Patent classifications
C22C29/18
Degradable metal matrix composite
The present invention relates to the composition and production of an engineered degradable metal matrix composite that is useful in constructing temporary systems requiring wear resistance, high hardness, and/or high resistance to deformation in water-bearing applications such as, but not limited to, oil and gas completion operations.
Degradable Metal Matrix Composite
The present invention relates to the composition and production of an engineered degradable metal matrix composite that is useful in constructing temporary systems requiring wear resistance, high hardness, and/or high resistance to deformation in water-bearing applications such as, but not limited to, oil and gas completion operations.
Degradable Metal Matrix Composite
The present invention relates to the composition and production of an engineered degradable metal matrix composite that is useful in constructing temporary systems requiring wear resistance, high hardness, and/or high resistance to deformation in water-bearing applications such as, but not limited to, oil and gas completion operations.
Negative electrode active material for electrical device
A negative electrode active material having high cycle durability contains an alloy represented by the following chemical formula (1):
Si.sub.xSn.sub.yM.sub.zA.sub.a(1)
wherein M is Zn, A is unavoidable impurities, x, y, z, and a represent % by mass values, and in that case, 0<x<100, 0<y<100, 0<z<100, 0a<0.5, and x+y+z+a=100, in which the half width of the diffraction peak of the (111) surface of Si in the range of 2=24 to 33 by X ray diffraction measurement of the alloy using CuK ray is 0.7 or more, and the x is more than 23 and less than 64, the y is 4 or more and less than 34, and the z is more than 0 and less than 65.
Negative electrode active material for electrical device
A negative electrode active material having high cycle durability contains an alloy represented by the following chemical formula (1):
Si.sub.xSn.sub.yM.sub.zA.sub.a(1)
wherein M is Zn, A is unavoidable impurities, x, y, z, and a represent % by mass values, and in that case, 0<x<100, 0<y<100, 0<z<100, 0a<0.5, and x+y+z+a=100, in which the half width of the diffraction peak of the (111) surface of Si in the range of 2=24 to 33 by X ray diffraction measurement of the alloy using CuK ray is 0.7 or more, and the x is more than 23 and less than 64, the y is 4 or more and less than 34, and the z is more than 0 and less than 65.
INSITU METAL MATRIX NANOCOMPOSITE SYNTHESIS BY ADDITIVE MANUFACTURING ROUTE
A unique and novel additive manufacturing route has been proposed to form a thermally stable in-situ metal matrix nano composite by interfacing reactive plasma in the selective laser melting process chamber. The proposed route gives very high compositional freedom, i.e, nitrides, carbides, oxides, suicides and other ceramics with different stoichiometries can be reinforced in nanoscale in any metallic matrix. Components with such a nanocomposite structure dispiay superior high temperature structural properties.
Advanced high temperature and fatigue resistant environmental barrier coating bond coat systems for SiC/SiC ceramic matrix composites
Advanced environmental barrier coating bond coat systems with higher temperature capabilities and environmental resistance are disclosed. These bond coat systems can be applied to ceramic substrates such as SiC/SiC ceramic matrix composite substrates, and can provide protection from extreme temperature, mechanical loading and environmental conditions, such as in high temperature gas turbines. Example bond coat systems can include either an advanced silicon/silicide component, an oxide/silicate component, or a combination thereof.
Advanced high temperature and fatigue resistant environmental barrier coating bond coat systems for SiC/SiC ceramic matrix composites
Advanced environmental barrier coating bond coat systems with higher temperature capabilities and environmental resistance are disclosed. These bond coat systems can be applied to ceramic substrates such as SiC/SiC ceramic matrix composite substrates, and can provide protection from extreme temperature, mechanical loading and environmental conditions, such as in high temperature gas turbines. Example bond coat systems can include either an advanced silicon/silicide component, an oxide/silicate component, or a combination thereof.
SINTERING WITH SPS/FAST URANIUM FUEL WITH OR WITHOUT BURNABLE ABSORBERS
The present invention relates to nuclear fuel compositions including uranium dioxide with integral fuel burnable absorber, and triuranium disilicide and a composite of uranium mononitride and triuranium disilicide with or without integral fuel burnable absorber, and methods of sintering these compositions. The sintering is conducted using SPS/FAST apparatus and techniques. The sintering time and temperature is reduced using SPS/FAST as compared to conventional sintering methods for nuclear fuel compositions. The nuclear fuel compositions of the present invention are particularly useful in light water reactors.
Magnesium alloy powder metal compact
A powder metal compact is disclosed. The powder metal compact includes a cellular nanomatrix comprising a nanomatrix material. The powder metal compact also includes a plurality of dispersed particles comprising a particle core material that comprises an MgZr, MgZnZr, MgAlZnMn, MgZnCuMn or MgW alloy, or a combination thereof, dispersed in the cellular nanomatrix.