead-containing material and the metal substance is caused directly by the grinder through a mechanical force to obtain a reaction product; step 2, washing and filtering the reaction product to obtain the lead and a metal salt solution corresponding to the metal substance; step 3, performing a melt casting on the lead to obtain a crude lead, crystallizing the metal salt solution to obtain a metal salt corresponding to the metal substance.
METHOD OF EXTRACTING METALS FROM POLYMETALLIC SULPHIDE ORES OR CONCENTRATES
A method of extracting metals from polymetallic sulphide ores or concentrates comprising at least Cu, Zn, Pb and Ag, comprising a first step of atmospheric leaching in sulphate medium in the presence of recycled silver for extracting Cu and Zn and a second step of atmospheric leaching in chloride medium for extracting Pb and Ag.
Methods for purifying and recycling lead from spent lead-acid batteries
The present disclosure relates to methods by which lead from spent lead-acid batteries may be extracted, purified, and used in the construction of new lead-acid batteries. A method includes: (A) forming a mixture including a carboxylate source and a lead-bearing material; (B) generating a first lead salt precipitate in the mixture as the carboxylate source reacts with the lead-bearing material; (C) increasing the pH of the mixture to dissolve the first lead salt precipitate; (D) isolating a liquid component of the mixture from one or more insoluble components of the mixture; (E) decreasing the pH of the liquid component of the mixture to generate a second lead salt precipitate; and (F) isolating the second lead salt precipitate from the liquid component of the mixture. Thereafter, the isolated lead salt precipitate may be converted to leady oxide for use in the manufacture of new lead-acid batteries.
SYSTEMS AND METHODS FOR CLOSED-LOOP RECYCLING OF A LIQUID COMPONENT OF A LEACHING MIXTURE WHEN RECYCLING LEAD FROM SPENT LEAD-ACID BATTERIES
The present disclosure relates generally to systems and methods for recycling lead-acid batteries, and more specifically, relates to purifying and recycling the lead content from lead-acid batteries. A system includes a reactor that receives and mixes a lead-beating material waste, a carboxylate source, and a recycled liquid component to form a leaching mixture yielding a lead carboxylate precipitate. The system also includes a phase separation device coupled to the reactor, wherein the phase separation device isolates the lead carboxylate precipitate from a liquid component of the leaching mixture. The system further includes a closed-loop liquid recycling system coupled to the phase separation device and to the reactor, wherein the closed-loop liquid recycling, system receives the liquid component isolated by the phase separation device and recycles a substantial portion of the received liquid component back to the reactor as the recycled liquid component.
Treated geothermal brine compositions with reduced concentrations of silica, iron and manganese
This invention relates to treated geothermal brine compositions containing reduced concentrations of iron, silica, and manganese compared to the untreated brines. Exemplary compositions contain a concentration of manganese less than 10 mg/kg, a concentration of silica ranging from less than 10 mg/kg, and a concentration of iron less than 10 mg/kg, and the treated geothermal brine is derived from a Salton Sea geothermal reservoir.
INTEGRATED RECOVERY OF METALS FROM COMPLEX SUBSTRATES
Described is a method of recovering a metal from a substrate having a metal sulphide, metal oxide, or combination thereof, by contacting the substrate with an aqueous oxidant to oxidize the metal sulphide to elemental sulphur and oxidized metal or convert the complex metal oxide to a metal salt, contacting the oxidized metal or simple metal oxide with ammonium hydroxide to form soluble a ammine complex of the metal to obtain a leachate and residual solids; separating the leachate from the residual solids; and recovering the metal.
METHODS FOR PURIFYING AND RECYCLING LEAD FROM SPENT LEAD-ACID BATTERIES
The present disclosure relates to methods by which lead from spent lead-acid batteries may be extracted, purified, and used in the construction of new lead-acid batteries. A method includes: (A) forming a mixture including a carboxylate source and a lead-bearing material; (B) generating a first lead salt precipitate in the mixture as the carboxylate source reacts with the lead-bearing material; (C) increasing the pH of the mixture to dissolve the first lead salt precipitate; (D) isolating a liquid component of the mixture from one or more insoluble components of the mixture; (E) decreasing the pH of the liquid component of the mixture to generate a second lead salt precipitate; and (F) isolating the second lead salt precipitate from the liquid component of the mixture. Thereafter, the isolated lead salt precipitate may be converted to leady oxide for use in the manufacture of new lead-acid batteries.
Hydrometallurgical process for the recovery of copper, lead or zinc
A hydrometallurgical process for the treatment of polymetallic ores and sulphide concentrates of copper and zinc, and by-products of lead and zinc from smelting plants, treated independently and/or as mixtures thereof, which contain relevant amounts of lead, copper, zinc, iron, gold and silver, such as the matte-speiss mixture of lead foundries, and copper cements from the purification processes of electrolytic zinc plants. The process allows the recovery of metallic copper, zinc, copper as copper and zinc basic salts, which may be hydroxides, carbonates, hidroxysulphates or mixtures thereof; the production of stable arsenic residues; and the effective and efficient recovery of Pb, Au and Ag as a concentrate of lead sulphide and/or lead, Au, and Ag sulphate.
Processes for recovering non-ferrous metals from solid matrices
A process for recovering non-ferrous metals from a solid matrix may include: (a) leaching the solid matrix with an aqueous-based solution containing chloride ions, ammonium ions, and Cu.sup.2+ ions, having a pH of 6.5-8.5, in a presence of oxygen, at a temperature of 100 C.-160 C. and a pressure of 150 kPa-800 kPa, so as to obtain an extraction solution comprising leached metals and solid leaching residue; (b) separating the solid leaching residue from the extraction solution; and/or (c) subjecting the extraction solution to at least one cementation so as to recover the leached metals in elemental state. The pH may be greater than or equal to 6.5 and less than or equal to 8.5. Temperature may be greater than or equal to 100 C. and less than or equal to 160 C. Pressure may be greater than or equal to 150 kPa and less than or equal to 800 kPa.