C22C29/16
Cermet, method for producing cermet, and cutting tool
A cermet contains hard phase particles containing Ti and a binding phase containing at least one of Ni and Co, and 70% or more (by number) of the hard phase particles have a cored structure containing a core and a peripheral portion around the core. The core is composed mainly of at least one of Ti carbide, Ti nitride, and Ti carbonitride, and the peripheral portion is composed mainly of a Ti composite compound containing Ti and at least one selected from W, Mo, Ta, Nb, and Cr. The core has an average particle size α, the peripheral portion has an average particle size β, and α and β satisfy 1.1≦β/α≦1.7.
Cermet and cutting tool
A cermet contains hard phase particles containing Ti and a binding phase containing at least one of Ni and Co. 70% or more of the hard phase particles have a cored structure containing a core and a peripheral portion around the core. The core is composed mainly of at least one of Ti carbide, Ti nitride, and Ti carbonitride. The peripheral portion is composed mainly of a Ti composite compound containing Ti and at least one selected from W, Mo, Ta, Nb, and Cr. The core has an average particle size α, the peripheral portion has an average particle size β, and α and β satisfy 1.1≦β/α≦1.7. The hard phase particles in the cermet have an average particle size of more than 1.0 μm.
Cermet and cutting tool
A cermet contains hard phase particles containing Ti and a binding phase containing at least one of Ni and Co. 70% or more of the hard phase particles have a cored structure containing a core and a peripheral portion around the core. The core is composed mainly of at least one of Ti carbide, Ti nitride, and Ti carbonitride. The peripheral portion is composed mainly of a Ti composite compound containing Ti and at least one selected from W, Mo, Ta, Nb, and Cr. The core has an average particle size α, the peripheral portion has an average particle size β, and α and β satisfy 1.1≦β/α≦1.7. The hard phase particles in the cermet have an average particle size of more than 1.0 μm.
Composite wear pad and methods of making the same
A composite wear pad includes a substrate that is selected from the group of iron based alloys, steel, nickel based alloys, and cobalt based alloys. A hard particle-matrix alloy layer is bonded at a surface to the substrate. The hard particle-matrix alloy layer has a plurality of hard particles dispersed in a matrix alloy. The hard particle-matrix alloy layer has a thickness ranging between greater than about 13 millimeters and about 20 millimeters.
Composite wear pad and methods of making the same
A composite wear pad includes a substrate that is selected from the group of iron based alloys, steel, nickel based alloys, and cobalt based alloys. A hard particle-matrix alloy layer is bonded at a surface to the substrate. The hard particle-matrix alloy layer has a plurality of hard particles dispersed in a matrix alloy. The hard particle-matrix alloy layer has a thickness ranging between greater than about 13 millimeters and about 20 millimeters.
Induction infiltration and cooling of matrix drill bits
Zonal heating and cooling during the production of matrix drill bits may be achieved with a system that includes a cavity defined within a mold assembly having a central axis; reinforcing particles and a binder material disposed within the cavity; and a plurality of induction coils about a periphery of the mold assembly, each induction coil being spaced from each other along the height of the mold assembly, wherein a first induction coil of the plurality of induction coils is arranged proximal to a portion of mold assembly containing a portion of the reinforcing particles and a second induction coil of the plurality of induction coils is arranged proximal to a portion of the mold assembly containing a portion of the binder material.
Negative electrode for lithium secondary battery and method of manufacturing the same
In an aspect, a negative electrode for a lithium secondary battery and a method of manufacturing the same is provided. The negative electrode for the lithium secondary battery includes a negative active material layer.
Negative electrode for lithium secondary battery and method of manufacturing the same
In an aspect, a negative electrode for a lithium secondary battery and a method of manufacturing the same is provided. The negative electrode for the lithium secondary battery includes a negative active material layer.
Composite sintered material
A composite sintered material includes a plurality of diamond grains, a plurality of cubic boron nitride grains, and a remainder of a binder phase, wherein the binder phase includes cobalt, a content of the cubic boron nitride grains in the composite sintered material is more than or equal to 3 volume % and less than or equal to 40 volume %, and an average length of line segments extending across continuous cubic boron nitride grains in appropriately specified straight lines extending through the composite sintered material is less than or equal to a length three times as large as an average grain size of the cubic boron nitride grains.
METHOD FOR TREATING A SUPERHARD COMPOSITE MATERIAL INTENDED FOR BEING USED IN THE PRODUCTION OF CUTTING TOOLS
The invention relates to a method of processing a superhard composite material (21) comprising a polycrystalline microstructure and a binder, said method comprising the following steps: contacting (200) a surface of said superhard composite material (21) with an absorbent material (30), and applying (300) an electric current to the superhard composite material (21), causing the binder to move from the superhard composite material (21) to the absorbent material (30) so as to create a continuous gradient (221) of binder content within the superhard composite material (21).