C22B21/0015

Process, apparatus, and system for recovering materials from batteries
11273453 · 2022-03-15 · ·

An apparatus for carrying out size reduction of battery materials under immersion conditions can include a housing configured to hold an immersion liquid comprising at least one of sodium hydroxide and calcium hydroxide. A first feed chute may define an opening therein for receiving battery materials of a first type into the housing and a first submergible comminuting device may be disposed within the housing and submerged in the immersion liquid to receive the battery materials of the first type from the first feed chute. The first submergible comminuting device may be configured to cause a size reduction of the battery materials of the first type to form a first reduced-size battery material.

Process, apparatus, and system for recovering materials from batteries
11135595 · 2021-10-05 · ·

An apparatus for carrying out size reduction of battery materials under immersion conditions can include a housing configured to hold an immersion liquid comprising at least one of sodium hydroxide and calcium hydroxide. A first feed chute may define an opening therein for receiving battery materials of a first type into the housing and a first submergible comminuting device may be disposed within the housing and submerged in the immersion liquid to receive the battery materials of the first type from the first feed chute. The first submergible comminuting device may be configured to cause a size reduction of the battery materials of the first type to form a first reduced-size battery material.

Process, apparatus, and system for recovering materials from batteries
11077452 · 2021-08-03 · ·

The present application provides a process to recover materials from rechargeable lithium-ion batteries, thus recycling them. The process involves processing the batteries into a size-reduced feed stream; and then, via a series of separation, isolation, and/or leaching steps, allows for recovery of a copper product, cobalt, nickel, and/or manganese product, and a lithium product; and, optional recovery of a ferrous product, aluminum product, graphite product, etc. An apparatus and system for carrying out size reduction of batteries under immersion conditions is also provided.

DECISION-MAKING METHOD OF COMPREHENSIVE ALUMINA PRODUCTION INDEXES BASED ON MULTI-SCALE DEEP CONVOLUTIONAL NETWORK
20210192272 · 2021-06-24 ·

The invention provides a decision-making method of comprehensive alumina production indexes based on a multi-scale deep convolutional network. The method mainly consists of several sub-models: a multi-scale deep splicing convolutional neural network prediction sub-model reflecting the influence of bottom-layer production process indexes on the comprehensive alumina production indexes, a full connecting neural network prediction sub-model reflecting the influence of upper-layer dispatching indexes on the comprehensive alumina production indexes, a full connecting neural network prediction sub-model reflecting the influence of the comprehensive alumina production indexes at a past time on current comprehensive alumina production indexes, and a multi-scale information neural network integrated model for collaborative optimization of sub-model parameters. According to the method, through an integrated prediction model structure, a memory capacity of a superficial-layer network and a feature extraction capacity of a deep-layer network, a precise decision-making for the comprehensive alumina production indexes is realized.

Method of Processing and Treatment of Alunite Ores
20210071281 · 2021-03-11 ·

The alunite ore processing method consists of crushing, grinding and flotation of raw alunite ore. The enriched alunite ore is roasted at 520 to 620 C., the roasting time is 1 to 3 hours. The roasted alunite is leached with 5 to 20% sodium carbonate solution, which is in 100 to 110% of the stoichiometric amount required to bond the SO.sub.3 aluminum sulfate in the alunite with leaching conditions of 70-100 C. for 0.5-2.0 hours. The obtained slurry contains all of the potassium sulfate from the alunite and all of the sodium sulfate obtained from sodium carbonate. In the insoluble residue remains all aluminium oxide and residual rock. The sulfate solution is separated from the insoluble residue and is converted with potassium chloride to potassium sulphate (fertilizer) and kitchen salt. The insoluble residue is treated by the Bayer method without the use of an autoclave and results in aluminium oxide (alumina) and quartz sand.

PROCESS, APPARATUS, AND SYSTEM FOR RECOVERING MATERIALS FROM BATTERIES
20210078012 · 2021-03-18 ·

An apparatus for carrying out size reduction of battery materials under immersion conditions can include a housing configured to hold an immersion liquid comprising at least one of sodium hydroxide and calcium hydroxide. A first feed chute may define an opening therein for receiving battery materials of a first type into the housing and a first submergible comminuting device may be disposed within the housing and submerged in the immersion liquid to receive the battery materials of the first type from the first feed chute. The first submergible comminuting device may be configured to cause a size reduction of the battery materials of the first type to form a first reduced-size battery material.

PROCESS, APPARATUS, AND SYSTEM FOR RECOVERING MATERIALS FROM BATTERIES
20210078013 · 2021-03-18 ·

An apparatus for carrying out size reduction of battery materials under immersion conditions can include a housing configured to hold an immersion liquid comprising at least one of sodium hydroxide and calcium hydroxide. A first feed chute may define an opening therein for receiving battery materials of a first type into the housing and a first submergible comminuting device may be disposed within the housing and submerged in the immersion liquid to receive the battery materials of the first type from the first feed chute. The first submergible comminuting device may be configured to cause a size reduction of the battery materials of the first type to form a first reduced-size battery material.

Process, apparatus, and system for recovering materials from batteries
10960403 · 2021-03-30 · ·

A process for recovering component materials from lithium battery materials, the process comprising the steps of: a) processing lithium battery materials in a comminuting apparatus comprising at least a first comminuting device that is submerged in an immersion liquid, thereby creating reduced-size battery materials and liberating electrolyte material and a black mass material comprising anode and cathode powders from within the lithium battery materials and providing a sized-reduced feed stream comprising the reduced size battery materials and the black mass material and electrolyte materials entrained within the immersion liquid; and b) processing the size-reduced feed stream to obtain at least a black mass solid stream that comprises the black mass material and a retained portion of the immersion liquid having entrained electrolyte materials.

Process, apparatus, and system for recovering materials from batteries
10919046 · 2021-02-16 · ·

An apparatus for carrying out size reduction of battery materials under immersion conditions having a battery inlet and at least a first comminuting device disposed within a housing and configured to cause a size reduction of the battery materials to form reduced-size battery materials and to liberate electrolyte materials and a black mass material comprising anode and cathode powders from within the battery materials. An immersion liquid can be within the housing and can submerge the first comminuting device so the black mass material and the reduced-size battery material are entrained within the immersion liquid to form a sized-reduced feed stream. A feed outlet may be downstream from the first comminuting device.

METHOD FOR CONTROLLING THE CONCENTRATION OF IMPURITIES IN BAYER LIQUORS
20210070624 · 2021-03-11 ·

A method for controlling the concentration of impurities in Bayer liquors, the method comprising the steps of adding an oxide and/or a hydroxide of a metal other than aluminium to a Bayer liquor with a desired TA; forming a layered double hydroxide; and incorporating at least one impurity in said layered double hydroxide, wherein the impurities are selected from the group comprising phosphorus, vanadium and silicon.